1-20 of 21 Search Results for

meter shafts

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1998) 47 (9): Al-352.
Published: 01 September 1998
...) are known for being small in size. Alloy 2011 is typically used in connectors and fittings, brake pistons, computer parts, knobs, and meter shafts. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes...
Journal Articles
Alloy Digest (1998) 47 (7): Al-350.
Published: 01 July 1998
.... OF machine 300 sfm IS suggesesred rmmmum Applications: Aircraft fittings, gears and shafts. fuse parts, meter shafts, gears, missile parts, regulating valves, worm gears, keys, aerospace connectors and fittings, and defense parts bility and anodizing response. The T73 and T7351 tern Producer: ALCOA Wire, Rod...
Journal Articles
Alloy Digest (1997) 46 (3): Al-341.
Published: 01 March 1997
... include automotive fuel system componen- try, clock parts, gears, camera parts, meter shafts, ordnance, in- dustrial connectors, and speedometer components. Producer: Aluminum Company of America Wm. Rod, and Bar Division Massena, NY 13662-0160 (800) 622-5262 ISSN: 002-614X AL341B Get-11 conosion...
Journal Articles
Alloy Digest (2021) 70 (1): Al-472.
Published: 01 January 2021
... solderability. Auto fuel systems, bolts, camera parts, clock parts, fittings, Comparable Grades gears, industrial connectors, machine parts, meter shafts, nuts, ordnance, pipe stems, screw-machine products, screws, Atlas Steels Atlas 2011 TV fittings. ASTM Alloy 2011 (UNS A92011) EN EN AW-2011 (EN AW-Al Cu6BiPb...
Journal Articles
Alloy Digest (1979) 28 (10): Bi-14.
Published: 01 October 1979
...) 0.045 Yield temperature, oF (oC) 240 (116) Thermal coef. expansion/oC (Approx) 22 x 10-6 Electrical conductivity, % IACS Electrical resistivity,* Ohms/mm2/meter Volume change (liquid to solid), % Volume change (Linear growth after solidification), % *Ohms based on volume standard (meter, mm2) PROPERTIES...
Journal Articles
Alloy Digest (1983) 32 (3): Bi-30.
Published: 01 March 1983
... heat. Btu/lb/OF (Liquid) (Solid) Thermal coef. expansion! F (60-130°F) (13&218 F) Electrical conductivity, %iACS (Volume basis) Electrical resistivity. l * Ohms/mm ~meter Volume change (Liquid to solid Volume change (Linear growth after solidification 0.343 9.5 218440 240 0.04. 0.045 I29 x 10-6 Zero...
Journal Articles
Alloy Digest (1970) 19 (12): Cu-223.
Published: 01 December 1970
.... bushings. gears. pinions. screws. cams. meter parts. pump parts. washers, shafts. valve parts. screw machine products. bolts. and electrical equipment. Manufacturer: hlost copper and brass mills. .4naconda .r\merican Brass (Rod, Bar). Bridgeport Brass (Rod. Bar, W ire). Scovill hlanufacturing (Rod. Wire W...
Journal Articles
Alloy Digest (1995) 44 (7): Cu-602.
Published: 01 July 1995
... valve bolting (1 meter long). Actuator components and bolting on Xmas tree valves. (Statfjord satellites). Pump drive shaft couplings (Australia). Towing slip components and bolting on UK submarines. Bolting on MOD (N) equipment. Propeller shafts. Components in head-up display units on combat aircraft...
Journal Articles
Alloy Digest (1979) 28 (12): Bi-15.
Published: 01 December 1979
... Electrical resistivity, ** Ohms/mm2/meter Volume change (Liquid to solid), % Volume change (Linear growth after solidification), % *Approximate. **Ohms based on volume standard (meter, mm2). 0.05* 5.00 0.3445 +0.77 0.05 Table 1 - MECHANICAL PROPERTIES (As-cast condition) Tensile strength, psi Elongation (2...
Journal Articles
Alloy Digest (1982) 31 (9): Bi-29.
Published: 01 September 1982
... Electrical resistivity Ohms/mm2/meter Volume change (Liquid to solid), Qo Volume change (Linear growth after solidification), Qo *Approximate. **Ohms based on volume standard (meter, mm2). PROPERTIES Table 1 - MECHANICAL PROPERTIES (As-cast condition) Tensile strength, psi 8ooO Elongation (2 in Qo (Slow...
Journal Articles
Alloy Digest (1983) 32 (12): Bi-33.
Published: 01 December 1983
... coed. expansion 1 F C Thermal conductivity (solid), cal /cm*/cm Is / C Electrical conductivity, 9% IACS Electrical resistivity. &* Ohms/mm2/meter Volume change (liquid to solid). 9% Volume change (Linear growth after solidification). % Approximate. **Ohms based on volume standard (meter. mm...
Journal Articles
Alloy Digest (1995) 44 (6): Cu-601.
Published: 01 June 1995
... HIDURON alloy 191 was developed for marine applications where both a combination of strength and good corrosion/ impingement resistance is needed. It finds applications in shafts, fasteners and valve stems. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1988) 37 (9): SA-18.
Published: 01 September 1988
...) 212 (100) 392 (200) 752 (400) 1112(600) Thermal Conductivity Btu/ftVftWF(W/m°C) - - 24.7 (42.7) 24.4 (42.3) 21.8 (37.7) 19.1 (33.1) Electrical Resistivity n&ohm-meter 0.22 0.26 0.33 0.48 0.65 Table 2 - ROOM-TEMPERATUREMECHANICAL PROPERTIES 7.85 0.283 O.ll(473) 0.12(519) 0.13 (561) 6.0 x lad 7.12 x lad...
Journal Articles
Alloy Digest (1985) 34 (11): SS-466.
Published: 01 November 1985
... % % Hardness 392 200 2 16000 1490 171000 I I76 28 10 425 752 400 2 10000 1450 171000 I I76 33 8 425 1112 600 I44000 996 107000 735 50 17 280 I292 700 99000 686 78000 539 62 0 200 Table 3 - TURNING .L\ND MlLLlNG MACHINING P.AR.\METERS Tool Material Cemented Carbide High-Speed Steel Operation Depth of cut...
Journal Articles
Alloy Digest (1976) 25 (12): Cu-323.
Published: 01 December 1976
... applications including couplings and fit- tings, taps, cocks, faucets, valves, flanges and water mixers for bathrooms; housings for water-meters and thermostats; pump housings, shafts and wheels; end pieces for brake lines in cars. buses and trucks; marine hardware; halyard and sheet winches for boats...
Journal Articles
Alloy Digest (1976) 25 (9): SS-333.
Published: 01 September 1976
.... Machinability: Carpenter No. 5 BQ cuts freely because of the addition of sulfur. In automatic screw machines, it machines similar to SAE 1120 with cutting speeds of 140 to 155 surface feet per minute (43 to 47 meters per minute) on high-speed form tools. Copyright © ASM International® 1996DOI: 10.31399...
Journal Articles
Alloy Digest (1958) 7 (1): Cu-58.
Published: 01 January 1958
...- meter. Use a lubricant especially for cutting speed of 75-250 feet per minute and feed of 0.003-O.O2O /rev for drill sizes of l/8 to 3,/4 . The lighter feeds are used with the smaller diameter drills. Slow spiral brass dtitls with thin webs and polished flutes are recommended. DOI: 10.31399...
Journal Articles
Alloy Digest (1960) 9 (8): Cu-91.
Published: 01 August 1960
... applications as it retains its ductility, tensile and impact strengths at low temperatures. Forms Available: Sheet, rod and wire. Applications: Springs, diaphrams, shafts, marine parts, meter gears, clips, Fourdrinier wire, clutch disks, bellows, fasteners, lock washers, switch parts, wire brushes, chemical...
Journal Articles
Alloy Digest (1970) 19 (10): SS-244.
Published: 01 October 1970
... direct material costs by reducing the sire of the part. Forms Available: All standard product forms, finishes, and conditions. Applications: Aircraft and aerospace nozzles, ducting, hub assemblies, vanes, etc.; marine shafting. impellers, hardware, diaphragms, chain, pump parts, fittings, tension devices...
Journal Articles
Alloy Digest (1985) 34 (6): CS-107.
Published: 01 June 1985
... surface meters/ minute. ipr q inches per revolution. mm/r = millimeters per revolution. Nore: Similar data are available from the manufacturer on box tools, reamers, threading, tapping and cut off. DOI: 10.31399/asm.ad.cs0107 Copyright © ASM International® 1996 Heet Treatment: La Salle Series 83-420 steel...