1-20 of 690 Search Results for

metal cores

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1981) 30 (7): SA-381.
Published: 01 July 1981
... AIRCO METAL-COR 6 is a continuous tubular steel welding electrode with a powdered-metal core; gas shielding rather than slag is used to protect the core. It eliminates 50 to 70% of the smoke and fumes generated by self-shielded flux-cored electrodes and about 30% of the smoke from gas-shielded...
Journal Articles
Alloy Digest (1998) 47 (5): Ni-542.
Published: 01 May 1998
... INCO-CORED 625DH and 625AP flux-cored wires were developed as companion welding materials to Inconel Filler Metal 625 (Alloy Digest Ni-327, December 1985) and Inconel Welding Electrode 112 (Alloy Digest Ni-313, April 1985). This datasheet provides information on composition and tensile properties...
Journal Articles
Alloy Digest (1998) 47 (6): Ni-543.
Published: 01 June 1998
... INCO-CORED 82DH (down-hand) and 82AP (all-position) flux cored wired were developed as companion welding materials to INCONEL Filler Metal 82 and INCO-WELD A Welding Electrode. Applications include welding Inconel or Incoloy alloys to themselves or to ferritic, austenitic, or ferric/austenitic...
Journal Articles
Alloy Digest (2006) 55 (7): SS-968.
Published: 01 July 2006
... as friction or inertia welding, as well as high-energy processes, such as laser and electron beam welding, may be satisfactory. Postweld heat treatment is desirable for toughness and magnetic performance. Use of austenitic stainless steel filler metal is not recommended due to the magnetic air gap...
Journal Articles
Alloy Digest (1990) 39 (4): Fe-90.
Published: 01 April 1990
... properties CARPENTER SILICON CORE IRON B Filing Code: Iron Alloy Fe-90 - DIGEST- APRIL 1990 DATA ON WORLD WIDE METALS AND ALLOYS Pdiishedby: Alloy Digest. Inc 1201-677-9161 27 Canfield Street. Orange. N.J. 07050 / U.S.A. CARPENTER SILICON CORE IRON B Carpenter Silicon Core Iron B is melted in...
Journal Articles
Alloy Digest (1991) 40 (1): Fe-94.
Published: 01 January 1991
... properties CARPENTER SILICON CORE IRON A Filing Code: Iron Alloy Fe-94 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS JANUARY 1991 Ptiidhed byr Ahy Digeet. Inc /2[)1-6Z -9161 27 CaMeId Stmet. Orange. NJ. 07060 I U.SA CARPENTER SILICON CORE IRON A (High Initial Permeability Magnetic Core Iron...
Journal Articles
Alloy Digest (1986) 35 (12): Fe-74.
Published: 01 December 1986
... properties pole pieces switches tensile properties workability CARPENTER SILICON CORE IRON C Filing Code: Iron Fe-74 DECEMBER 1986 - DATA ON WORLD WIDE METALS AND ALLOYS Puhliched h, 411oy Digest. inc. 2 Canfield Street Orange. lieu Jersey 07050 1101 I 61-1090 CARPENTER* SILICON CORE IRON C...
Journal Articles
Alloy Digest (1968) 17 (11): Fe-36.
Published: 01 November 1968
... - DATA ON WORLD WIDE METALS AND ALLOYS SILICON CORE IRON Published by Engineering Alloys Digest, Inc. Upper Montclair, New Jersey (Magnetic Core Iron) Silicon Core Iron is a low carbon silicon electric furnace melted iron recommended for direct current and alternating current magnetic applications in...
Journal Articles
Alloy Digest (2004) 53 (1): Fe-125.
Published: 01 January 2004
... Copper/Invar/Copper is a wrought metallic composite material used in printed circuit boards, power planes, metal cores, hybrid enclosures, heat sinks, and other applications where coefficients of thermal expansion (CTE) match or where constraint of thermal expansion is required or beneficial. The...
Journal Articles
Alloy Digest (2007) 56 (11): Ag-13.
Published: 01 November 2007
... information on physical properties and tensile properties. Filing Code: AG-13. Producer or source: Fort Wayne Metals. Producer or Source: Fort Wayne Metals Copyright © ASM International® 2007 2007 ASM International DFT wire physical properties tensile properties Composition: Core materials...
Journal Articles
Alloy Digest (1984) 33 (3): SA-399.
Published: 01 March 1984
... the homogeneous metal-core composition and the carbon dioxide shielding gas. Both weld-metal composition and mechantcal properties are consistent. uniform and predictable. Tuf-Cor I Welding Electrode produces a low-hydrogen quality weld metal with good ductility and Charpy V-notch impact values...
Journal Articles
Alloy Digest (1998) 47 (3): Ni-538.
Published: 01 March 1998
... restrained joints in gray iron. None of the cast irons require a postweld heat treatment. General Characteristics: NI-ROD FC 55 cored wire is a filler metal specifically designed for semiautomatic or automatic welding of ductile iron. malle- able iron, and gray cast irons to themselves and to steel. NI-ROD...
Journal Articles
Alloy Digest (2012) 61 (4): SS-1118.
Published: 01 April 2012
... workability DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2012, ASM International®. All rights reserved. Data shown are typical, not to be used for specification or final design. Published by: ASM International, Materials Park, OH 44073-0002, 440-338-5151 MemberServiceCenter@asminternational.org Fax 440...
Journal Articles
Alloy Digest (1994) 43 (4): SA-473.
Published: 01 April 1994
... metal is required, consider AWS E/ER430. Post weld heat treatment is desirable for tough- ness and magnetic performance. Use of austenitic stainless filler metal is not recommended due to the magnetic air gap created. Chrome Core 8-M alloy is not recommended for welding. Applications could include...
Journal Articles
Alloy Digest (1994) 43 (5): SA-474.
Published: 01 May 1994
... 12-FM are available from the producer. Weldabllity: Chrome Core 12 alloy can be satisfactorily welded by shielded fusion and resistance welding processes. Oxyacetylene weld- ing is not recommended. When filler metal is required, con- sider AWS E/ER430. Post weld heat ueatment is desirable for...
Journal Articles
Alloy Digest (2007) 56 (9): SS-996.
Published: 01 September 2007
... austenitic stainless steel filler metal is not recommended due to the magnetic air gap created. Table 1 Comparison of the Physical/Magnetic Properties of Various Alloys Magnetic peak inductance Resistivity Coercivity Alloy T G Maximum permeability · m circular-mil/ft A/m Oe Chrome Core 13-XP 1.7 17,000...
Journal Articles
Alloy Digest (1998) 47 (1): Fe-116.
Published: 01 January 1998
... - DATA ON WORLD WIDE METALS AND ALLOYS Filing Code: Fe-116 a Iron Alloy u P January 1996 PuMshed by: ASM /nIernationa/ Mareriab Park, Ohio 44073-mwz 4m-m-5151 Fax&M Mem&?rv&o.ASM-lnti.org CARPENTER SILICON CORE IRON (Machinable Soft Magnetic Alloy) B-FM Carpenter Silicon Core Iron B-FM is melted in...
Journal Articles
Alloy Digest (1993) 42 (12): Fe-103.
Published: 01 December 1993
... physical properties tensile properties workability thermal properties UNS K94101 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS CARPENTER LOW EXPANSION ;n gnf;;e: 42 @DUMET CORE ROD Fe-l 03 DECEMBER 1993 PuElish.sdby: Aloy Dige~I. II-C. /201-677-9161 27 Canfield SIreel. Orange. N.J. 07050 1 U.S.A...
Journal Articles
Alloy Digest (1994) 43 (3): Fe-106.
Published: 01 March 1994
... workability Filing Code: Fe-l 06 NK SUPER-E CORE Iron Alloy - DIGEST- MARCH 1994 DATA ON WORLD WIDE METALS AND ALLOYS Published by: Alloy Digest. Inc /201-677-9161 27 Canhdd SIreeL Orange. N.J. 07060 / U.S.A NK SUPER-E CORE (Very High Silicon Electrical Steel) NK SUPER-E CORE is a non-oriented silicon...
Journal Articles
Alloy Digest (2005) 54 (1): Fe-135.
Published: 01 January 2005
...: 10.31399/asm.ad.fe0135 Product Forms Available: Coils with thickness 0.2 mm or 0.1 mm, and width 600 mm max- imum. Applications: Typical applications include high-frequency AC/DC reactors for insulated gate bipolar transistors (IGBT), metal oxide semicon- ductor field effect transistor (MOS-FET) inverters...