Alloy Digest (1995) 44 (2): Al-332.
Published: 01 February 1995
.... tnc. All rghls r(LFBNBd. Publrshedby: Alloy DigesI. Inc. IZO1-677.9161 L?afashwnivattobsusedlor 27 Canfield SIreel. Orange. N.J. 07U50 / U.S.A Jpecrication or fmt desgn. DURALCAN F3N.l OS/F3N.20S (Aluminum metal matrix composite for pressure die castings) DURALCAN F3N.xxS is an aluminum composite...
Journal Articles
Alloy Digest (1956) 5 (6): Zn-3.
Published: 01 June 1956
... DI-METAL 3 is a zinc-base alloy of high fluidity capable of producing fine detail in die castings. It is the most stable of the zinc die casting alloys, but on aging loses about 20% of its tensile strength with practically no impact drop. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1957) 6 (4): Zn-4.
Published: 01 April 1957
... No. 2 DIE METAL is a zinc-base alloy recommended primarily for die castings and sand castings (stamping and drop-hammer dies). This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fracture toughness and fatigue...
Journal Articles
Alloy Digest (1953) 2 (11): CI-4.
Published: 01 November 1953
... ABK Metal is a nickel-chromium cast iron with excellent wear resistance, recommended for severe abrasive service. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on wear...
Journal Articles
Alloy Digest (1959) 8 (3): Cu-72.
Published: 01 March 1959
... NI-VEE TYPE C is a leaded precipitation hardening nickel bronze alloy suitable for constructional, pressure, and bearing metal castings. Its strength is superior to red brass; its mechanical properties are comparable to those of lead-free G-bronze. This datasheet provides information...
Journal Articles
Alloy Digest (1955) 4 (4): CI-10.
Published: 01 April 1955
... EASTERN Z-METAL is a cast ferrous alloy that possesses a unique combination of high strength, machinability, wear resistance, and toughness. Its microstructure consists of temper carbon nodules dispersed through a uniform matrix of spheroidite and ferrite. This alloy is made in several different...
Journal Articles
Alloy Digest (2022) 71 (7): Cu-932.
Published: 01 July 2022
... bars; forged round, square, and flat bars; forged plates; rough and pre-machined pieces cut from round bar and plates. Applications Die casting pistons in cold chamber die casting machines; cooling inserts in molds; molds for nonferrous metal casting (e.g., low pressure casting). Hot-pressed parts...
Journal Articles
Alloy Digest (1993) 42 (5): Ni-432.
Published: 01 May 1993
... Hastelloy Alloy G-30 filler metal is used as matching composition filler metal for fabrication of Hastelloy G-30 wrought and cast products and as filler metal for fabrication of G/G-3 alloy wrought products. It is also used for weld repair of high chromium castings and for weld overlay cladding...
Journal Articles
Alloy Digest (1963) 12 (8): Cu-132.
Published: 01 August 1963
... OUNCE Metal, also known as Composition Metal, is a cast 5% leaded bronze recommended for bearings, valves and pump bodies. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1996) 45 (11): Fe-114.
Published: 01 November 1996
... Ni-Rod Filler Metal 44 is a solid, nickel-iron-manganese wire designed for automatic and semiautomatic welding of ductile, malleable, and gray cast irons in all positions. NI-Rod Filler Metal 44 offers high-speed, high-quality welds and can be used with all robotics, automatic, and semiautomatic...
Journal Articles
Alloy Digest (1978) 27 (5): Cu-353.
Published: 01 May 1978
... BELMONT Alloy 4582 is a alloy developed to meet the special needs of jewelers for a base-metal alloy suitable for casting centrifugally in refractory molds. It can be joined readily to itself and other alloys by soldering or brazing. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1993) 42 (8): Co-93.
Published: 01 August 1993
... properties compared to the cast counterparts. The types of carbides present in STELLlTE STAR J-Metal PM, M6C and M7C3 are similar to those present in STELLITE STAR J-Metal Cast. Applications: Typical applications include vane plugs, fuel metering pins, and spacer bushings for the aerospace industry; ball...
Journal Articles
Alloy Digest (1973) 22 (10): Al-15.
Published: 01 October 1973
... information on corrosion resistance as well as casting, heat treating, machining, and surface treatment. Filing Code: Al-15. Producer or source: Federated Metals Corporation, ASARCO Inc.. Originally published April 1954, revised October 1973. Producer or Source: Federated Metals Corporation, ASARCO Inc...
Journal Articles
Alloy Digest (1954) 3 (11): CI-9.
Published: 01 November 1954
..., backed by grey cast iron where the metal has cooled more slowly. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, heat treating, machining, and joining. Filing Code: CI-9. Producer or source...
Journal Articles
Alloy Digest (1968) 17 (10): Al-180.
Published: 01 October 1968
... and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-180. Producer or source: Federated Metals Corporation, ASARCO Inc.. Producer or Source: Federated Metals Corporation, ASARCO Inc. Copyright © ASM International®...
Journal Articles
Alloy Digest (1962) 11 (5): Al-114.
Published: 01 May 1962
... performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-114. Producer or source: Federated Metals Corporation, ASARCO Inc.. Producer or Source: Federated Metals Corporation, ASARCO Inc. Copyright © ASM International® 1996 1996 ASM International...
Journal Articles
Alloy Digest (1980) 29 (3): Cu-392.
Published: 01 March 1980
... resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-392. Producer or source: Ampco Metal Inc.. Producer or Source: Ampco Metal Inc. Copyright © ASM International® 1996 1996 ASM International AMPCOLOY 570 cast copper alloys castability chemical composition...
Journal Articles
Alloy Digest (1963) 12 (12): Al-132.
Published: 01 December 1963
..., elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-132. Producer or source: Federated Metals Corporation, ASARCO Inc.. Producer or Source: Federated...
Journal Articles
Alloy Digest (1975) 24 (2): Al-213.
Published: 01 February 1975
... properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-213. Producer or source: Federated Metals Corporation, ASARCO Inc.. Producer or Source: Federated Metals Corporation, ASARCO Inc...
Journal Articles
Alloy Digest (1977) 26 (8): Al-228.
Published: 01 August 1977
..., physical properties, hardness, and tensile properties as well as fatigue. It also includes information on casting, forming, heat treating, and machining. Filing Code: Al-228. Producer or source: Belmont Metals Inc.. Producer or Source: Belmont Metals Inc. Copyright © ASM International® 1996 1996...