Alloy Digest (2017) 66 (4): Ti-159.
Published: 01 April 2017
... ATI 6-4 ELI, also known as Grade 23, is a higher purity grade of ATI Ti-6Al-4V for use in surgical and medical applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (2020) 69 (8): SS-1326.
Published: 01 August 2020
... Zapp Ergste 1.4028YN is a medium-carbon, 13% Cr, martensitic stainless steel that is designed for medical applications requiring high strength and hardness along with good corrosion resistance in moderately corrosive environments. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2010) 59 (2): SS-1055.
Published: 01 February 2010
.../medical applications. CARPENTER CTS-40CP ALLOY (Martensitic Stainless Die Steel) CARPENTER CTS- 40CP ALLOY Chemical Composition, wt (Type Analysis) Carbon 0.95 1.20 Manganese 1.00 Phosphorus 0.04 max Sulfur 0.030 max Silicon 1.00 Chromium 16.00 18.00 Molybdenum 0.75 Iron bal Physical Properties: Density...
Journal Articles
Alloy Digest (2005) 54 (7): Ti-136.
Published: 01 July 2005
... Applications: Typical applications are with orthopedic, trauma, spinal, and cardiovas- cular devices. References: 1. L. Zardiackas, D. Mitchell, and J. Disegi, Characterization of Ti-15Mo Alloy for Orthopaedic Implant Applications, Medical Applications of Titanium and Its Alloys, STP 1272, S.A. Brown and J.E...
Journal Articles
Alloy Digest (2021) 70 (5): Ti-178.
Published: 01 May 2021
... equipment. It also has numerous applications in the medical industry. Arcam Ti6Al4V ELI is very similar to Arcam Ti6Al4V, except that Arcam Ti6Al4V ELI contains reduced levels of oxygen, nitrogen, carbon, and iron. These lower interstitials provide improved ductility and better fracture toughness...
Journal Articles
Alloy Digest (2013) 62 (8): SS-1154.
Published: 01 August 2013
... food processing, paper processing, textile, packaging, recycling/refuse, kitchen knives, hand tools, scissors/shears, shaving razors, sport/hunting knives, ice skates, military/defense, law enforcement, salon blades, and various surgical/medical applications. CTS-BD30P ALLOY (Martensitic Stainless...
Journal Articles
Alloy Digest (2014) 63 (9): Ti-157.
Published: 01 September 2014
... Sandvik Bioline Ti6Al4V ELI is an alpha-beta titanium alloy used mainly for medical implant applications. It is an extra low interstitial alloy with a high purity, which confers improved ductility and fracture toughness. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2006) 55 (7): Ti-139.
Published: 01 July 2006
... Allvac Titanium Alloy 6Al-7Nb uses niobium to stabilize the beta phase. It is very similar to Ti-6Al-4V and is widely used in medical and surgical device applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (2019) 68 (6): Cu-890.
Published: 01 June 2019
... chemical composition corrosion-resistant alloys food processing applications medical equipment Olin Brass Alloy C77000 physical properties solderability spring applications stiffness switches wrought copper alloys thermal properties UNS C77000 Olin Brass Alloy C77000 is an excellent spring...
Journal Articles
Alloy Digest (2021) 70 (8): Co-139.
Published: 01 August 2021
... Deloro Stellite 21 (UNS R30021), previously known as Stellite 8, is similar to the medical implant alloy ASTM F75. It is a Co-Cr- Mo-Ni alloy that was developed in the mid-1930s as a corrosion resistant alloy, and rapidly found application as a biocompatible hip implant and denture alloy...
Journal Articles
Alloy Digest (2010) 59 (12): Co-120.
Published: 01 December 2010
... applications medical instruments physical properties springs tensile properties workability thermal properties UNS R30035 DATA ON WORLDWIDE METALS AND ALLOYS Copyright © 2010, ASM International®. All rights reserved. Data shown are typical, not to be used for specification or final design. Published...
Journal Articles
Alloy Digest (2000) 49 (1): SS-774.
Published: 01 January 2000
... CORRAX is a precipitation-hardening (PH) stainless mold steel that may be used for many demanding applications. Its superior resistance to corrosion, combined with a hardness of up to 50 HRC, makes it well suited for molds making medical parts, all molds running in a clean-room environment, parts...
Journal Articles
Alloy Digest (2023) 72 (5): SS-1358.
Published: 01 May 2023
... for demanding applications such as molds for medical parts, parts made of corrosive plastics, and parts made of rubber. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on corrosion...
Journal Articles
Alloy Digest (2014) 63 (11): SS-1188.
Published: 01 November 2014
... for many blade applications, including commercial food processing, paper processing, textile, packaging, recycling/refuse, kitchen knives, hand tools, scissors/shears, shaving razors, sport/hunting knives, ice skates, military/ defense, law enforcement, salon blades, and various surgical/medical...
Journal Articles
Alloy Digest (2021) 70 (3): Ti-176.
Published: 01 March 2021
..., automotive, indus- trial, marine, and medical applications. Aging (Precipitation Heat Treatment). Heat to 482 538 °C (900 1000 °F). Wait for equalization of the temperature. Soak Supplier for 8 h. Cool in still air. TIMET Machinability 4832 Richmond Road Suite 100 The lathe machinability V15 test values...
Journal Articles
Alloy Digest (2015) 64 (9): SS-1224.
Published: 01 September 2015
..., and strip Typical Applications: Pulp and paper industry, chemical industry, medical applications, textile finishing, pharmaceutical industry, low temperature equipment, applications with high magnetic fields. Producer: Outokumpu Stainless Bar, Inc. Richburg, SC 29706, USA Tel: (888) 458-4600 Fax: (803) 789...
Journal Articles
Alloy Digest (1995) 44 (6): SS-596.
Published: 01 June 1995
... that is required for medical applications. Turning cut-off 6nd Form Tools IPR .OOl cut-off l/8 SFPM 56-85 Tool Width IPR .0015 114 SPPM 56-85 Workability: Hot Working/Forging l/2 Form 1 Tool Width l-1/2 114 Drilling BioDur 316LS stainless can be readily forged, upset, and hot headed. To forge, heat...
Journal Articles
Alloy Digest (2014) 63 (10): SS-1185.
Published: 01 October 2014
... skates, military/defense, law enforcement, salon blades, and various surgical/medical applications. CARPENTER® CTS® BDZ1 ALLOY (Martensitic Stainless Steel) CARPENTER® CTS® BDZ1 ALLOY Chemical Composition, wt (Type analysis, maximum) Carbon 0.60 0.70 Manganese 1.00 Phosphorus 0.025 Sulfur 0.010 Silicon...
Journal Articles
Alloy Digest (2016) 65 (1): SS-1235.
Published: 01 January 2016
... industry, chemical industry, medical applications, textile finishing, pharmaceutical industry, and low temperature equipment Producer: Outokumpu Stainless Bar Richburg, SC 29706, USA Tel: (888) 458-4600 Fax: (803) 789-3177 www.outokumpu.com ISSN: 002-614X SS-1235B Table 2 Grade S31655 properties measured...
Journal Articles
Alloy Digest (2023) 72 (6): Ti-193.
Published: 01 June 2023
.... Applications Elgiloy CP Titanium Grade 1 is used for aerospace, automotive, chemical processing, marine, and medical applications. Typical applications include heat exchangers and surgical implants. Supplier Elgiloy Specialty Metals 1565 Fleetwood Drive Elgin, Illinois 60123, USA Tel: +1 888 843 2350 Web...