Alloy Digest (2011) 60 (9): SA-634.
Published: 01 September 2011
... Dillidur 325L is a wear resistant steel with a surface hardness at room temperature of 325 HB for 10 mm plate thickness. The material is easy to bend, hot work and machine. Due to its increased wear resistance, it is used to produce excavators, conveyors, and materials handling systems as well...
Journal Articles
Alloy Digest (1969) 18 (11): Co-59.
Published: 01 November 1969
..., machining, and joining. Filing Code: Co-59. Producer or source: Union Carbide Materials Systems Division. Producer or Source: Union Carbide Materials Systems Division Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity...
Journal Articles
Alloy Digest (1976) 25 (12): Cu-323.
Published: 01 December 1976
... DZR Yellow Brass is a new, corrosion-resistant brass. It has excellent resistance to dezincification which makes it highly suitable for water-system applications, marine hardware, ornaments and door handles. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1983) 32 (8): Ni-289.
Published: 01 August 1983
... tendency to crack during welding. Consult the manufacturer for recommenda- tions on joining materials. Corrosion Resistance: As mentioned in the introduction, Jessop JS Alloy G resists corrosion in both oxidizing and reducing environments; also, it can handle both acid and alkaline solutions. it resists...
Journal Articles
Alloy Digest (2001) 50 (6): Ni-569.
Published: 01 June 2001
...- rials may contain, in varying concentrations, elemental constitu- tions of chromium, iron manganese, molybdenum, cobalt, nickel, tungsten, and aluminum. Inhalation of metal dust from welding, grinding, melting, and dross handling of these alloy systems may cause adverse health effects. Specifications...
Journal Articles
Alloy Digest (2008) 57 (9): Ni-665.
Published: 01 September 2008
... handling thermal spray powders, avoid inhalation or contact with the skin or eyes. See AWS Publication C2.1 Recommended Safe Practices for Thermal Spray, and read the manufacturer s material safety data sheet before use. Storage Requirements. Keep thermal spray powders dry and in a closed container...
Journal Articles
Alloy Digest (2010) 59 (4): Cu-781.
Published: 01 April 2010
... nozzles and manifolds for hot runner systems. BOEHLER UDDEHOLM ALLOY BeCu172 (Beryllium Copper Mold Material) BOEHLER UDDEHOLM ALLOY BeCu172 Chemical Composition, wt (Typical) Beryllium 1.9 Cobalt + nickel 0.25 Copper bal Physical Properties: Age-hardened to 30 or 40 HRC. Data at room and elevated...
Journal Articles
Alloy Digest (1955) 4 (4): Fe-7.
Published: 01 April 1955
... silicon iron alloy, which is qua& if not the superior, of any other com- mercially available material for handling hydrochloric acid at all concentrations and at high, as well as low temperatures. It is produced in the cast form only. The hardness of the alloy makes it very resistant to abrasion...
Journal Articles
Alloy Digest (1994) 43 (5): SS-566.
Published: 01 May 1994
..., and castings. Contact the producer. Specification Equivalents: UNS S32550 ASTM A240 Applications: UR 52N is used for its seawater resistance in offshore sour-gas transportation and sea water injection systems. It is fabricated into equipment for the chemical industry to handle acids (phos- phoric), pulp...
Journal Articles
Alloy Digest (2013) 62 (9): Cu-824.
Published: 01 September 2013
... part dimensional control, better parting line maintenance, and excellent corrosion resistance. Safe Handling of Copper Beryllium. Handling copper beryllium in solid form poses no special health risk. Like many industrial materials, beryllium-containing materials may pose a health risk if recommended...
Journal Articles
Alloy Digest (1992) 41 (10): Ni-413.
Published: 01 October 1992
... and Safety: Beryllium containing materials can present a health risk unless precautions are employed. Consult Brush Wellman for the most effective methods of safely handling beryl- lium containing materials. General Characteristics: Brush Alloy 360 beryllium nickel combines mechanical strength and physical...
Journal Articles
Alloy Digest (2013) 62 (8): Cu-823.
Published: 01 August 2013
... copper beryllium in solid form poses no special health risk. Like many industrial materials, beryllium-containing materials may pose a health risk if recommended safe handling practices are not followed. Inhalation of airborne beryllium may cause a serious lung disorder in susceptible individuals...
Journal Articles
Alloy Digest (1990) 39 (1): P-15.
Published: 01 January 1990
... tensile properties ii f kby TACTIX 123 & TACTIX 138 Filing Code: P-15 RESIN SYTEMS Plastic JANUARY 1990 -DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS PWbiWdby: AlOyD@t. lnC/ZOl-677-9161 27 Cankdd SlreeI. Orange. NJ. 07060 I U.S.A. TACTIX 123 & TACTIX 138 RESIN SYSTEMS (Resin Systems for Ik(uld molding...
Journal Articles
Alloy Digest (2004) 53 (4): SS-902.
Published: 01 April 2004
... to oxidation and corrosion. It is typically used in automotive exhaust systems or where more forming is required. Table 1 Mechanical Properties for Material with 2D Finish Hardness, Yield strength Tensile strength Elongation, HRB MPa ksi MPa ksi % ASTM A 240, 92 max 275 min 40 min 415 min 60 min 20 min UNS...
Journal Articles
Alloy Digest (1973) 22 (7): Zn-16.
Published: 01 July 1973
... slirrhtly before they are formed. Castability: Korloy alloy 2570 can be melted and handled easily by nonferrous foundries, usually without altering patterns or molding materials. It has excellent casting character- istics and can be cast in sand, plaster, rubber or permanent molds. The optimum casting...
Journal Articles
Alloy Digest (1993) 42 (1): Fe-98.
Published: 01 January 1993
... constituents. These alloy are not recommended for nitric acid solutions containing flue rides. Hydrochloric Acid: Durichlor 51 and Superchlor are economical materials to handle all concentrations of hy- drochloric acid up to 80°F. Most alloys that possess any degree of resistance to commercially pure...
Journal Articles
Alloy Digest (2009) 58 (8): SS-1041.
Published: 01 August 2009
... and weapons handling equipment in naval vessels. Tank bridging system components. Oil and Gas. Pumps, valves, bolting, electrical connectors, pipe work/flanges, and wellhead equipment. Nuclear. Mechanical handling equipment. Chemical. Pumps, valves, fans, agitators, centrifuges, seals, boltings, filters, pipe...
Journal Articles
Alloy Digest (1991) 40 (12): P-32.
Published: 01 December 1991
... melt adhesives and excellent ther- mal cycling properties for tooling. TACTIX 741 in solu- tion in acetone is designed for composites prepared by solution prepregging. Glass transition temperatures for these resins are about 300°C. Safety and Handling: Resin systems comprised of resins, curing agents...
Journal Articles
Alloy Digest (2003) 52 (6): Ni-608.
Published: 01 June 2003
... °C (1800 °F). Laboratory tests show that 8500 has erosion resistance equal to that of Metco 465. Metallographic evaluation found lit- tle loss of chromium during the spray process, maximizing the corrosive barrier characteristics of this material. When sprayed with nitrogen instead of air...
Journal Articles
Alloy Digest (1981) 30 (6): Co-77.
Published: 01 June 1981
... Characteristics: As mentioned in the introduction, lncor 16 is a new permanent- magnet material that is vastly superior to other available per- manent-magnet materiab. In fact, the magnetic fields produced by lncor 16 are so high that additional caution in handling is necessary. The force of attraction between...