1-20 of 558 Search Results for

martensite

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1971) 20 (2): SS-251.
Published: 01 February 1971
... CUSTOM 450 Stain essStee Filing Code: SS-251 FEBRUARY 1971 DIGEST - DATA ON WORLD WIDE METALS AND ALLOYS Pvblisbrd by CARPENTER CUSTOM 450* Engineering Alloys Digest, Inc. Upper Montclair. New Jersey (Martensitic Age-Hardenable Stainless Steel) CARPENTER CUSTOM 450 stainless steel has very good...
Journal Articles
Alloy Digest (1972) 21 (3): SS-269.
Published: 01 March 1972
... weldability CAIGN M Filing Code: ES-269 Stainless Steel MARCH 1972 - DATA ON WORLD WIDE METALS AND ALLOYS Publisbd by Engineering Alloys Digest, Inc Upper Montclair, New Jersey CA-6NM (Martensitic Stainless Steel) CA-6NM is a cast stainless steel that has good resistance to cracking during and after...
Journal Articles
Alloy Digest (1972) 21 (4): SS-271.
Published: 01 April 1972
... PYROTOOL 15 is a low-carbon martensitic precipitation-hardenable (maraging) heat-resistant steel designed to possess high strength from room temperature to 1050 F. Uses include tooling applications. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1972) 21 (5): SS-273.
Published: 01 May 1972
... Montclair. New Jersey EMPIRE ISO450* (Martensitic Age-Hardenable Cast Stainless Steel) EMPIRE IS0450 is a cast stainless steel with excellent corrosion resistance. A simple, single-step aging treatmcnl dcvclop, high strength with good ductility and toughness. *EMPIRE and IS0 are registered trademarks...
Journal Articles
Alloy Digest (1974) 23 (1): TS-266.
Published: 01 January 1974
... FERRO-TIC M-6 is comprised of ultra-hard titanium carbide grains dispersed through a matrix of age-hardenable martensitic steel. There are three grades: regular M-6 and M-6A and M-6B. The latter two have increased carbide which gives greater hardness at some sacrifice in machinability...
Journal Articles
Alloy Digest (1967) 16 (9): SS-200.
Published: 01 September 1967
... AISI No. 616 is a hardenable martensitic type stainless steel recommended for high temperature applications up to 1200 F. It is used for steam turbine blades and buckets, valves, jet engine components, and high temperature bolting. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1968) 17 (4): SS-208.
Published: 01 April 1968
... Fifth-Vickers F.V. 520(S) is a corrosion resistant martensitic steel which is readily weldable and capable of being hardened by low temperature heat treatment. It is recommended for turbine components and supersonic aircraft parts. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1962) 11 (6): SS-133.
Published: 01 June 1962
... Filing Code: 55-133 JETHETE M.152 Stainless Steel JUNE 1962 -DATA ON WORLD WIDE METALS AND ALLOYS JETHETE M.152 Pmblirbed by Engineering Alloys Digest, Inc. Upper Montclair. New Jersq (Martensitic Stainless Steel) Jethete M.152 is a new martensitic stainless steel combining high tensile strength...
Journal Articles
Alloy Digest (1978) 27 (10): SS-356.
Published: 01 October 1978
... LESCALLOY BG42 IIIM-VAR Filing Code: SS-356 Stainless Steel OCTOBER 1978 - DATA ON WORLD WIDE METALS AND ALLOYS Publidml bu LESCALLOY* BG42 VIM-VAR W.&W&~ 1~ (Martensitic, Stainless, High-Speed Steel) Upper Montclair. New Jeroey LESCALLOY BC42 VIM-VAR combines the tempering, hardness and hardness-retention...
Journal Articles
Alloy Digest (1979) 28 (8): SS-367.
Published: 01 August 1979
... STEEL Stainless Steel 01T AUGUST 1979 matid - DATA ON WORLD WIDE METALS AND ALLOYS Publid& by CARPENTER* STAINLESS No. 2 MOLD STEEL w-&y*h IDc. (Martensitic Stainless Steel for Molds; AISI Type 420) Upper Mm~, New Jersey Carpenter Stainless No. 2 Mold Steel is a 13% chromium steel ideally suited...
Journal Articles
Alloy Digest (1983) 32 (7): SS-429.
Published: 01 July 1983
Journal Articles
Alloy Digest (1983) 32 (10): SS-434.
Published: 01 October 1983
... UNILOY 15-5 can be annealed (solution treated) to produce a martensite-austenite mixture and then aged to various levels of hardness and strength. It offers a broad range of mechanical properties. It is consumable remelted to improve cleanliness and mechanical properties. Normally, bars...
Journal Articles
Alloy Digest (1984) 33 (10): SS-452.
Published: 01 October 1984
... - DATA ON WORLD WIDE METALS AND ALLOYS <B Copyright 1980. Engineering Publications. Inc. A41 rights reserved. ISSN: 002-614x Published by Alloy Digest. Inc. Post Office Box 823 Upper Montclair, New Jersey CARPENTER* STAINLESS TYPE 440A (Martensitic Stainless Steel) CARPENTER STAINLESS TYPE 440A is a high...
Journal Articles
Alloy Digest (1985) 34 (1): SS-457.
Published: 01 January 1985
...-614X UNILOY* 13-8 27 Canfield Street Orange. New Jersey 07050 (Precipitation-Hardenable Martensitic Stainless Steel) (201) 761-1090 IJNILOY 13-g has high strength. ductility and toughness in large cross sections in both longitudinal and transverse directions. The alloy has excellent mechanical property...
Journal Articles
Alloy Digest (1964) 13 (2): SS-152.
Published: 01 February 1964
... Pyromet X-12 is a martensitic stainless steel offering high strength at both room temperature and high heat. It is recommended for use in jet engines, steam turbines and aircraft structural parts. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1974) 23 (7): SS-297.
Published: 01 July 1974
... ALLEGHENY STAINLESS AM-363 is an economical, low-carbon martensitic stainless steel. It is higher in strength than annealed austenitic stainless steels but maintains their excellent forming and welding properties. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1974) 23 (8): CI-43.
Published: 01 August 1974
... The CLIMAX 15-3 type alloys are martensitic white irons having an excellent combination of abrasion resistance and thoughness. For specific purposes, the use of four carbon ranges is recommended. These are: (1) Extra High Carbon (XHC), (2) High Carbon (HC), (3) Medium Carbon (MC), and (4) Low...
Journal Articles
Alloy Digest (1974) 23 (9): SS-300.
Published: 01 September 1974
... UNITEMP 1415NW is a high-strength modification of the hardenable, martensitic 12% chromium stainless steel. It has both corrosion and oxidation resistance through its useful temperatures range which is up to about 1050 F. Its applications include compressor blades of gas turbines and turbine discs...
Journal Articles
Alloy Digest (1985) 34 (3): SS-459.
Published: 01 March 1985
... 07050 (201) 761-1090 CARPENTER PROJECT 70* STAINLESS TYPE 416 (Free-Machining Martensitic Stainless Steel) CARPENTER PROJECT 70 STAINLESS TYPE 416 is an improved modification of Carpenter Stainless No. 5. the first free- machining stainless steel ever made. This grade is the product of extensive...
Journal Articles
Alloy Digest (1988) 37 (7): SS-88.
Published: 01 July 1988
... 1 MAY 1999 - DATA ON WORLD WIDE METALS AND ALLOYS 0 copyri#bl I9 m. Alloy upw. Inc. All n#Na r ened. ISSNtOOZ-614X llrcrsbown~t~icd.nurrobruwd /a rpcrfialion 01 Jbd kign Rhkhrd by: Alloy Dipr Inc. 21 camd slreu ona= th AMY omso (201) 621-9161 AISI TYPE 431 (Martensitic Stainless Steel) AISI TYPE...