Alloy Digest (1980) 29 (4): Ti-76.
Published: 01 April 1980
... by many chemicals, seawater and marine atmospheres. It is used for equipment in the chemical and marine industries. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1966) 15 (9): SS-186.
Published: 01 September 1966
... Uranus-50T is a chromium-nickel austenitic stainless steel having high resistance to acids and freedom from intergranular corrosion. It is recommended for the chemical, food and marine industries. This datasheet provides information on composition, physical properties, microstructure, hardness...
Journal Articles
Alloy Digest (1971) 20 (3): SS-252.
Published: 01 March 1971
... ARMCO 22-13-5 provides an unusually good combination of corrosion resistance and strength for an austenitic stainless steel. It is nonmagnetic even after severe cold work. Common applications are in the petrochemical, chemical, pulp and paper, textile, food processing, and marine industries...
Journal Articles
Alloy Digest (1974) 23 (2): Cu-275.
Published: 01 February 1974
... LEADED NICKEL BRONZE 65-20 is a cast copper-nickel zinc-tin alloy to which lead has been added to improve machinability. It is sometimes known as DAIRY BRONZE and has many marine, industrial and ornamental uses. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2018) 67 (4): SA-815.
Published: 01 April 2018
... Strenx 700 OME is a structural steel with a minimum yield strength of 700 MPa (102 ksi) developed for use in demanding load-bearing structures within the offshore and marine industry. Strenx 700 OME exceeds the requirements of S690QL, EN 10 025-6. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1979) 28 (10): Ti-73.
Published: 01 October 1979
.... It has a guaranteed minimum yield strength of 70,000 psi with good ductility and formability. It has excellent resistance to corrosion by marine atmospheres and seawater. It is used ln the aircraft, marine and chemical process@ industries. l RMI is a registered trademark of the RMI Company. Composition...
Journal Articles
Alloy Digest (2020) 69 (4): Ti-165.
Published: 01 April 2020
... Ulbrich Titanium Grade 1 (UNS R50250) is an unalloyed commercially pure titanium. It is one of the softest and the most ductile of the commercially pure grades, and exhibits excellent formability. It has excellent corrosion resistance and is mainly used in marine and chemical industries where...
Journal Articles
Alloy Digest (1985) 34 (5): Al-257.
Published: 01 May 1985
... Resistance: The atmosphere corrosion resistance of GALVA- LUME is much superior to that of galvanized steel. Based on 13-year atmospheric test results, it is estimated that GALVALUME (AZ50) sheet will outlast galvanized by two to four times in marine, industrial and rural atmospheres. When compared...
Journal Articles
Alloy Digest (1981) 30 (1): Ti-81.
Published: 01 January 1981
... characterisitcs, strength and corrosion resistance equal to the parent metal. Corrosion Rasistanca: RbiI 55 is immune to wrrosive attack by salt water and marine atmospheres. It also exhibits exceptional resistance to a broad range of acids, alkaBes. and industrial chemicals Welded fabrica- tions of this metal...
Journal Articles
Alloy Digest (1979) 28 (2): Cu-366.
Published: 01 February 1979
... to industrial, rural and marine atmospheres; also to salt and fresh water im- mersion, in both stagnant and moving water. It has fair resistance to weak bases and poor resistance to strong acids and bases. Its resistance to petroleum products, alcohols, and dry gases is good. Specification Equivalents: CDA...
Journal Articles
Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... temperatures. It can be hot upset, forged, deep drawn, impact extruded and welded. Applications include highly corrosive environments in agrichemical, petrochemical, pulp and paper, oil and gas, marine and other chemical process industries. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1989) 38 (5): Ti-92.
Published: 01 May 1989
... Titanium Development Association commercially pure wrought titanium, Grade 4 is used in equipment where resistance to corrosion in chemical, marine and other industries is required. At a guaranteed 80,000 psi minimum mill annealed tensile strength, titanium Grade 4 is the strongest...
Journal Articles
Alloy Digest (1999) 48 (7): Ni-555.
Published: 01 July 1999
... Crucible P/M N625 is a powder metallurgical nickel-base alloy with excellent corrosion resistance, high strength, chemical homogeneity, and thermal stability. Applications include use for highly corrosive situations in the marine, nuclear power, pulp and paper, and chemical process industries...
Journal Articles
Alloy Digest (2002) 51 (6): SS-786.
Published: 01 June 2002
... 304, 316, and 317L stainless steels. Its many uses include marine scrubbers, desalination equipment, sulfuric acid production, wet phosphoric acid production, mild sour gas wells, urea production, and applications in the pulp and paper industry. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2002) 51 (10): SS-865.
Published: 01 October 2002
... valuable property is high creep strength at elevated temperatures. The alloy has extensive use in marine exterior trim, chemical- and food-process equipment, pharmaceutical and textile-finishing equipment, and in the pulp and paper industry. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1970) 19 (9): SS-243.
Published: 01 September 1970
... ALLEGHENY Type 216 is an austenitic stainless steel offering superior corrosion resistance, excellent strength properties, and low magnetic permeability. It finds applications in marine engineering, aerospace, and the process industries. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2009) 58 (8): SS-1041.
Published: 01 August 2009
... (typically up to 600 MPa yield strength) and good ductility with outstanding corrosion resistance to marine environments and a wide, diverse range of industrial media. Ferrinox and Aminox are registered trade marks of Advance Metals International Chemical Composition, wt (Typical Analysis) Carbon 0.04 max...
Journal Articles
Alloy Digest (2015) 64 (11): Cu-844.
Published: 01 November 2015
... Nibron Special is an extra high-strength nickel bronze that is corrosion resistant in both marine environments and industrial media. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion...
Journal Articles
Alloy Digest (1982) 31 (9): SS-414.
Published: 01 September 1982
... severe cold work. Its many uses include cables, fasteners, pumps, valves, marine hardware and springs. *CRUCIBLE is a registered trademark of Colt Industries. Composition: Carbon Manganese Phosphorus Sulfur Silicon Chromium Nickel Molybdenum Columbium Vanadium Nitrogen Iron 0.03 max. 4.0-6.0 O.CMO max...
Journal Articles
Alloy Digest (2021) 70 (5): Ti-178.
Published: 01 May 2021
... Arcam Ti6Al4V ELI (Grade 23) is a titanium-based alloy that is used for the production of additively manufactured components using electron beam melting (EBM). This alloy offers the best all-round performance for a variety of weight reduction applications in aerospace, automotive, and marine...