1-20 of 818

Search Results for marine applications

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1977) 26 (4): SS-338.
Published: 01 April 1977
... by AQUAMET 22 El&WiDgAllopsDigcst.Ioc (Material for Boat Shafting and Other Marine Applications) Uppt Monrdrir. New Jmcr AQUAMET 22 is an austenitic stainless steel with an outstanding combination of strength. toughness and corrosion resistance. Its corrosion rt sistance is equal to or better than any other...
Journal Articles
Alloy Digest (1995) 44 (6): Cu-601.
Published: 01 June 1995
... HIDURON alloy 191 was developed for marine applications where both a combination of strength and good corrosion/ impingement resistance is needed. It finds applications in shafts, fasteners and valve stems. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1961) 10 (9): Al-107.
Published: 01 September 1961
... APEX 400 is a 4% magnesium type aluminum casting alloy having high corrosion resistance. It is not heat treatable. It is recommended for marine applications and food processing equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1964) 13 (11): Al-141.
Published: 01 November 1964
... Aluminum 214 is a non-heat treatable alloy containing 4% magnesium and characterized by excellent corrosion resistance and excellent weldability. It is recommended for marine applications and food processing equipment. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2023) 72 (1): Al-493.
Published: 01 January 2023
... for marine applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: Al-493. Producer or source: Austral Wright Metals. Producer...
Journal Articles
Alloy Digest (1987) 36 (4): Al-280.
Published: 01 April 1987
...-resistant alloys elasticity fatigue properties food-processing equipment hardness heat treatability high-temperature alloys joinability machinability marine applications physical properties shear strength tensile properties UNS A05140 weldability UNS A05140 DOI: 10.31399/asm.ad.al0280...
Journal Articles
Alloy Digest (1975) 24 (12): Al-220.
Published: 01 December 1975
... ALUMINUM B514.0 is an aluminum sand casting alloy recommended where excellent resistance to corrosion and tarnishing are required. It has moderate strength and pressure tightness. Cooking utensils and marine applications are among its uses. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1982) 31 (2): Al-236.
Published: 01 February 1982
... ALUMINUM 514.0 is a non-heat-treatable alloy containing nominally 4% magnesium. It has relatively low strength and hardness. It is characterized by excellent weldability and excellent resistance to corrosion. Aluminum 514.0 is recommended for food-processing equipment and marine applications...
Journal Articles
Alloy Digest (1982) 31 (5): Cu-436.
Published: 01 May 1982
... MUELLER Alloy 4820 is a copper-zinc alloy (brass) containing a medium amount of lead (0.4-1.0%) to make it free machining. It has a good combination of strength and ductility. Its good resistance to corrosion by salt water makes it suitable for marine applications. It also is used for screw...
Journal Articles
Alloy Digest (2014) 63 (2): SS-1168.
Published: 01 February 2014
... Sandvik SanRig 80, an austenitic stainless steel, has high fatigue and tensile strength for marine applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2010) 59 (12): Co-120.
Published: 01 December 2010
... obtain ultrahigh tensile strengths 2068 MPa (300 ksi) through work hardening and aging, and has good toughness and ductility. Applications include electrical components, springs, and instrument parts in medical, chemical, food processing and marine environments. HPM® MP35N-LTi (High Strength Cobalt Alloy...
Journal Articles
Alloy Digest (1986) 35 (2): Al-265.
Published: 01 February 1986
... ALUMINUM 513.0 is an aluminum-magnesium-zinc permanent-mold casting alloy. It cannot be hardened nor strengthened by any thermal treatment and is characterized by moderate strength and ductility. It is recommended for such applications as chemical-plant equipment, food handling and marine hardware...
Journal Articles
Alloy Digest (1987) 36 (1): Ni-51.
Published: 01 January 1987
... UDIMET 700 is a wrought nickel-base alloy produced by vacuum-induction melting and further refined by vacuum-arc remelting. It has excellent mechanical properties at high temperatures. Among its applications are blades for aircraft, marine and land-based gas turbines and rotor discs...
Journal Articles
Alloy Digest (1985) 34 (7): Ni-317.
Published: 01 July 1985
... temperatures. It can be hot upset, forged, deep drawn, impact extruded and welded. Applications include highly corrosive environments in agrichemical, petrochemical, pulp and paper, oil and gas, marine and other chemical process industries. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1986) 35 (12): Cu-518.
Published: 01 December 1986
...: Mueller Alloy 4851 is a high-leaded naval brass that has somewhat greater strength, ductility and corrosion resistance than Free-Cutting Brass. It has good resistance to salt water corrosion and is used in marine applications. It can be hot worked readily by press- forging, extrusion or rolling but has...
Journal Articles
Alloy Digest (1961) 10 (12): Al-109.
Published: 01 December 1961
... International® 1996 1996 ASM International Alcan A320 architectural applications castability chemical composition compressive strength corrosion-resistant alloys elasticity fatigue properties hardness heat treatability joinability machinability marine applications ornamental application...
Journal Articles
Alloy Digest (2020) 69 (9): Al-468.
Published: 01 September 2020
... applications. The principal application for Atlas 5083 is in marine environments. The magnesium content in Atlas 5083 is more than 3.5%; therefore, this alloy is susceptible to stress-corrosion cracking, which limits its application temperature to below 65 °C (150 °F) and also limits the amount of cold work...
Journal Articles
Alloy Digest (1961) 10 (12): Cu-111.
Published: 01 December 1961
... 1996 1996 ASM International Bridgeport alloy 77 chemical composition condenser tubes corrosion-resistant alloys dezincification elasticity hardness heat exchanger tubes heat treatability joinability machinability marine applications physical properties tensile properties...
Journal Articles
Alloy Digest (2012) 61 (8): Cu-810.
Published: 01 August 2012
.... Applications: This alloy is widely used in marine applications, seawater piping, desalination plants, power plants, and in condensers and evaporators in petrochemical plants. The alloy was originally developed as a cost-effective alternative to higher nickel alloys such as Electralloy s EC71500. The addition...
Journal Articles
Alloy Digest (1979) 28 (2): Cu-366.
Published: 01 February 1979
... MUELLER Alloy 4640 (formerly MBCo Alloy 203) is a classic marine alloy known as Naval Brass. It contains nominally 0.75% tin which has made it the most widely used marine alloy. It is suitable for both salt and fresh water applications. This datasheet provides information on composition, physical...