Alloy Digest (2023) 72 (5): SS-1358.
Published: 01 May 2023
... Uddeholm Corrax for AM is a stainless steel developed for additive manufacturing. Its unique set of properties makes it a choice for tools where superior corrosion resistance combined with high hardness is needed. These properties make it suitable for tools for plastic molds, including...
Journal Articles
Alloy Digest (2006) 55 (10): Al-401.
Published: 01 October 2006
... Alcoa extrusion alloy 2026 was developed as an improvement over 2024 and 2224 extrusions in aerospace structural applications where the governing selection criteria are high damage tolerance, good fatigue resistance, and a high degree of manufacturability. In addition to improved damage tolerance...
Journal Articles
Alloy Digest (1981) 30 (5): TS-382.
Published: 01 May 1981
... CARPENTER STAR-ZENITH is an 18% tungsten-4% chromium-1% vanadium type of high-speed steel that, because of the practice used in its manufacture, has improved toughness to provide it with a stronger, keener cutting edge than is furnished by conventional steel manufacturing practice. For this reason...
Journal Articles
Alloy Digest (1985) 34 (12): Cu-504.
Published: 01 December 1985
... Copper Alloy No. C81400 is a precipitation-hardenable alloy of moderate hardness and strength. Its common name is beryllium-modified chromium copper and a previous trade name was Beryllium Copper 70C. Because of its beryllium content, its manufacture may present a health hazard. Typical uses...
Journal Articles
Alloy Digest (1986) 35 (11): TS-466.
Published: 01 November 1986
... COLUMBIA SPECIAL is the manufacturer's highest quality best grade of water-hardening tool steel. It contains small amounts of chromium and vanadium. Its manufacture is controlled closely to insure uniform predictable hardenability. When brine quenched it develops a uniform high-hardness case...
Journal Articles
Alloy Digest (2022) 71 (8): SS-1350.
Published: 01 August 2022
... Atlas 302HQ is a chromium-nickel-copper austenitic stainless steel. It is a specialized wire grade with very wide usage for the manufacture of stainless steel fasteners. The inclusion of 3% copper in the composition reduces the cold work hardening rate substantially compared to type 304 austenitic...
Journal Articles
Alloy Digest (2012) 61 (9): Al-439.
Published: 01 September 2012
... Alcoa has developed this Al-Li alloy with the benefits of excellent corrosion resistance, a good spectrum of fatigue crack growth performance, a good strength and toughness combination, and compatibility with standard manufacturing techniques for aircraft internal structures. This datasheet...
Journal Articles
Alloy Digest (2013) 62 (2): TS-714.
Published: 01 February 2013
... Böhler (or Boehler) S601 is a modified M2 and is used for the manufacture of cutting tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-714. Producer...
Journal Articles
Alloy Digest (2013) 62 (5): Nd-4.
Published: 01 May 2013
... NEOQUENCH-P GRADE NP-7L is one of a series of isotropic polymer bonded magnets based on Nd-Fe-B. The raw material powder is manufactured by rapid quenching of prescribed alloys into nanocrystalline flakes that are subsequently annealed for optimum magnetic properties. NP-7L is made by compression...
Journal Articles
Alloy Digest (2014) 63 (5): SA-700.
Published: 01 May 2014
... Mecasteel 75 (minimum yield strength 75 ksi) is a high-strength prehardened steel that can be used in substitution for conventional steels, such as AISI 4130, in the manufacture of massive steel components such as machines, hydraulic systems, and pumps. This datasheet provides information...
Journal Articles
Alloy Digest (2014) 63 (10): SS-1185.
Published: 01 October 2014
... Carpenter CTS BDZ1 alloy is a martensitic steel chemically balanced and processed to provide a uniform, fine carbide structure. This structure has been suitable for the manufacture of thin sections and fine blanking operations. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2019) 68 (10): TS-777.
Published: 01 October 2019
... Cryodur 2833 is a wear-resistant water-hardening steel with resistance to overheating. Applications include cold heading dies; first and finish upsetting punches; cold stamps; dies for the manufacturing of screws, rivets, and bolts; and compression pistons. This datasheet provides information...
Journal Articles
Alloy Digest (2016) 65 (2): SA-742.
Published: 01 February 2016
... Induction hardened Cromax IH 482 is based on a medium carbon, microalloyed steel, which is characterized by high strength in the as-rolled condition, i.e., without heat treatment. The alloy is used for the manufacture of piston rods, pistons, and eyes for hydraulic cylinders. This datasheet...
Journal Articles
Alloy Digest (2018) 67 (2): SA-812.
Published: 01 February 2018
... FERRO-TITANIT C-SPEZIAL is one of a series of metal-matrix composites manufactured by a powder metallurgy process. Ferro-Titanit C-SPEZIAL contains 33% titanium carbide, one of the hardest and most resistant carbides. Because of its high wear resistance and low tendency towards cold welding, Ferro...
Journal Articles
Alloy Digest (2018) 67 (3): Ti-160.
Published: 01 March 2018
... AncorTi is a gas atomized spherical titanium powder for applications in additive manufacturing. The data sheet covers both commercial pure titanium and Ti6Al4V. This datasheet provides information on composition. Filing Code: Ti-160. Producer or source: Hoeganaes Corporation. Producer or Source...
Journal Articles
Alloy Digest (2018) 67 (3): SS-1281.
Published: 01 March 2018
... Ferro-Titanit WFN is one of a series of metal-matrix composites manufactured by a powder metallurgy process and is a range of carbide-alloyed materials from Deutsche Edelstahlwerke. The WFN grade contains 33 wt.% titanium carbide. Because of its high wear resistance and low tendency toward cold...
Journal Articles
Alloy Digest (2018) 67 (4): Ti-161.
Published: 01 April 2018
... AncorTi is a gas atomized spherical titanium powder for applications in additive manufacturing. This datasheet provides information on composition. It also includes information on powder metal forms. Filing Code: Ti-161. Producer or source: Hoeganaes Corporation. Producer or Source: Hoeganaes...
Journal Articles
Alloy Digest (2018) 67 (4): SS-1283.
Published: 01 April 2018
... Ferro-Titanit Nikro 128 is one of a series of metal-matrix composites manufactured by a powder metallurgy process and is a range of carbide-alloyed materials from Deutsche Edelstahlwerke. The matrix structure consists of a highly tough, age-hardenable nickel martensite. The chromium content...
Journal Articles
Alloy Digest (2018) 67 (5): Fe-168.
Published: 01 May 2018
... Ferro-Titanit Nikro 143 is one of a series of metal-matrix composites manufactured by a powder metallurgy process and is a range of carbide-alloyed materials from Deutsche Edelstahlwerke. The Nikro 143 grade is an iron-base alloy containing 30 wt.% titanium carbide. Because of its high wear...
Journal Articles
Alloy Digest (2018) 67 (6): SS-1290.
Published: 01 June 2018
... Ferro-Titanit S is one of a series of metal-matrix composites manufactured by a powder metallurgy process and is a range of carbide-alloyed materials. This datasheet provides information on composition, physical properties, hardness, and compressive, shear, bearing, and bend strength. It also...