1-20 of 185 Search Results for

manganese bronze

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2008) 57 (12): Cu-763.
Published: 01 December 2008
... Ansonia alloy C67500 and C67600 are manganese bronze and manganese leaded bronze that are high strength; the latter being the machinable equivalent. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1958) 7 (1): Cu-58.
Published: 01 January 1958
... MANGANESE BRONZE is a copper-zinc alloy having excellent combination of high strength and good corrosion resistance in fresh and salt water. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength. It also includes...
Journal Articles
Alloy Digest (1966) 15 (4): Cu-163.
Published: 01 April 1966
... PROMET BRONZE No. 100 is a manganese bronze containing alpha and beta phases and offering an excellent combination of mechanical properties. It is recommended for cast gears, bearings, propellers and marine hardware. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2011) 60 (8): Cu-801.
Published: 01 August 2011
... Wieland-FX9 is a high-manganese bronze alloy that has good strength and is available in numerous cold work tempers related to its minimum tensile strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1977) 26 (11): Cu-344.
Published: 01 November 1977
... NOVEMBER 1977 - DATA ON WORLD WIDE METALS AND ALLOYS - by wyg%&y$h% IE Copper Alloy No. 865 UpperMontdai~NewJersey (Cast Low-Tensile Manganese Bronze) Copper Alloy No. 865 is a copper-zinc-aluminum-iron-manganese alloy that is classified as high-strength yellow brass. It has a tensile strength about 20,000...
Journal Articles
Alloy Digest (1978) 27 (5): Cu-353.
Published: 01 May 1978
...: cu-353 Copper Alloy MAY 1978 - DATA ON WORLD WIDE METALS AND ALLOYS BELMONT* Alloy 4582 (Jewelers Manganese Bronze for Castings) BELMONT Ahoy 4582 is a proprietary alloy developed to meet the special needs of jewelers for a base-metal alloy suitable for casting centrifugally in refractory molds...
Journal Articles
Alloy Digest (1975) 24 (11): Cu-303.
Published: 01 November 1975
... ATLANTIC 8A Alloy is a cast manganese bronze offering an excellent combination of mechanical properties and resistance to corrosion in fresh and sea water. It is used for applications such as gears, marine hardware and waveguide components. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1957) 6 (12): Cu-57.
Published: 01 December 1957
... UMEN ALLOY 9 is a manganese bronze having excellent combination of strength and corrosion resistance in fresh and sea water. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness...
Journal Articles
Alloy Digest (1979) 28 (11): Cu-383.
Published: 01 November 1979
... AMPCOLOY 66 is a copper-zinc-aluminum-manganese-iron alloy; it is classified as a high-strength yellow brass (manganese bronze). It has an excellent combination of strength and ductility along with good resistance to corrosion. Its many uses include bearings, gears and marine hardware...
Journal Articles
Alloy Digest (1979) 28 (11): Cu-384.
Published: 01 November 1979
... MUELLER Alloy 6750 (formerly MBCo 241A) is a moderately high-strength wrought manganese bronze possessing good torsional properties and general corrosion resistance. The material possesses excellent hot-working properties and is readily joined by either soldering, brazing or oxyacetylene welding...
Journal Articles
Alloy Digest (1971) 20 (3): Cu-228.
Published: 01 March 1971
... MUELLER ALLOY 6700 is a high-strength manganese bronze which conforms to CDA No. 670. A series of numbers is used to indicate the temper, i.e. 6700 is soft temper, 6701 is half hard and 6702 is hard. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1971) 20 (11): Cu-244.
Published: 01 November 1971
... Jersey COPPER ALLOY No. 675 (Manganese Bronze) COPPER ALLQY No. 675 is a copper-zinc ahoy having excellent mechanical properties and good corrosion resistance. Composition: Copper 57.0-60.0 Iron 0.8-2.0 Tin 0.5-l .5 Manganese 0.05-0.50 Lead 0.20 max Aluminum 0.25 max Total other impurities 0.10 max zinc...
Journal Articles
Alloy Digest (1979) 28 (1): Cu-365.
Published: 01 January 1979
... - DATA ON WORLD WIDE MEfAl!i AND ALLOYS Copper Alloy No. 862 (Cast Medium-Tensile Manganese Bronze) Uppa Montclair, New Jersey Copper Alloy No. 862 is a copper-zinc-aluminum-manganese-iron alloy; aluminum is the principal strengthening element. It is classified as a high-strength yellow brass; its...
Journal Articles
Alloy Digest (1979) 28 (3): Cu-369.
Published: 01 March 1979
... AMPCOLOY 62 is a cast copper-base alloy known as low-tensile manganese bronze. Despite the fact that it is at the low-strength end of the manganese bronzes, it has a tensile strength about 20,000 psi greater than that of the corresponding copper-zinc alloys; therefore, it is often classified...
Journal Articles
Alloy Digest (1980) 29 (6): Cu-396.
Published: 01 June 1980
... Upper Montdair. Now Jemy AMPCOLOY 64 (Cast Medium-Strength Manganese Bronze) AMPCOLOY 64 is a casting alloy that is frequently classified as a high-strength yellow brass; its typical tensile strength is 95,000 psi in the as-cast condition. This alloy has an excellent combination of strength, ductility...
Journal Articles
Alloy Digest (1962) 11 (6): Cu-118.
Published: 01 June 1962
... LUMEN ALLOY 20 is a high strength manganese bronze having good wear and fatigue resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1962) 11 (12): Cu-123.
Published: 01 December 1962
... REVERE No. 454 is a manganese bronze having high tensile strength and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining...
Journal Articles
Alloy Digest (1964) 13 (4): Cu-140.
Published: 01 April 1964
... Ampcoloy 668 Alloy is a leaded manganese bronze recommended for high quality screw machine work. It is a high strength, free-machining alloy that has good hot working characteristics. This datasheet provides information on composition, physical properties, and elasticity. It also includes...
Journal Articles
Alloy Digest (1965) 14 (2): Cu-148.
Published: 01 February 1965
... Bohnolloy R-57 is a very strong manganese bronze recommended for parts which are subjected to heavy loads. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1986) 35 (5): Cu-510.
Published: 01 May 1986
... Alloy ( oP)rlpht IYXh. All I)qx\l. Inc. I right, rcrcr\cd. ISSh,l\: Ib/,i \111111.ll r ,I/. 10 /u. c,, ,lW %/WI 1/h ,111 Cl,, 0, lOl I Alloy Digest. Inc. 27 Canfield Street Orange. New Jersey 07050 (201) 761-1090 Copper Alloy No. C86100 (Cast Medium-Tensile Manganese Bronze) Copper Alloy No. C86100...