1-20 of 123 Search Results for

malleability

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1968) 17 (2): CI-35.
Published: 01 February 1968
... PROMAL is a specially processed pearlitic malleable iron recommended for highly stressed applications. It has high strength and good toughness suitable for gears, power shovels, conveyor chains and diesel engine drive pulleys. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1954) 3 (2): CI-6.
Published: 01 February 1954
... BELMALLOY is a high grade pearlitic malleable iron providing rigidity and shock resistance to high torque loads. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1955) 4 (4): CI-10.
Published: 01 April 1955
... grades. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on casting, heat treating, machining, and joining. Filing Code: CI-10. Producer or source: Eastern Malleable...
Journal Articles
Alloy Digest (1956) 5 (11): CI-17.
Published: 01 November 1956
... BISBO is a pearlitic malleable iron readily cast in thick sections with consistently high mechanical properties. It has high yield strength, excellent wear resistance, and adaptability to selective hardening. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1958) 7 (11): CI-23.
Published: 01 November 1958
... MALLEABLE IRON is a tough, malleable, shock-resisting cast iron. It has good corrosion resistance and excellent stability at elevated temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength...
Journal Articles
Alloy Digest (1959) 8 (3): CI-26.
Published: 01 March 1959
... PEARLITIC MALLEABLE IRON is a high strength cast iron recommended for dependable service, strength and machinability in highly stressed parts at work in mobile and stationary mechanisms. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1978) 27 (7): In-1.
Published: 01 July 1978
... INDALLOY No. 4 is the metallic element indium. It is a very versatile, malleable and soft metal; it is softer even than lead. Indium remains malleable at temperatures approaching absolute zero; therefore, it is an excellent for a variety of applications including gaskets and seals. It is a useful...
Journal Articles
Alloy Digest (1998) 47 (3): Ni-538.
Published: 01 March 1998
... NI-ROD FC 55 cored wire is used for flux-cored-arc and submerged-arc welding of gray, malleable, and ductile cast irons. It is also used for surfacing of cast irons and for joining cast irons to various wrought materials such as carbon steels and low-alloy steels. The cored wire combines...
Journal Articles
Alloy Digest (1998) 47 (5): SS-718.
Published: 01 May 1998
... UGIMA 4301 (formerly known as UGIMA 304) is an austenitic stainless steel produced by special steelmaking techniques that produce a steel with inclusions of malleable oxides, which have a low melting point and a controlled composition. The presence of the inclusions lubricates the metal-tool...
Journal Articles
Alloy Digest (1998) 47 (11): SS-734.
Published: 01 November 1998
... UGIMA 4401 (UGIMA 316) is identical to UGINE 4401 (AISI 316) in analysis, corrosion resistance, mechanical properties, and forging and welding abilities but dissimilar in machinability. A specific melting process creates inclusions (malleable oxides with a low melting point), which improve...
Journal Articles
Alloy Digest (1998) 47 (11): SS-722.
Published: 01 November 1998
... UGIMA 4307 (also known as UGIMA 304L) is an austenitic stainless steel produced by special steelmaking techniques that produce a steel with inclusions of malleable oxides, a low melting point, and a controlled composition. The presence of the inclusions lubricates the metal-tool interface during...
Journal Articles
Alloy Digest (1998) 47 (12): SS-735.
Published: 01 December 1998
... UGIMA 4404 (UGIMA 316L) is identical to UGINE 4404 (AISI 316L) in analysis, corrosion resistance, mechanical properties, and forging and welding ability, but not with respect to machinability. A specific melting process creates inclusions of malleable oxides with a low melting point...
Journal Articles
Alloy Digest (1999) 48 (9): SS-760.
Published: 01 September 1999
... of calcium by the UGIMA process. This steelmaking technique produces malleable oxide inclusions with a low melting point. The inclusions then lubricate the metal-tool interface in machining and improve productivity. This datasheet provides information on composition. It also includes information on corrosion...
Journal Articles
Alloy Digest (2002) 51 (10): Cu-691.
Published: 01 October 2002
... Carlson Alloy 70 30 Cu Ni is strong and ductile and has excellent cold-forming properties. Malleability approaches that of copper, and the alloy does not work harden rapidly. It is readily weldable by all of the arc processes and by resistance arc welding and can be brazed and soldered. Alloy 70...
Journal Articles
Alloy Digest (1969) 18 (7): Cu-202.
Published: 01 July 1969
... COPPER Alloy No. 240 is a copper-zinc alloy having high ductility and malleability combined with good corrosion resistance and relative freedom from intergranular corrosion and embrittlement. It is recommended for pump lines, flexible hose and ornamental work. This datasheet provides information...
Journal Articles
Alloy Digest (1969) 18 (12): Cu-209.
Published: 01 December 1969
... Cunife-II is a permanent magnet alloy recommended where magnets must be formed or machined, as this material is ductile, malleable, and machinable after heat treatment. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1961) 10 (5): Cu-100.
Published: 01 May 1961
... REVERE No. 533 is an 18% nickel silver alloy having high ductility, malleability and resistance to corrosion. It is recommended for deep drawing applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1961) 10 (6): Cu-101.
Published: 01 June 1961
... CUNICO is a permanent magnet alloy of copper, nickel, and cobalt. It is ductile and malleable. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu...
Journal Articles
Alloy Digest (1961) 10 (8): Cu-105.
Published: 01 August 1961
... CUNIFE-I is a permanent magnet alloy recommended where magnets must be formed or machined, as this material is ductile, malleable and machinable after heat treatment. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1962) 11 (1): Al-110.
Published: 01 January 1962
... Adaptaloy is a malleable aluminum casting alloy providing high ductility and toughness. It is recommended only for castings requiring moderate strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...