Skip Nav Destination
Close Modal
Search Results for
magnetic shielding
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 317 Search Results for
magnetic shielding
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1973) 22 (6): Ni-191.
Published: 01 June 1973
... MU GUARD 80 is a nickel-iron-molybdenum alloy. It is furnished in strip and foil form and provides optimum initial and maximum permeabilities for electromagnetic shielding applications. It is a high purity, soft magnetic alloy produced by powder metallurgy techniques. This datasheet provides...
Abstract
View article
PDF
MU GUARD 80 is a nickel-iron-molybdenum alloy. It is furnished in strip and foil form and provides optimum initial and maximum permeabilities for electromagnetic shielding applications. It is a high purity, soft magnetic alloy produced by powder metallurgy techniques. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-191. Producer or source: Spang Industries Inc..
Journal Articles
Alloy Digest (1975) 24 (6): Fe-52.
Published: 01 June 1975
.... It is excellent for rotor and stator laminations, and is also a very effective magnetic shielding material. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating...
Abstract
View article
PDF
ALLOY 48 is a vacuum-melted, 48% nickel-iron alloy designed for high permeability, and low core losses. It is ideal in applications requiring efficient magnetic core materials, such as audio and instrument transformers, instrument relays, and many other communication equipment devices. It is excellent for rotor and stator laminations, and is also a very effective magnetic shielding material. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Fe-52. Producer or source: Magnetics Specialty Metals Division. See also Alloy Digest Fe-96, April 1992.
Journal Articles
Alloy Digest (1972) 21 (11): Ni-181.
Published: 01 November 1972
... BLENDALLOY 25-7904 is an 80% nickel-15% iron-5% molybdenum alloy having very high permeability and low coercive force for magnetic cores in such applications as transformer laminations, sensitive magnetic amplifiers and magnetic shielding. This datasheet provides information on composition...
Abstract
View article
PDF
BLENDALLOY 25-7904 is an 80% nickel-15% iron-5% molybdenum alloy having very high permeability and low coercive force for magnetic cores in such applications as transformer laminations, sensitive magnetic amplifiers and magnetic shielding. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-181. Producer or source: Spang Industries Inc..
Journal Articles
Alloy Digest (1976) 25 (11): Ni-235.
Published: 01 November 1976
... are typically 0.038-mm thick and 1.78-mm wide. Continuous lengths of several hundred meters can be produced readily. Magnetic Shielding: From a great deal of preliminary work, magnetic shielding was selected as the specific application which would take greatest advantage of the unique magnetic and mechanical...
Abstract
View article
PDF
METGLAS Alloy 2826 (Fe40Ni40P14B6) is a ferromagnetic, high permeability, nickel-iron metallic glass which, when appropriately annealed, yields a material similar to the higher nickel containing permalloys in magnetic properties. Alloy 2826 is a single phase, opaque metallic material with a glass-like structure obtained by a very rapid quench from the liquid state. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on forming and heat treating. Filing Code: Ni-235. Producer or source: Allied Chemical Corporation.
Journal Articles
Alloy Digest (1993) 42 (4): Fe-99.
Published: 01 April 1993
... Method Fig. 3 - Magnetic Shielding Performance I (bzmm) pmax kc Hc F 0 0.6 - 2 5 0.4 f ii s 0.2 - 1.0 . 0.0 iz . 0.6 - 2 * 0.4 5 ; 6 * 0.2 9OWOO 1106 700 o- 0 000 900 1000 1106 Annrallng tbmprrrturr ( C) Annealing tamprrnturr ( C) Fig. 4 - Influence of annealing temperature on the dc magnetic properties...
Abstract
View article
PDF
Ferroperm is a soft magnetic alloy that contains 1% aluminum. This addition of aluminum combined with high-temperature annealing increases permeability and reduces coercivity without decreasing the high-saturation magnetization of pure iron. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming. Filing Code: FE-99. Producer or source: NKK Corporation.
Journal Articles
Alloy Digest (2001) 50 (1): Fe-4.
Published: 01 January 2001
... latitude of good magnetic properties to control hysteresis loop shape via crystallization modes. Applica- tions for this grade include electromechanical relay cores, very low current holding magnets for natural gas safety valves, and magnetic shielding used in multiple-wall shielding to produce very low...
Abstract
View article
PDF
AL 4750 is a low-expansion, high-permeability iron-nickel alloy. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: FE-4. Producer or source: Allegheny Ludlum Corporation. Originally published as Allegheny 4750, February 1954, revised January 2001.
Journal Articles
Alloy Digest (1991) 40 (12): Ni-398.
Published: 01 December 1991
...: MUMETAL is a very high permeability soft magnetic alloy. When tested under direct current conditions at a flux density of 40 gauss, the guaranteed minimum DC perme- ability is 60000 for shielding gages, properly annealed. The alloy has good forming and deep drawing characteristics. Width 15-16 1.16 1.16...
Abstract
View article
PDF
MUMETAL is a very high permeability soft magnetic alloy. (See also Alloy Digest Ni-25, April 1956.) This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating. Filing Code: Ni-398. Producer or source: Spang Specialty Metals.
Journal Articles
Alloy Digest (1995) 44 (10): Ni-488.
Published: 01 October 1995
... requirements to a minimum. It is used in transformers, inductors, magnetic amplifi- ers, switching devices, magnetic shields, tape recorder heads and memory storage devices. Forms Available: Sheet, strip Producer: INCO Alloys International, Inc. Huntington, WV 25720 304-526-5000 0 4.0 8.0 1 Magne(iring Fone...
Abstract
View article
PDF
NILOMAG ALLOY 77 is a 77 Ni soft magnetic alloy with a high level of initial permeability. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating. Filing Code: Ni-488. Producer or source: Inco Alloys International Inc.
Journal Articles
Alloy Digest (1997) 46 (12): Ni-133.
Published: 01 December 1997
... Hipernom is a high nickel-iron alloy that is magnetically soft and has high minimum and maximum magnetic permeabilities. It is used in many applications including shielding, saturable reactors, transformers, and relays. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
Hipernom is a high nickel-iron alloy that is magnetically soft and has high minimum and maximum magnetic permeabilities. It is used in many applications including shielding, saturable reactors, transformers, and relays. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ni-133. Producer or source: Carpenter. Originally published as Hipernom, May 1968, revised December 1997.
Journal Articles
Alloy Digest (1976) 25 (1): Ni-223.
Published: 01 January 1976
... Round Permalloy 80 is an 80% nickel-iron-molybdenum alloy that provides very high initial and maximum magnetic permeabilities and minimal core losses at low field strengths. This vacuum-melted product also offers the advantages of small size and weight in magnetic core and shielding materials...
Abstract
View article
PDF
Round Permalloy 80 is an 80% nickel-iron-molybdenum alloy that provides very high initial and maximum magnetic permeabilities and minimal core losses at low field strengths. This vacuum-melted product also offers the advantages of small size and weight in magnetic core and shielding materials for numerous applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-223. Producer or source: Spang Industries Inc..
Journal Articles
Alloy Digest (2001) 50 (12): Fe-123.
Published: 01 December 2001
... 2190 °F) depending on the application and the required magnetic and mechanical properties, with an annealing time of 2 6 h. The finished parts should then be cooled to below 500 °C (930 °F) under shielding gas. If surface oxidation is to be avoided, the parts should not be removed from the shielding...
Abstract
View article
PDF
Magnifer 4008 is a soft-magnetic alloy with 40% Ni and 8% Cr. The alloy has high permeability values and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming and heat treating. Filing Code: FE-123. Producer or source: Krupp VDM.
Journal Articles
Alloy Digest (1983) 32 (11): Ni-294.
Published: 01 November 1983
... MAGNIFER 75 is a soft magnetic nickel-iron alloy containing about 5% copper and 2% chromium. It offers very high permeability, very low coercive force and minimum hysteresis loss. It is used primarily for transformers, tape-wound toroids, laminations, shielding and relay parts. This datasheet...
Abstract
View article
PDF
MAGNIFER 75 is a soft magnetic nickel-iron alloy containing about 5% copper and 2% chromium. It offers very high permeability, very low coercive force and minimum hysteresis loss. It is used primarily for transformers, tape-wound toroids, laminations, shielding and relay parts. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-294. Producer or source: Vereingte Deutsche Metallwerke AG.
Journal Articles
Alloy Digest (1984) 33 (2): Ni-291.
Published: 01 February 1984
... MAGNIFER 7904 is a soft magnetic nickel-iron alloy containing about 5% molybdenum. It offers extremely high permeability, very low coercive force and minimum hysteresis loss. It is used primarily for transformers, tape-wound troids, laminations, shielding and relay parts. This datasheet provides...
Abstract
View article
PDF
MAGNIFER 7904 is a soft magnetic nickel-iron alloy containing about 5% molybdenum. It offers extremely high permeability, very low coercive force and minimum hysteresis loss. It is used primarily for transformers, tape-wound troids, laminations, shielding and relay parts. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-291. Producer or source: Vereingte Deutsche Metallwerke AG. Originally published September 1983, revised February 1984.
Journal Articles
Alloy Digest (1984) 33 (12): Ni-307.
Published: 01 December 1984
... INCO-WELD B is a nickel-base alloy developed for shielded metal-arc welding of nickel steels for cryogenic applications. It is similar to INCO-WELD A Electrode (Alloy Digest Ni-305, November 1984) except that it is designed for use with alternating current to minimize magnetic arc blow. It can...
Abstract
View article
PDF
INCO-WELD B is a nickel-base alloy developed for shielded metal-arc welding of nickel steels for cryogenic applications. It is similar to INCO-WELD A Electrode (Alloy Digest Ni-305, November 1984) except that it is designed for use with alternating current to minimize magnetic arc blow. It can be operated in all welding positions. This datasheet provides information on composition and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-307. Producer or source: Huntington Alloys.
Journal Articles
Alloy Digest (1994) 43 (3): Fe-106.
Published: 01 March 1994
... excitation VA Curves. Application: Due to such distinct magnetic characteristics. the 6.5% silicon steel sheet can be widely used in various electric devices, elec- tronic parts and shielding materials, offering reduced noise and weight as well as power saving advantages. Transformers: high-frequency...
Abstract
View article
PDF
NK SUPER-E CORE is a non-oriented silicon steel plate containing 6.5% Si with enhanced magnetic characteristics. Higher silicon level is attained by addition to existing silicon steel plate. This datasheet provides information on composition and physical properties. It also includes information on forming and joining. Filing Code: FE-106. Producer or source: NKK Corporation, Keihin Works.
Journal Articles
Alloy Digest (1964) 13 (5): Fe-25.
Published: 01 May 1964
... hydrogen annealing. Hysteresis loss is very low in either direct current circuits or alrernar- ing current circuits in which the frequency is less than 400 cycles pet second. It is used in laminated cores for instrument transformers, magnetic shields and cores for certain electronic and communication...
Abstract
View article
PDF
CARPENTER HIGH PERMEABILITY 49 is an iron-nickel alloy of high magnetic permeability recommended for magnetic and electrical equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating. Filing Code: Fe-25. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1969) 18 (4): Ni-144.
Published: 01 April 1969
... annealing equipment. In specific applications where a part cannot be given a full anneal due to physical reasons, etc., a compromise treatment may have to be given. Any deviation from the standard practice, however, wiU obviously result in a compromise in the magnetic properties. Laminations, shields...
Abstract
View article
PDF
Allegheny Ludlum Moly Permalloy is a nickel-iron-molybdenum alloy having excellent permeability and core loss properties. It has high initial and maximum permeability, low coercive force, and low hysteresis loss. It is recommended for toroids, tape and lamination cores. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-144. Producer or source: Allegheny Ludlum Steel Corporation.
Journal Articles
Alloy Digest (2013) 62 (6): Fe-160.
Published: 01 June 2013
... in.) Applications: Safeni 48 can be used in many applications requiring high relative permeability and a high saturation magnetization. The grade is typically used in the following applications: solenoid valves, AC and DC relays, transformers, parts for measuring instruments, and magnetic shielding for electronic...
Abstract
View article
PDF
Safeni 48 is a soft magnetic iron-nickel alloy with high relative permeability, low coercive field strength, and high saturation magnetization. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: Fe-160. Producer or source: Sandvik Steel Company.
Journal Articles
Alloy Digest (1971) 20 (10): Ni-5.
Published: 01 October 1971
...: Transformer cores, tape-wound toroids and laminations for compactness and weight saving, and magnetic shields for protection of electrical components against stray magnetic tieids. Manufacturer: Carpenter Technology Corporation Reading, Pennsylvania 19603. lhrsted~ (Silberts per Centimeter)-Magnetizing Fonx...
Abstract
View article
PDF
Carpenter HYMU 80 is an unoriented 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability and maximum permeability with minimum hysteresis loss at low magnetic field strengths. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-5. Producer or source: Carpenter Technology Corporation. Originally published May 1953, revised October 1971.
Journal Articles
Alloy Digest (1956) 5 (5): Ni-26.
Published: 01 May 1956
...- forgo earphone and microphone diaphragms, sensitive akernarmg current meters, magnetic shields, high- frequky aircraft equipment, audio transformers and re- actors, D. C. positioning motor poles. Manufacturer: Westinghouse Electric Corporation Blairsville, Pennsylvania ...
Abstract
View article
PDF
HIPERNIK is an alloy of iron and nickel in nearly equal proportions with small amounts of manganese and silicon added. It has exceptionally high initial and maximum permeability and extremely low hysteresis loss. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-26. Producer or source: Westinghouse Electric Corporation.