Alloy Digest (1957) 6 (4): Fe-13.
Published: 01 April 1957
... HIPERCO is a magnetic alloy having a high magnetic saturation value. It permits the design of motors with less metal for the same power, or more power from the same amount of metal. This datasheet provides information on composition, physical properties, and tensile properties. It also includes...
Journal Articles
Alloy Digest (2004) 53 (11): CS-144.
Published: 01 November 2004
... HP magnet steel is designed for use wherever high magnetic permeability or high saturation values are required. Its magnetic qualities result from careful control of sulfur and residual elements plus the special deoxidization practice, which minimizes nonmetallic inclusions. This datasheet...
Journal Articles
Alloy Digest (1970) 19 (1): Fe-41.
Published: 01 January 1970
... Hiperco 35 is an iron-cobalt type of soft magnetic material recommended for use in motors, generators, transformers and relays at temperature above 950 F. It yields the highest known saturation value of 24,500 gausses. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1982) 31 (2): Fe-64.
Published: 01 February 1982
... Table 1 - MAGNETIC PROPERTIES* Property As Cast Annealed Saturation magnetization (BS), kC 15.7 16.1 Coercive force (H,& Oe 0.08 0.04 Residual induction (B kG 6.7 14.2 Induction at 1 Oersted (B1), kG 8.0 15.4 Curie temperature (T8), OC 370 Saturation magnetostriction (As) 30x10-6 1 *All values...
Journal Articles
Alloy Digest (2013) 62 (6): Fe-160.
Published: 01 June 2013
... properties, nominal values at 20 ºC (68 ºF) after optimized annealing cycle Coercive field strength, Hc, A/m (Oe) 5 ( 0.06) Remanent flux density, Br, T (G) 1.1 (11,000) Saturation magnetization, BS, T (G) 1.5 (15,000) Max relative permeability, r 100,000 Mechanical Properties: Mechanical properties...
Journal Articles
Alloy Digest (1982) 31 (4): Fe-65.
Published: 01 April 1982
... (circ mil/ft) Magnetic properties PROPERTIES Table 1 - MAGNETIC PROPERTIES* Propeny As Cast Annealed Saturation magnetization (B kG 15.2 15.6 Coercive force (H Oe 0.17 0.03 Residual induction (B kG 4.0 13. Induction at I Oerstcd (Bl), kG 5.0 IS. Curie temperature (Tg). C 415 - Saturation...
Journal Articles
Alloy Digest (2017) 66 (8): Fe-167.
Published: 01 August 2017
... magnetic properties. Typical values measured on rings sample thickness 0.350 mm (0.014 in.) after annealing treatment at 1150 °C (2102 °F) in dry pure hydrogen cooling rate not critical, 50 to 100°C/hour. Heat Treatment: The optimum magnetic properties for this alloy are obtained by high temperature heat...
Journal Articles
Alloy Digest (2001) 50 (12): Fe-123.
Published: 01 December 2001
... Magnifer 4008 is a soft-magnetic alloy with 40% Ni and 8% Cr. The alloy has high permeability values and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (1960) 9 (7): Fe-18.
Published: 01 July 1960
... - TYPICAL D.C. MAGNETIC PROPERTIES - ANNEALED Coercive force Hc at B max. = 15500, oersteds 0.20 max. Remanence Bt at B max. = 15500, gausses 14500 min. Maximum permeability 75000 min. Saturation value, gausses (at 10 oersteds) 16000 Table 2 - TYPICAL MJXHANICAL PROPERTIES Cold Rolled Annealed Tensile...
Journal Articles
Alloy Digest (1983) 32 (10): Fe-69.
Published: 01 October 1983
... METGLAS Alloy 2605CO is an amorphous iron-base soft magnetic alloy. It has the highest saturation induction of any amorphous alloy commercially available, combined with very low core loss. It is the alloy of choice when low weight is as important as efficiency. It is particularly suited to 400 Hz...
Journal Articles
Alloy Digest (2004) 53 (2): Fe-126.
Published: 01 February 2004
... ( circular-mil/ft) 0.40 (241) Coefficient of linear thermal 9.5 (5.3) expansion, 10 6/K (10 6/°F) Thermal conductivity, W/m K 25 (14.4) (Btu/(ft h °F)) Specific heat capacity, 420 (0.10) J/kg K (Btu/lb °F) Curie temperature, °C (°F) 940 (1724) Magnetic peak inductance, 2.34 (23,400) saturation...
Journal Articles
Alloy Digest (2004) 53 (6): Fe-130.
Published: 01 June 2004
... HS 50 alloy was developed to provide an increase of approximately 0.1 T (1000 G) in saturation magnetization compared with standard Permendur 49. The heat treatment of HS 50 can be carried out at a higher temperature, which gives increased permeability and lower coercive force. The mechanical...
Journal Articles
Alloy Digest (1982) 31 (12): Fe-68.
Published: 01 December 1982
... PROPERTIES Table 1 - MAGNETIC PROPERTIES* Property As Cast Annealed Saturation magnetization (B& kG 15.4 15.8 Coercive force (H& Oe 0.20 0.10 Residual induction (B kG 3.0 4.0 Induction at 1 Oersted (Bl). kG 5.0 11.0 Curie Temperature (Te), C 405 - Saturation magnetrostriction ( As) 27x10-6 - l AJJ values...
Journal Articles
Alloy Digest (1996) 45 (8): Fe-111.
Published: 01 August 1996
... Magnifier 36 is a soft-magnetic nickel-iron alloy with 36% nickel. It has a saturation induction of 1.3 T and a rather high electrical resistance of 0.75 0.75 ohm mm 2 /m. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes...
Journal Articles
Alloy Digest (2006) 55 (7): Fe-139.
Published: 01 July 2006
... Metglas 2605 SA1 is an amorphous iron-base soft magnetic alloy designed for extremely low core loss at distribution and power transformer frequencies and inductions. Applications include high-frequency inductors and current transformers. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2004) 53 (4): Fe-128.
Published: 01 April 2004
... (°F) 940 (1724) Magnetic peak induction, saturation 2.34 (23,400) induction, at 40,000 A/m (500 Oe), T (G) Magnetic permeability, maximum, 13,000 dc, strip Magnetic residual induction, 1.62 (16,200) remanence from saturation, T (G) Coercivity, dc, strip, A/m (Oe) 65 (0.812) See also Fig. 1 3...
Journal Articles
Alloy Digest (2007) 56 (9): SS-996.
Published: 01 September 2007
... Chrome Core 13-XP alloy is a ferritic stainless steel with a controlled chemistry to improve corrosion resistance without significantly decreasing saturation induction in magnetic fields. This datasheet provides information on composition, physical properties, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1961) 10 (5): Fe-19.
Published: 01 May 1961
... pound at 60 cycles and 10,000 gausses 0.286 Coercive Force - oersteds 0.1 Saturation Value - gausses 20,200 Resistivity, microhmsjcm3 47 Maximum Aging - core loss nil Magnetizing Force - oersteds for 10,000 gausses 2.00 Core Loss for 0.012 cores, watts/lb $J 60 cycles & 15,000 gausses 0.90 Curie Point...
Journal Articles
Alloy Digest (1956) 5 (6): SA-44.
Published: 01 June 1956
... is magnetized im&d~ately after hardening, its strength will be found to decrease slightly with time, eventually reaching a stable value. If it is then remagoetized, it will be found to be considerably stronger - and in the case of long magnets, may have a value higher yet than that before aging occurred...
Journal Articles
Alloy Digest (1964) 13 (5): Fe-25.
Published: 01 May 1964
... Permeability BlOO 5,000 Maximum Permeability 6,500 50,000 Residual Magnetism, gausses 60,000 Coercive Force, oersceds 6,000 9,000 from 10,000 gausses 0.05. 0.10 0.05, 0.06 from 5,000 gausses 0.02. 0.03 0.02 0.03 Saturation Inductance, gausses from H q 100 oersreds 15,000 15,000 Table 2 - MECHANICAL PROPERTIES...