Alloy Digest (1998) 47 (7): Fe-117.
Published: 01 July 1998
... MagneDur 20-4 is a cobalt-free alloy with semihard magnetic properties. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming and heat treating. Filing Code: FE-117. Producer or source: Carpenter. Producer...
Journal Articles
Alloy Digest (1978) 27 (6): SA-347.
Published: 01 June 1978
... LOCORE M43 is a cold-rolled, non-oriented electrical steel used primarily for alternating current (AC) and direct current (DC) motors, generators and transformers. It is produced either semiprocessed (the consumer anneals to produce the desired magnetic properties) or fully processed (the steel...
Journal Articles
Alloy Digest (1979) 28 (1): SA-353.
Published: 01 January 1979
... LOCORE M45 is a cold-rolled, non-oriented electrical steel used primarily for alternating current (AC) and direct current (DC) motors, generators and transformers. It is produced either semiprocessed (the consumer anneals to produce the desired magnetic properties) or fully processed (the steel...
Journal Articles
Alloy Digest (1987) 36 (1): Fe-75.
Published: 01 January 1987
... CMI-C Magnetic Iron is a low-carbon magnetic iron especially processed with a critical strain for optimum uniformity. Maximum magnetic properties are achieved following suggested final anneal applied to fabricated parts. Its applications include electromagnet cores, plungers and pole pieces...
Journal Articles
Alloy Digest (1956) 5 (6): SA-44.
Published: 01 June 1956
... Cobalt magnet steels have high coercive force which makes it possible to maintain strong magnetic fields with relatively short magnets. These alloys must be hardened by drastic quenching in oil to obtain the maximum magnetic properties. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1994) 43 (1): Fe-104.
Published: 01 January 1994
... CARPENTER ELECTRICAL IRON is an iron with very low interstitials and other elements present to provide good direct current soft magnetic properties. Used in magnetic circuit cores. This datasheet provides information on composition and physical properties. It also includes information on heat...
Journal Articles
Alloy Digest (1967) 16 (11): Fe-31.
Published: 01 November 1967
... ALNICO II is a general purpose permanent magnet alloy recommended for applications where better magnetic properties than Alnico I are desired. It is a high coercive force, high energy magnetic alloy. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1980) 29 (12): SS-378.
Published: 01 December 1980
...-magnetic in the annealed condition but slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1981) 30 (6): SS-387.
Published: 01 June 1981
... a uniquely soft and machinable sulfide inclusion. This grade is non-magnetic in the annealed condition but slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties. This datasheet provides...
Journal Articles
Alloy Digest (1981) 30 (9): SS-392.
Published: 01 September 1981
... condition but slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1983) 32 (2): SS-421.
Published: 01 February 1983
... but slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1986) 35 (10): Fe-73.
Published: 01 October 1986
... CMI-B Magnetic Iron is an ultra-low-carbon magnetic iron especially processed for good magnetic properties and processability. It is used for relays and other electromagnetic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1975) 24 (9): Fe-54.
Published: 01 September 1975
... MAGNESIL-O is an oriented silicon-iron alloy of exceptional magnetic qualities designed for applications involving frequencies of 400 Hertz and higher. It has pronounced directional magnetic properties in the direction of rolling. It is recommended for wound cores and stacked laminations which...
Journal Articles
Alloy Digest (2013) 62 (10): Nd-5.
Published: 01 October 2013
... NEOQUENCH-P GRADE NP-8 is one of a series of isotropic polymer bonded magnets based on Nd-Fe-B. The raw material powder is manufactured by rapid quenching of prescribed alloys into nanocrystalline flakes that are subsequently annealed for optimum magnetic properties. This alloy is an isotropic...
Journal Articles
Alloy Digest (1964) 13 (8): Co-39.
Published: 01 August 1964
... Alnico 8 is a permanent magnet material having over twice as much resistance to demagnetization as Alnico 5. It requires a magnetic heat treatment to develop strong directional magnetic properties. This datasheet provides information on composition, physical properties, and hardness. It also...
Journal Articles
Alloy Digest (1965) 14 (2): Co-42.
Published: 01 February 1965
... Vicalloy-1 is a precipitation hardening cobalt-base alloy recommended for electromechanical devices. It is a permanent magnet alloy, combining improved magnetic properties and a high degree of ductility. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1999) 48 (1): Fe-88.
Published: 01 January 1999
... Armco DI-MAX nonoriented electrical steels have practically identical magnetic properties in any direction of magnetism in the plane of the material. They have superior permeability at high inductions, low average core loss, good gage uniformity, excellent flatness, and a high stacking factor...
Journal Articles
Alloy Digest (1966) 15 (10): Fe-29.
Published: 01 October 1966
... ALNICO V-7 is a heat treatable cast alloy of iron, aluminum, nickel, cobalt and copper. It is a permanent magnet alloy having directional magnetic properties and a maximum energy product of 7,500,000 gauss-oersteds. (Also known as ALNICO 5-7) This datasheet provides information on composition...
Journal Articles
Alloy Digest (2013) 62 (5): Nd-4.
Published: 01 May 2013
... NEOQUENCH-P GRADE NP-7L is one of a series of isotropic polymer bonded magnets based on Nd-Fe-B. The raw material powder is manufactured by rapid quenching of prescribed alloys into nanocrystalline flakes that are subsequently annealed for optimum magnetic properties. NP-7L is made by compression...
Journal Articles
Alloy Digest (2013) 62 (12): SS-1164.
Published: 01 December 2013
... MAGIVAL MG3 is a ferritic free machining stainless steel grade with similar magnetic properties to MG1 (Alloy Digest SS-1159, October 2013); it has better pitting corrosion resistance due to its molybdenum content, allowing applications in mild chloride corrosive environments. Magival is a group...