Skip Nav Destination
Close Modal
Search Results for
magnetic permeability
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 686
Search Results for magnetic permeability
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1994) 43 (1): SS-561.
Published: 01 January 1994
... CARPENTER STAINLESS TYPE 430F SOLENOID QUALITY offers much of the properties of 430 stainless steel, but through composition and processing maintains consistently high magnetic permeability and low residual induction. This datasheet provides information on composition, physical properties...
Abstract
View articletitled, CARPENTER STAINLESS TYPE 430F SOLENOID QUALITY: High <span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span> Chromium Iron Stainless Steel
View
PDF
for article titled, CARPENTER STAINLESS TYPE 430F SOLENOID QUALITY: High <span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span> Chromium Iron Stainless Steel
CARPENTER STAINLESS TYPE 430F SOLENOID QUALITY offers much of the properties of 430 stainless steel, but through composition and processing maintains consistently high magnetic permeability and low residual induction. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: SS-561. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1953) 2 (6): Fe-1.
Published: 01 June 1953
... GLOBEIRON is a high purity, thoroughly killed, low carbon iron. It is ductile, tough, and has high magnetic permeability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating...
Abstract
View articletitled, GLOBEIRON: High <span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span> Iron
View
PDF
for article titled, GLOBEIRON: High <span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span> Iron
GLOBEIRON is a high purity, thoroughly killed, low carbon iron. It is ductile, tough, and has high magnetic permeability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Fe-1. Producer or source: Globe Steel Tubes Company.
Journal Articles
Alloy Digest (1999) 48 (6): SS-748.
Published: 01 June 1999
... Carpenter SCF 19 alloy is a high-strength and low-magnetic permeability alloy developed for nonmagnetic drill collars. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes...
Abstract
View articletitled, CARPENTER SCF 19 ALLOY: Austenitic Low-<span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span> Alloy
View
PDF
for article titled, CARPENTER SCF 19 ALLOY: Austenitic Low-<span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span> Alloy
Carpenter SCF 19 alloy is a high-strength and low-magnetic permeability alloy developed for nonmagnetic drill collars. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-748. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1974) 23 (7): Fe-51.
Published: 01 July 1974
... UNILOY 888 is an iron-base, age-hardenable alloy designed primarily for applications requiring low magnetic permeability and high strength. It is austenitic at all times and its essentially non-magnetic characteristics are not impaired by various combinations of heat treatment and cold working...
Abstract
View articletitled, UNILOY 888: Low <span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span> Alloy
View
PDF
for article titled, UNILOY 888: Low <span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span> Alloy
UNILOY 888 is an iron-base, age-hardenable alloy designed primarily for applications requiring low magnetic permeability and high strength. It is austenitic at all times and its essentially non-magnetic characteristics are not impaired by various combinations of heat treatment and cold working used to produce desired mechanical properties. It is used primarily between 70 and 700 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: Fe-51. Producer or source: Cyclops Corporation.
Journal Articles
Alloy Digest (1968) 17 (8): Fe-35.
Published: 01 August 1968
... B and W IRON is a thoroughly killed, low carbon steel having a combination of ductility, toughness and high magnetic permeability. It is recommended for applications where good magnetic characteristics are of primary significance, such as in the manufacture of electric motor and generator housings...
Abstract
View articletitled, B&amp;W IRON: High <span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span> Iron
View
PDF
for article titled, B&amp;W IRON: High <span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span> Iron
B and W IRON is a thoroughly killed, low carbon steel having a combination of ductility, toughness and high magnetic permeability. It is recommended for applications where good magnetic characteristics are of primary significance, such as in the manufacture of electric motor and generator housings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Fe-35. Producer or source: Babcock & Wilcox Company.
Journal Articles
Alloy Digest (1976) 25 (11): Ni-235.
Published: 01 November 1976
... METGLAS Alloy 2826 (Fe40Ni40P14B6) is a ferromagnetic, high permeability, nickel-iron metallic glass which, when appropriately annealed, yields a material similar to the higher nickel containing permalloys in magnetic properties. Alloy 2826 is a single phase, opaque metallic material with a glass...
Abstract
View articletitled, METGLAS ALLOY 2826: Metallic Glass with High <span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span>
View
PDF
for article titled, METGLAS ALLOY 2826: Metallic Glass with High <span class="search-highlight">Magnetic</span> <span class="search-highlight">Permeability</span>
METGLAS Alloy 2826 (Fe40Ni40P14B6) is a ferromagnetic, high permeability, nickel-iron metallic glass which, when appropriately annealed, yields a material similar to the higher nickel containing permalloys in magnetic properties. Alloy 2826 is a single phase, opaque metallic material with a glass-like structure obtained by a very rapid quench from the liquid state. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on forming and heat treating. Filing Code: Ni-235. Producer or source: Allied Chemical Corporation.
Journal Articles
Alloy Digest (2004) 53 (11): CS-144.
Published: 01 November 2004
... HP magnet steel is designed for use wherever high magnetic permeability or high saturation values are required. Its magnetic qualities result from careful control of sulfur and residual elements plus the special deoxidization practice, which minimizes nonmetallic inclusions. This datasheet...
Abstract
View articletitled, HP <span class="search-highlight">MAGNET</span> PLATE STEEL: High-<span class="search-highlight">Permeability</span> Steel
View
PDF
for article titled, HP <span class="search-highlight">MAGNET</span> PLATE STEEL: High-<span class="search-highlight">Permeability</span> Steel
HP magnet steel is designed for use wherever high magnetic permeability or high saturation values are required. Its magnetic qualities result from careful control of sulfur and residual elements plus the special deoxidization practice, which minimizes nonmetallic inclusions. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: CS-144. Producer or source: ISG Plate International Steel Group Inc.
Journal Articles
Alloy Digest (1994) 43 (12): Fe-108.
Published: 01 December 1994
... CARPENTER SILICON CORE IRON A-FM (High Initial Permeability Magnetic Core ton) Caxpenter Silicon Core Iron A-FM , melted to exacting chemical specifications and carefuliy process controkd to produce a fine-grained uniform quality magnetic core iron. This alloy exhibits improved machining characteristics...
Abstract
View articletitled, CARPENTER SILICON CORE IRON A-FM: High Initial <span class="search-highlight">Permeability</span> <span class="search-highlight">Magnetic</span> Core Iron
View
PDF
for article titled, CARPENTER SILICON CORE IRON A-FM: High Initial <span class="search-highlight">Permeability</span> <span class="search-highlight">Magnetic</span> Core Iron
Carpenter Silicon Core Iron A-FM, melted to exacting chemical specifications and carefully process controlled to produce a fine-grained uniform quality magnetic core iron. This alloy exhibits improved machining characteristics over Silicon Core Iron A (Alloy Digest Fe-94, January 1991). This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining. Filing Code: FE-108. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1990) 39 (9): Ni-385.
Published: 01 September 1990
... (Type Analysis): Carbon 0.02 Mangan= 050 Silicon 0.35 NiCkd 80.00 Molybdenum 420 Iron Remainder PROPERTIES Magnetic Properties: DC and impedence permeabilities are shown in Figures 1 to 3 inclusive. w.cw lum llilll i I 1111111 I I f Illif] mQD( 01 .w 10 Figure 1 - Typical DC permeability range, 0.014...
Abstract
View articletitled, HYPERNOM ALLOY: Soft <span class="search-highlight">Magnetic</span>, High <span class="search-highlight">Permeability</span> Alloy
View
PDF
for article titled, HYPERNOM ALLOY: Soft <span class="search-highlight">Magnetic</span>, High <span class="search-highlight">Permeability</span> Alloy
HYPERNOM alloy is a high-permeability, low-hysteresis nickel-base alloy which is provided with the correct temper for sheet metal cold formability for shielding components. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: Ni-385. Producer or source: Carpenter Technology Corporation.
Journal Articles
Alloy Digest (1991) 40 (1): Fe-94.
Published: 01 January 1991
... properties CARPENTER SILICON CORE IRON A Filing Code: Iron Alloy Fe-94 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS JANUARY 1991 Ptiidhed byr Ahy Digeet. Inc /2[)1-6Z -9161 27 CaMeId Stmet. Orange. NJ. 07060 I U.SA CARPENTER SILICON CORE IRON A (High Initial Permeability Magnetic Core Iron...
Abstract
View articletitled, CARPENTER SILICON CORE IRON A: High Initial <span class="search-highlight">Permeability</span> <span class="search-highlight">Magnetic</span> Core Iron
View
PDF
for article titled, CARPENTER SILICON CORE IRON A: High Initial <span class="search-highlight">Permeability</span> <span class="search-highlight">Magnetic</span> Core Iron
Carpenter Silicon Core Iron A, melted to exacting chemical specifications and carefully process controlled is a uniform quality magnetic core iron. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining. Filing Code: Fe-94. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1969) 18 (8): Fe-38.
Published: 01 August 1969
... Permeability Magnetic Iron) AJfenol is an unoriented 125, to 16% aluminum-iron alloy which has high electrical resistivity and low eddy current losses. It is furnished in the 12% aluminum and in the 16% aluminum grades. The recommended uses are for relays, gyro mechanisms, servo-mechanisms and toroid tape...
Abstract
View articletitled, ALFENOL: High <span class="search-highlight">Permeability</span> <span class="search-highlight">Magnetic</span> Iron
View
PDF
for article titled, ALFENOL: High <span class="search-highlight">Permeability</span> <span class="search-highlight">Magnetic</span> Iron
Alfenol is an unoriented 12% to 16% aluminum-iron alloy which has high electrical resistivity and low eddy current losses. It is furnished in the 12% aluminum and in the 16% aluminum grades. The recommended uses are for relays, gyro mechanisms, servo-mechanisms and toroid tape cores. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating. Filing Code: Fe-38. Producer or source: Carpenter.
Journal Articles
Alloy Digest (2019) 68 (6): SA-847.
Published: 01 June 2019
... for use as large fabricated DC magnets. Chemical Composition, wt.% (Maximum) HP magnet steel is fully killed. Carbon 0.08 Manganese 0.25 0.45 Phosphorus 0.025 Sulfur 0.025 Silicon 0.50 Cu+Ni+Cr+Mo 0.50 Physical Properties Permeability and hysteresis are noted in Fig. 1 and 2. Mechanical Properties...
Abstract
View articletitled, HP <span class="search-highlight">MAGNET</span> STEEL: High-<span class="search-highlight">Permeability</span> <span class="search-highlight">Magnet</span> Plate
View
PDF
for article titled, HP <span class="search-highlight">MAGNET</span> STEEL: High-<span class="search-highlight">Permeability</span> <span class="search-highlight">Magnet</span> Plate
Arcelor Mittal HP magnet plate was developed for use as large fabricated DC magnets. This datasheet provides information on composition, tensile properties, and shear strength. It also includes information on heat treating, machining, and joining. Filing Code: SA-847. Producer or source: ArcelorMittal USA.
Journal Articles
Alloy Digest (1964) 13 (5): Fe-25.
Published: 01 May 1964
... CARPENTER HIGH PERMEABILITY 49 is an iron-nickel alloy of high magnetic permeability recommended for magnetic and electrical equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Abstract
View articletitled, CARPENTER HIGH <span class="search-highlight">PERMEABILITY</span> 49: High <span class="search-highlight">Permeability</span> Alloy
View
PDF
for article titled, CARPENTER HIGH <span class="search-highlight">PERMEABILITY</span> 49: High <span class="search-highlight">Permeability</span> Alloy
CARPENTER HIGH PERMEABILITY 49 is an iron-nickel alloy of high magnetic permeability recommended for magnetic and electrical equipment. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating. Filing Code: Fe-25. Producer or source: Carpenter.
Journal Articles
Alloy Digest (1960) 9 (6): SA-99.
Published: 01 June 1960
... JESSOP No. 200 is a non-magnetic, austenitic steel developed especially for the electrical industry. It has low magnetic permeability and high electrical resistance. Jessop No. 200 is ideal for a great number of applications requiring low permeability material where corrosion resistance...
Abstract
View articletitled, JESSOP No. 200: Manganese-Nickel Alloy Steel
View
PDF
for article titled, JESSOP No. 200: Manganese-Nickel Alloy Steel
JESSOP No. 200 is a non-magnetic, austenitic steel developed especially for the electrical industry. It has low magnetic permeability and high electrical resistance. Jessop No. 200 is ideal for a great number of applications requiring low permeability material where corrosion resistance is not a factor and where cost is important. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-99. Producer or source: Jessop Steel Company.
Journal Articles
Alloy Digest (2013) 62 (11): SS-1161.
Published: 01 November 2013
... MAGIVAL MG2 is a free machining ferritic stainless steel grade with the same high machinability and corrosion resistance as type 430F, but offering a higher magnetic permeability and lower coercive force than MG1 (Alloy Digest SS-1159, October 2013). Magival is a group of easily workable ferritic...
Abstract
View articletitled, MAGIVAL MG2: Workable Ferritic Stainless Steel
View
PDF
for article titled, MAGIVAL MG2: Workable Ferritic Stainless Steel
MAGIVAL MG2 is a free machining ferritic stainless steel grade with the same high machinability and corrosion resistance as type 430F, but offering a higher magnetic permeability and lower coercive force than MG1 (Alloy Digest SS-1159, October 2013). Magival is a group of easily workable ferritic stainless steels developed for magnetic applications where high permeability and low coercive force are required. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1161. Producer or source: Valbruna Stainless Steel.
Journal Articles
Alloy Digest (1992) 41 (4): Fe-97.
Published: 01 April 1992
... Allegheny Ludlum No. 2 and No. 5 relay steels are iron/silicon alloys. They are soft magnetic alloys that combine high magnetic permeability, low residual magnetization and low coercive force with good mechanical properties and fabricability. This datasheet provides information on composition...
Abstract
View articletitled, ALLEGHENY LUDLUM No. 2, No. 5, RELAY STEELS: Soft <span class="search-highlight">Magnetic</span> Iron Silicon Alloys
View
PDF
for article titled, ALLEGHENY LUDLUM No. 2, No. 5, RELAY STEELS: Soft <span class="search-highlight">Magnetic</span> Iron Silicon Alloys
Allegheny Ludlum No. 2 and No. 5 relay steels are iron/silicon alloys. They are soft magnetic alloys that combine high magnetic permeability, low residual magnetization and low coercive force with good mechanical properties and fabricability. This datasheet provides information on composition and physical properties. It also includes information on forming, heat treating, and machining. Filing Code: Fe-97. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Alloy Digest (1973) 22 (2): Ni-186.
Published: 01 February 1973
... BLENDALLOY 25-8005 is a soft magnetic alloy for use in a variety of precise magnetic devices. It has high magnetic permeability, low coercive force, low hysteresis loss, exceptional purity and cleanliness, precise chemical composition, and good reproducibility in production heats. It is a powder...
Abstract
View articletitled, BLENDALLOY 25-8005: Soft <span class="search-highlight">Magnetic</span> Alloy
View
PDF
for article titled, BLENDALLOY 25-8005: Soft <span class="search-highlight">Magnetic</span> Alloy
BLENDALLOY 25-8005 is a soft magnetic alloy for use in a variety of precise magnetic devices. It has high magnetic permeability, low coercive force, low hysteresis loss, exceptional purity and cleanliness, precise chemical composition, and good reproducibility in production heats. It is a powder-metallurgy product. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-186. Producer or source: Spang Industries Inc..
Journal Articles
Alloy Digest (1997) 46 (12): Ni-133.
Published: 01 December 1997
... Hipernom is a high nickel-iron alloy that is magnetically soft and has high minimum and maximum magnetic permeabilities. It is used in many applications including shielding, saturable reactors, transformers, and relays. This datasheet provides information on composition, physical properties...
Abstract
View articletitled, CARPENTER HIPERNOM: <span class="search-highlight">Magnetically</span> Soft Alloy
View
PDF
for article titled, CARPENTER HIPERNOM: <span class="search-highlight">Magnetically</span> Soft Alloy
Hipernom is a high nickel-iron alloy that is magnetically soft and has high minimum and maximum magnetic permeabilities. It is used in many applications including shielding, saturable reactors, transformers, and relays. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ni-133. Producer or source: Carpenter. Originally published as Hipernom, May 1968, revised December 1997.
Journal Articles
Alloy Digest (1976) 25 (1): Ni-223.
Published: 01 January 1976
... Round Permalloy 80 is an 80% nickel-iron-molybdenum alloy that provides very high initial and maximum magnetic permeabilities and minimal core losses at low field strengths. This vacuum-melted product also offers the advantages of small size and weight in magnetic core and shielding materials...
Abstract
View articletitled, ROUND PERMALLOY 80: Soft <span class="search-highlight">Magnetic</span> Alloy
View
PDF
for article titled, ROUND PERMALLOY 80: Soft <span class="search-highlight">Magnetic</span> Alloy
Round Permalloy 80 is an 80% nickel-iron-molybdenum alloy that provides very high initial and maximum magnetic permeabilities and minimal core losses at low field strengths. This vacuum-melted product also offers the advantages of small size and weight in magnetic core and shielding materials for numerous applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-223. Producer or source: Spang Industries Inc..
Journal Articles
Alloy Digest (2013) 62 (8): Fe-161.
Published: 01 August 2013
... Safeni 52 is a soft magnetic iron-nickel alloy with high magnetic permeability, low coercive force, a low content of nonmetallic inclusions, and thermal expansion properties that make it suitable for glass-sealing applications. This datasheet provides information on composition, physical...
Abstract
View articletitled, SANDVIK SAFENI 52: Soft <span class="search-highlight">Magnetic</span> Alloy
View
PDF
for article titled, SANDVIK SAFENI 52: Soft <span class="search-highlight">Magnetic</span> Alloy
Safeni 52 is a soft magnetic iron-nickel alloy with high magnetic permeability, low coercive force, a low content of nonmetallic inclusions, and thermal expansion properties that make it suitable for glass-sealing applications. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: Fe-161. Producer or source: Sandvik Steel Company.
1