Alloy Digest (1972) 21 (11): Ni-181.
Published: 01 November 1972
... BLENDALLOY 25-7904 is an 80% nickel-15% iron-5% molybdenum alloy having very high permeability and low coercive force for magnetic cores in such applications as transformer laminations, sensitive magnetic amplifiers and magnetic shielding. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1960) 9 (7): Fe-18.
Published: 01 July 1960
... HIPERNIK-V is an alloy of iron and nickel possessing a very high remanent magnetization accompanied by a low coercive force. Most applications of this alloy take the form of tape wound cores for use in magnetic amplifiers and saturable reactors. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1967) 16 (1): Co-50.
Published: 01 January 1967
... with the field maintained, will exhibit a low-energy rectangular hysteresis loop approaching that of Supermendur. It is recommended that &is type of anneal be considered if Hiperco 50 is to be used in transformers or magnetic amplifiers or other appli- cations in which a relatively low-enerm rectangular...
Journal Articles
Alloy Digest (1995) 44 (10): Ni-488.
Published: 01 October 1995
... requirements to a minimum. It is used in transformers, inductors, magnetic amplifi- ers, switching devices, magnetic shields, tape recorder heads and memory storage devices. Forms Available: Sheet, strip Producer: INCO Alloys International, Inc. Huntington, WV 25720 304-526-5000 0 4.0 8.0 1 Magne(iring Fone...
Journal Articles
Alloy Digest (1973) 22 (3): Ni-188.
Published: 01 March 1973
.... By using powder metalhrrgy, composition is controlled precisely, thus eliminating a significant variable. Heat treatment is controlled by annealing in hydrogen as described under Heat Treatment. Forms Avaiable: Cold-rolled strip 0.005 to 0.04~inch thick. Applications: Magnetic amplifiers, converters...
Journal Articles
Alloy Digest (1982) 31 (2): Fe-64.
Published: 01 February 1982
... nominal thickness and of almost any length. Several standard widths up to 2 inches are available and other widths can be obtained by slitting or special casting. Applications. METGLAS alloy 2605SC finds applications in pulse transformers, magnetic amplifiers. power transformers, current transducers...
Journal Articles
Alloy Digest (1975) 24 (9): Fe-54.
Published: 01 September 1975
... electrical properties. Strip coils 0.001, 0.002,0.003.0.004 and 0.006-in. thick, 15-m. rolled width. Slit coils are available in any desired width. Strip normally carries a thin layer of inorganic insulation but can be ordered without the insulation. Applications: Chokes, magnetic amplifiers, audio output...
Journal Articles
Alloy Digest (2001) 50 (1): Fe-4.
Published: 01 January 2001
... grade with an 8 9 grain size and transformer grade with a 2 cm grain size. Applications: Magnetic relay parts, magnetic shielding, pole pieces, specialty motor stators and rotors, electric transformers, magnetic amplifiers Producer: Allegheny Ludlum Corporation Pittsburgh, PA 16222-6479 (800) 258-3586...
Journal Articles
Alloy Digest (1975) 24 (7): Fe-53.
Published: 01 July 1975
.... Applications: Chokes, magnetic amplifiers, audio output and hi-t? trans- formers, instrument transformers, pulse transformers. inter- mediate frequency transformers. converters (inverters), motors. sensitive relays. reactors, computer and high-frequency power supplies. and filters. Manufacturer: Magnetics...
Journal Articles
Alloy Digest (1976) 25 (1): Ni-223.
Published: 01 January 1976
... Round Permalloy 80 is an 80% nickel-iron-molybdenum alloy that provides very high initial and maximum magnetic permeabilities and minimal core losses at low field strengths. This vacuum-melted product also offers the advantages of small size and weight in magnetic core and shielding materials...
Journal Articles
Alloy Digest (1973) 22 (6): Ni-191.
Published: 01 June 1973
... and widths. Applications: Typical uses for shielding include transformers, reed relays, amplifiers, vacuum tubes, cathode ray tubes, microphones, loud speakers, instruments, cables, and recording heads. Manufacturer: Magnetic Specialty Metals Division Spang Industries, Inc. Butler, Pennsylvania 16001. ...
Journal Articles
Alloy Digest (1981) 30 (6): Co-77.
Published: 01 June 1981
... applications include beam control and focusing in a vacuum, biasing applications, circulators, aoss field amplifiers, electron tubes, Hall effect switches, hearing aids, klystrons (magnets in a vacuum), microphones, miaowave devices, phono cartridges and vacuum ion pumps (aerospace). Use in instruments...
Journal Articles
Alloy Digest (1981) 30 (8): Co-78.
Published: 01 August 1981
... motors. Electronic applications include beam control and focusing in a vacuum, biasing applications, circulators, aoss f=ld amplifiers, electron tubes, Hall effect switches, hearing aids, klystrons (magnets in a vacuum), microphones, microwave devices, phono cartridges and vacuum ion pumps (aerospace...