1-20 of 4119

Search Results for machine tool

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1985) 34 (9): TS-446.
Published: 01 September 1985
... VISCOUNT 20 (Free-Machining Tool Steel; AISI Type H-13) VISCOUNT 20 is an air-hardening, 5% chromium hot-work steel with the same analysis as Latrobe s VDC* except for the addition of carefully controlled and evenly dispersed alloy sulfides. These additives improve the machinability of the steel so...
Journal Articles
Alloy Digest (1996) 45 (12): TS-547.
Published: 01 December 1996
... DH2F is a modified H13-type tool steel prehardened to 40 HRC that is free-machining. Applications include dies for plastics and zinc, plunger tips, and die plate strippers. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties...
Journal Articles
Alloy Digest (1992) 41 (8): TS-512.
Published: 01 August 1992
... THYRAPID 3341 is similar to AISI M2, but adds sulfur. It is general purpose high-speed tool steel with good toughness, red hardness, and excellent machinability. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1976) 25 (10): CS-63.
Published: 01 October 1976
... AISI 1065 is a high-carbon oil-hardening machinery and tool steel of low hardenability. It is used for springs, hand tools, machinery parts, shafts and many machine tools requiring strength and wear resistance. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1988) 37 (1): CS-118.
Published: 01 January 1988
... SAE 1065 is a high-carbon oil-hardening machinery and tool steel of low hardenability. It is used for springs, hand tools, machinery parts, shafts and many machine tools requiring strength and wear resistance. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1973) 22 (4): CS-51.
Published: 01 April 1973
... AISI 1070 is a high-carbon water or oil-hardening tool and spring steel of low hardenability. It is used for railroad and street railway rails, heavy machinery parts, shafts, springs and a wide variety of hand and machine tools requiring strength and wear resistance. This datasheet provides...
Journal Articles
Alloy Digest (1984) 33 (2): SA-397.
Published: 01 February 1984
... a relatively low tendency to develop temper embrittlement when tempered in the approximate range 850-1100 F. Among its many applications are springs, machine-tool parts, shafting, gears, bolts and heavy-duty hand tools. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1988) 37 (6): CS-121.
Published: 01 June 1988
... SAE 1070 is a high-carbon water or oil-hardening tool and spring steel of low hardenability. It is used for railroad and street railway rails, heavy machinery parts, shafts, springs and a wide variety of hand and machine tools requiring strength and wear resistance. This datasheet provides...
Journal Articles
Alloy Digest (1997) 46 (1): TS-549.
Published: 01 January 1997
... Carpenter Micro-Melt T-15 Alloy is a high-speed tool steel made by the powder metallurgy process. The alloy is high carbon with tungsten, cobalt, and vanadium for red hardness and excellent abrasion resistance. Applications include machine tools and cutters. This datasheet provides information...
Journal Articles
Alloy Digest (1954) 3 (1): CI-5.
Published: 01 January 1954
... MEEHANITE GA is a high strength iron casting having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, and housings. This datasheet provides information...
Journal Articles
Alloy Digest (1954) 3 (9): CI-8.
Published: 01 September 1954
... MEEHANITE GC is a high strength iron casting having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, permanent molds, lathe beds, bases, pistons...
Journal Articles
Alloy Digest (1955) 4 (10): CI-12.
Published: 01 October 1955
... MEEHANITE GE is a medium strength iron having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, pump bodies, valve bodies, steam cylinders, cylinder...
Journal Articles
Alloy Digest (1968) 17 (10): SA-232.
Published: 01 October 1968
... ISO-CAST 8 is a cast chromium-molybdenum steel recommended as a general purpose structural alloy of wide application with wide range of mechanical properties. It is used for aircraft and railroad car parts, machine tool and hammermill equipment, gears and shafts. This datasheet provides...
Journal Articles
Alloy Digest (1970) 19 (1): SA-248.
Published: 01 January 1970
... HY-TEN B Temper No. 3X-40 is a medium-carbon alloy steel having free-cutting characteristics. It is recommended for machine tools, mining and road building equipment, gears, crankshafts, bolts, etc. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Alloy Digest (1963) 12 (5): Cu-128.
Published: 01 May 1963
... AMPCOLOY 45 is a high strength, extra tough bronze for machine tool parts, gears, shafts, etc. It is heat treatable and has excellent to corrosion, wear and abrasion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1958) 7 (9): CI-22.
Published: 01 September 1958
... MEEHANITE GB is a high strength iron casting having high damping capacity, self-lubricating properties, and good machinability. It combines the good properties of both cast iron and steel. Applications include machine tools, gears, shafts, housings, lathe beds, bases, pistons, crankshafts...
Journal Articles
Alloy Digest (1986) 35 (7): SA-420.
Published: 01 July 1986
... SAE 4145 is a through-hardening, medium-carbon chromium-molybdenum alloy steel of high hardenability. It is recommended for heavy-duty service and is suitable for a wide variety of engineering uses. Its many applications include gears, axles, flanges, machine tool parts, nitrided parts, bolts...
Journal Articles
Alloy Digest (1977) 26 (9): CI-44.
Published: 01 September 1977
.... Typical applications are automotive equipment, compressors, machine tools and general machinery applications. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also...
Journal Articles
Alloy Digest (1977) 26 (11): SA-338.
Published: 01 November 1977
... it needs no heat treatment and is suitable for a wide variety of engineering uses such as shafts, axles and machine-tool parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1979) 28 (11): SA-365.
Published: 01 November 1979
... be used in the unhardened (annealed, as-rolled or normalized) condition. Its applications include gears, springs, wrenches and machine tool parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...