Alloy Digest (1997) 46 (7): SS-515.
Published: 01 July 1997
... Project 70 and Project 7000 Type 316L stainless steels are versions of conventional AISI Type 316L stainless steel having improved machinability, and having higher tensile and creep strengths than conventional 18-8 stainless steels. This datasheet provides information on composition and physical...
Journal Articles
Alloy Digest (1970) 19 (9): Ni-157.
Published: 01 September 1970
... MONEL alloy 502, a modification of MONEL alloy K-500, provides improved machinability. It maintains high strength up to about 800 F and has good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1962) 11 (3): Cu-115.
Published: 01 March 1962
... Mueller 799 tellurium copper combines the high electrical and thermal conductivity and corrosion resistance of copper with the excellent machinability of free turning brass. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (2009) 58 (10): Al-425.
Published: 01 October 2009
... Alcoa alloy 6013 Power Plate is a higher machinable development with higher strength over 6061-T651 by 22%. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (1992) 41 (8): TS-512.
Published: 01 August 1992
... THYRAPID 3341 is similar to AISI M2, but adds sulfur. It is general purpose high-speed tool steel with good toughness, red hardness, and excellent machinability. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1983) 32 (6): SS-428.
Published: 01 June 1983
... PROJECT 70 STAINLESS TYPE 303DQ is a modification of Project 70 Stainless Type 303 (Alloy Digest, SS-409, revised June 1997). Type 303DQ is designed and processed to optimize drilling and cut-thread tapping machining operations. Compared with regular Project 70 Stainless Type 303, the Type 303DQ...
Journal Articles
Alloy Digest (1987) 36 (9): SS-490.
Published: 01 September 1987
... CRUCIBLE 303 SUPER-X is a non-hardenable austenitic stainless steel with improved machinability and non-galling characteristics. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1985) 34 (6): CS-107.
Published: 01 June 1985
... LA SALLE SERIES 83-420 is a low-carbon, bismuth-bearing, free-machining, cold-finished steel that does not contain lead, tellurium or selenium. Its excellent machinability is achieved by the addition of a special bismuth alloy. Series 83-420 reduces friction during machining and the chips break...
Journal Articles
Alloy Digest (1985) 34 (9): TS-446.
Published: 01 September 1985
... VISCOUNT 20 is an air-hardening, 5% chromium hot-work steel with the same analysis as Latrobe's VDC except for the addition of carefully controlled and evenly dispersed alloy sulfides. These additives improve the machinability of the steel so that it is an excellent selection for a variety of hot...
Journal Articles
Alloy Digest (1985) 34 (11): CS-2.
Published: 01 November 1985
... STRESSPROOF is a medium carbon-manganese resulfurized free-machining steel. It is a heavy-drafted, cold drawn, straightened and stress relieved bar steel with high strength, improved fatigue resistance, and excellent machinability. It does not require heat treatment after fabrication...
Journal Articles
Alloy Digest (1986) 35 (8): Ni-338.
Published: 01 August 1986
... CARPENTER NICKEL-COPPER ALLOY 405 is the free-machining grade of Carpenter Nickel-Copper Alloy 400, the result of a controlled amount of added sulfur. Like Alloy 400, Alloy 405 is a solid-solution alloy and therefore strengthed only by cold work. Its strength is comparable to that of structural...
Journal Articles
Alloy Digest (1988) 37 (1): Cu-533.
Published: 01 January 1988
... the limits needed for most current-carrying requirements. Typical uses comprise electrical motor and switch parts, electrical connectors and screw-machine parts requiring high conductivity. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1988) 37 (7): SA-431.
Published: 01 July 1988
... INcut 200 is a premium free-machining steel containing no lead. Machinability is derived from added bismuth. The steel has excellent ductility and it can be welded and brazed readily. The absence of lead facilitates of machine shop scrap. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1989) 38 (4): Cer-2.
Published: 01 April 1989
... ALUMINA SILICATE 902 is a machinable ceramic with a limiting continuous service temperature of 2100 F(1150 C). This datasheet provides information on physical properties, hardness, and compressive and bend strength. It also includes information on machining. Filing Code: Cer-2. Producer or source...
Journal Articles
Alloy Digest (1989) 38 (5): Cer-3.
Published: 01 May 1989
... provides information on physical properties, hardness, tensile properties, and compressive and bend strength as well as fracture toughness. It also includes information on machining. Filing Code: Cer-3. Producer or source: AlSiMag Technical Ceramics Inc.. Producer or Source: AlSiMag Technical Ceramics...
Journal Articles
Alloy Digest (2001) 50 (6): Cu-668.
Published: 01 June 2001
... Swissmetal SM453C is a free-machining copper alloy with high electrical conductivity. It is recommended for male contacts in electrical and electronic applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2001) 50 (8): Cu-671.
Published: 01 August 2001
... Wieland-Z21 is a medium leaded brass with a good cold-working capability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining...
Journal Articles
Alloy Digest (2001) 50 (9): Cu-672.
Published: 01 September 2001
... Wieland-Z23 is a free-machining brass. The contrasting material properties of free machining and cold working are exceptionally well combined. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2001) 50 (11): Cu-673.
Published: 01 November 2001
... 380 °C (482 716 °F) for 1 3 h. Fabricability: Capacity for being cold worked Poor Hot formability, normally carried Excellent out 650 800 °C (1202 1472 °F) Machinability rating with 100% CuZn39Pb3 = 100% Capacity for being mechanically Good polished Capacity to be electropolished Poor Capacity...
Journal Articles
Alloy Digest (2002) 51 (1): Cu-675.
Published: 01 January 2002
... resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: CU-675. Producer or source: Wieland Metals Inc., Wieland-Werke AG. Producer or Source: Wieland Metals Inc., Wieland-Werke AG Copyright © ASM International® 2002 2002 ASM International chemical...