Skip Nav Destination
Close Modal
Search Results for
low-temperature alloys
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 3687 Search Results for
low-temperature alloys
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1962) 11 (4): SA-127.
Published: 01 April 1962
... elasticity fracture toughness hardness heat treatability joinability low-temperature alloys notch-impact resistance physical properties tensile properties workability COLTUF 28 Filing Code: SA-127 Steel -Alloy APRIL 1962 -DATA ON WORLD WIDE METALS AND ALLOYS Pnblisbed by Engineering Alloys Digest...
Abstract
View article
PDF
COLTUF 28 is a low carbon, manganese type structural steel having high notch-impact resistance and high ductility at subzero temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low temperature performance as well as forming, heat treating, and joining. Filing Code: SA-127. Producer or source: Colvilles Ltd.
Journal Articles
Alloy Digest (1972) 21 (6): SA-276.
Published: 01 June 1972
... International® 1996 1996 ASM International chemical composition corrosion-resistant alloys CRYONIC 5 elasticity fracture toughness heat treatability high-temperature alloys joinability low-temperature alloys machinability physical properties tensile properties workability All CRYONIC 5...
Abstract
View article
PDF
CRYONIC 5 is a 5% nickel-0.50% manganese-0.25% molybdenum steel designed and specially heat treated for use in storage vessels at 275 F or lower. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-276. Producer or source: Armco International Sales.
Journal Articles
Alloy Digest (1980) 29 (2): Ti-75.
Published: 01 February 1980
... RMI 5A1-2.5Sn ELI (ELI = Extra Low Interstitials) is an alpha titanium alloy that was developed for use at cryogenic temperatures. It has a guaranteed minimum yield strength of 100,000 psi at room temperature with good ductility and formability; its yield strength and elongation increase...
Abstract
View article
PDF
RMI 5A1-2.5Sn ELI (ELI = Extra Low Interstitials) is an alpha titanium alloy that was developed for use at cryogenic temperatures. It has a guaranteed minimum yield strength of 100,000 psi at room temperature with good ductility and formability; its yield strength and elongation increase substantially as temperature is lowered. It is used successfully for high-pressure vessels at temperatures below -320 F. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as fracture toughness. It also includes information on low temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ti-75. Producer or source: RMI Company.
Journal Articles
Alloy Digest (1986) 35 (1): SA-414.
Published: 01 January 1986
... ALLOY STEEL 21/4 Ni possesses a combination of moderate strength and superior resistance to brittle fracture at subzero temperatures. It is one of the most economical materials for the construction of equipment to operate at temperatures as low as 90 F. It is intended primarily for welded pressure...
Abstract
View article
PDF
ALLOY STEEL 21/4 Ni possesses a combination of moderate strength and superior resistance to brittle fracture at subzero temperatures. It is one of the most economical materials for the construction of equipment to operate at temperatures as low as 90 F. It is intended primarily for welded pressure vessels. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-414. Producer or source: Alloy steel mills and foundries.
Journal Articles
Alloy Digest (1987) 36 (12): Fe-81.
Published: 01 December 1987
... INCOLOYALLOY909 Filing Code: Iron Alloy Fe-81 - DATA ON WORLD WIDE METALS AND ALLOYS DECEMBER 1887 INCOLOY ALLOY 909 (High-Temperature. Low-Thermal Expansion Alloy) INCOLOY alloy 909 is a high-strength alloy having a constant low coefficient of thermal expansion rigidity up to 1200°F. The alloy is highly...
Abstract
View article
PDF
INCOLOY alloy 909 is a high-strength alloy having a constant low coefficient of thermal expansion and an essentially constant rigidity up to 1200 F. The alloy is highly resistant to thermal fatigue and thermal shock. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Fe-81. Producer or source: Inco Alloys International Inc..
Journal Articles
Alloy Digest (1988) 37 (2): Fe-83.
Published: 01 February 1988
... properties shear strength tensile properties thermal expansion workability INCOLOY ALLOY 907 Filing Code: Fe-83 Iron Alloy - DATA ON WORLD WIDE METALS AND ALLOYS FEBRUARY 1988 INCOLOY* ALLOY 907 (High-Temperature, Low-thermal Expansion Alloy) INCOLOY alloy 907 is a high-strength alloy having a IOU...
Abstract
View article
PDF
INCOLOY alloy 907 is a high-strength alloy having a low coefficient of thermal expansion. It is a precipitation hardening alloy. INCOLOY alloy 907 is useful for gas-turbine components where it provides for closer control of clearances and tolerances. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Fe-83. Producer or source: Inco Alloys International Inc..
Journal Articles
Alloy Digest (1955) 4 (5): Pb-2.
Published: 01 May 1955
... CERROSAFE is a low temperature melting alloy used to accurately proof-cast cavities such as molds, gun chambers, forging dies, etc. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting and joining. Filing...
Abstract
View article
PDF
CERROSAFE is a low temperature melting alloy used to accurately proof-cast cavities such as molds, gun chambers, forging dies, etc. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on casting and joining. Filing Code: Pb-2. Producer or source: Cerro de Pasco Corporation.
Journal Articles
Alloy Digest (1993) 42 (4): Ni-428.
Published: 01 April 1993
... elasticity heat treatability high-temperature alloys microstructure oxidation resistance physical properties thermal properties CRUCIBLE P/M LOW CARBON ASTROLOY Filing Code: Nickel Alloy Ni-428 APRIL 1993 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS tChtlhcMrigMsnemd. P-w AbyllQmI. lnc1201877-9161...
Abstract
View article
PDF
P/M LOW CARBON ASTROLOY offers good ductility and oxidation resistance in addition to excellent strength at high temperatures. This datasheet provides information on composition, physical properties, microstructure, and elasticity as well as creep. It also includes information on high temperature performance as well as heat treating. Filing Code: Ni-428. Producer or source: Crucible Compaction Metals.
Journal Articles
Alloy Digest (1992) 41 (11): Ni-416.
Published: 01 November 1992
... and the mechanical properties requirements of Table 3. One additional requirement is an average ASTM grain size of No. 5 or finer. The alloy s outstanding characteristic is low cycle fatigue life while maintaining strength at temperature. Figure 1 includes data on its low cycle fatigue strength at temperature. Table...
Abstract
View article
PDF
INCONEL Alloy 625LCF is a special alloyed, melted, and processed version of INCONEL alloy 625 (Alloy Digest Ni-121, February 1967) to optimize low-cycle and thermal fatigue up to 1200 deg F (650 deg C). This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: Ni-416. Producer or source: Inco Alloys International Inc..
Journal Articles
Alloy Digest (1980) 29 (11): SA-378.
Published: 01 November 1980
... : 002-6 14X yp Inc Upper Montclair, New Jersey 2X% Nickel Steel (Alloy Steel for Low-Temperature Applications) The 2% Nickel Steel possesses a combination of moderate strength and superior resistance to brittle fracture at subzero temperatures. It is one of the most economical materials...
Abstract
View article
PDF
The 21/4% Nickel Steel possesses a combination of moderate strength and superior resistance to brittle fracture at subzero temperatures. It is one of the most economical materials for the construction of equipment to operate at temperatures as low as -90 F. It is intended primarily for welded pressure vessels. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-378. Producer or source: Alloy steel mills and foundries.
Journal Articles
Alloy Digest (1981) 30 (7): Bi-25.
Published: 01 July 1981
... Ostalloy 255 is a bismuth-base eutectic alloy that melts at the low temperature of 255 F (124 C). After freezing it is characterized by initial shrinkage followed by slow growth. It provides scientists and engineers with an easily castable material that is ready for use practically as soon...
Abstract
View article
PDF
Ostalloy 255 is a bismuth-base eutectic alloy that melts at the low temperature of 255 F (124 C). After freezing it is characterized by initial shrinkage followed by slow growth. It provides scientists and engineers with an easily castable material that is ready for use practically as soon as it freezes. It can be recovered easily and recycled into new uses any number of times. Among its many uses are (1) Anchoring metal parts in glass, (2) Filler for large diameter tubes for bending, (3) Proof casting forging dies, (4) Fusable elements is safely plugs and (5) Mechanical dentistry. This datasheet provides information on composition, physical properties, and hardness. It also includes information on casting, heat treating, and machining. Filing Code: Bi-25. Producer or source: Arconium Corporation of America, A.J Oster Company.
Journal Articles
Alloy Digest (1968) 17 (4): Zr-4.
Published: 01 April 1968
... ZIRCONIUM Gr. 32 is an alloy with a low neutron cross-section, good high temperature mechanical properties and excellent corrosion resistance in water and steam. It is a reactor grade zirconium-tin alloy for corrosion resistance in irradiated water. This datasheet provides information...
Abstract
View article
PDF
ZIRCONIUM Gr. 32 is an alloy with a low neutron cross-section, good high temperature mechanical properties and excellent corrosion resistance in water and steam. It is a reactor grade zirconium-tin alloy for corrosion resistance in irradiated water. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Zr-4. Producer or source: AMAX.
Journal Articles
Alloy Digest (1973) 22 (10): Ni-196.
Published: 01 October 1973
... Ni-Cr 80-20 Alloy is an electrical-resistance alloy suitable for operation at temperatures up to 2100 F (1150 C). It has a low temperature coefficient of resistivity and is also highly resistant to corrosion and oxidation. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
Ni-Cr 80-20 Alloy is an electrical-resistance alloy suitable for operation at temperatures up to 2100 F (1150 C). It has a low temperature coefficient of resistivity and is also highly resistant to corrosion and oxidation. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-196. Producer or source: Electrical resistance alloy producers.
Journal Articles
Alloy Digest (1958) 7 (9): SA-75.
Published: 01 September 1958
... CHATILLON 709 is a low-carbon low-alloy structural steel having good high temperature creep resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high...
Abstract
View article
PDF
CHATILLON 709 is a low-carbon low-alloy structural steel having good high temperature creep resistance. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: SA-75. Producer or source: Societe des Usines St. Jacques.
Journal Articles
Alloy Digest (2008) 57 (4): SA-578.
Published: 01 April 2008
... Mittal Steel T-Star is a high-strength low-alloy (HSLA) multipurpose structural grade with reliable performance in cold weather. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on low temperature performance...
Abstract
View article
PDF
Mittal Steel T-Star is a high-strength low-alloy (HSLA) multipurpose structural grade with reliable performance in cold weather. This datasheet provides information on composition and tensile properties as well as fracture toughness. It also includes information on low temperature performance as well as forming. Filing Code: SA-578. Producer or source: Mittal Steel USA Flat Products.
Journal Articles
Alloy Digest (1974) 23 (1): Cu-274.
Published: 01 January 1974
... Cu-Ni 55-45 Alloy is an electrical-resistance alloy suitable for operation at temperatures up to about 930 F. It has a low temperature coefficient of resistivity and good resistance to corrosion. In thermocouples it can be used up to 1600 F. This datasheet provides information on composition...
Abstract
View article
PDF
Cu-Ni 55-45 Alloy is an electrical-resistance alloy suitable for operation at temperatures up to about 930 F. It has a low temperature coefficient of resistivity and good resistance to corrosion. In thermocouples it can be used up to 1600 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Cu-274. Producer or source: Electrical resistance and thermocouple alloy producers.
Journal Articles
Alloy Digest (1979) 28 (7): SA-362.
Published: 01 July 1979
... Inc., United Nuclear Corporation. Producer or Source: Unicore Inc., United Nuclear Corporation Copyright © ASM International® 1996 1996 ASM International chemical composition corrosion-resistant alloys elasticity fracture toughness heat treatability joinability low-temperature...
Abstract
View article
PDF
UNIFLUX 90 is a continuous flux-cored welding electrode (wire) for welding in carbon dioxide shielding gas in the flat groove and horizontal fillet positions. It was developed to weld high-strength low-alloy steels, but it can be used successfully to weld other low-alloy steels and carbon steels. It is used to deposit typically 2.40% nickel steel weld metal with good low-temperature impact properties. Uniflux 90 is used widely in shipbuilding and other fabricating industries. It provides around 85,000 psi tensile strength and around 25 foot-pounds Charpy V-notch impact at -60 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on low temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: SA-362. Producer or source: Unicore Inc., United Nuclear Corporation.
Journal Articles
Alloy Digest (1990) 39 (7): Al-305.
Published: 01 July 1990
... low-temperature alloys machinability physical properties shear strength tensile properties workability UNS A94032 AA 4032 Filing Code: AI-305 Aluminum Alloy JULY 1990 - DIGEST- DATA ON WORLD WIDE METALS AND ALLOYS PLdsshedby: Amy Digest. Inc 1201-677-9161 27 CanbId Street. Change, N.J. 07050...
Abstract
View article
PDF
AA 4032 has a comparatively low coefficient of thermal expansion and good forgeability. The alloy takes on an attractive dark gray appearance when anodized which may be desirable in architectural applications. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Al-305. Producer or source: Various aluminum companies.
Journal Articles
Alloy Digest (1992) 41 (9): Ti-66.
Published: 01 September 1992
... Ti-6A1-4V and its modification Ti-6A1-4V ELI are moderately age-hardenable titanium alloys, the latter containing extra low interstitials to impart additional toughness at sub-zero temperature. This alloy is the most widely used of all titanium alloys and a great wealth of data exists. Ti-6A1-4V...
Abstract
View article
PDF
Ti-6A1-4V and its modification Ti-6A1-4V ELI are moderately age-hardenable titanium alloys, the latter containing extra low interstitials to impart additional toughness at sub-zero temperature. This alloy is the most widely used of all titanium alloys and a great wealth of data exists. Ti-6A1-4V is characterized as an alpha rich alpha-beta titanium alloy. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ti-66. Producer or source: Timet. Originally published July 1972, revised September 1992.
Journal Articles
Alloy Digest (2015) 64 (10): SS-1228.
Published: 01 October 2015
... Carlson Alloy Nitronic 40 has corrosion resistance superior to 316L and 317L with twice the yield strength at ambient temperatures. Possesses good mechanical properties at both elevated and sub-zero temperatures. Retains low magnetic permeability even after severe cold working or at sub-zero...
Abstract
View article
PDF
Carlson Alloy Nitronic 40 has corrosion resistance superior to 316L and 317L with twice the yield strength at ambient temperatures. Possesses good mechanical properties at both elevated and sub-zero temperatures. Retains low magnetic permeability even after severe cold working or at sub-zero temperatures. This datasheet provides information on composition, physical properties, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1228. Producer or source: G.O. Carlson Inc..