Alloy Digest (1975) 24 (7): Zn-20.
Published: 01 July 1975
... NJZ ALLOY No. 10 is an alloy with medium tensile strength and elongation. It is produced from a high-grade zinc base by additions of cadmium, iron, and lead. It combines good ductility with stiffness and its applications include hardware and laundry tags. This datasheet provides information on...
Journal Articles
Alloy Digest (1976) 25 (1): Zn-25.
Published: 01 January 1976
... strip form, as shown in Table 2. Forms Available: Sheet strip and impact-extrusion fabricated parts. Applications: Laundry tags, sportingequipment components, hard- ware, eyelets, grommets, addressing plates, pre-plating, cable wrappings, fixtures, medallions, jewelry, fashion accessories and watch...