Alloy Digest (1990) 39 (2): Ni-378.
Published: 01 February 1990
... CARPENTER VACUMET HYMU "800" ALLOY is a vacuum melted nickel-iron-molybdenum alloy available in strip form for the manufacture of laminations and tape toroids. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating...
Journal Articles
Alloy Digest (1986) 35 (1): TS-454.
Published: 01 January 1986
... such as draw dies, forming rolls, powder-metal tooling and lamination dies. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on heat treating and machining. Filing Code: TS-454. Producer or source...
Journal Articles
Alloy Digest (2003) 52 (12): SS-897.
Published: 01 December 2003
... DuraFoil-Clad is a laminate composite form of DuraFoil (see Alloy Digest SS-892, November 2003), a heat-resistant ferritic stainless steel with excellent oxidation resistance for high-temperature applications. The material is a metallurgically bonded Al/Fe-Cr stainless steel/Al metallic composite...
Journal Articles
Alloy Digest (2004) 53 (1): Fe-125.
Published: 01 January 2004
.... The laminated Cu/Invar/Cu composite material is metallurgically bonded by roll bonding and normally used in the fully annealed condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance...
Journal Articles
Alloy Digest (2004) 53 (4): Fe-128.
Published: 01 April 2004
... Rotelloy 3 has the same composition as Permandur 49 and was specifically developed for aircraft generator rotor and stator laminations. In addition to a slightly improved magnetic performance, this grade is supplied with guaranteed minimum mechanical properties. This alloy complies...
Journal Articles
Alloy Digest (1969) 18 (4): Ni-144.
Published: 01 April 1969
... Allegheny Ludlum Moly Permalloy is a nickel-iron-molybdenum alloy having excellent permeability and core loss properties. It has high initial and maximum permeability, low coercive force, and low hysteresis loss. It is recommended for toroids, tape and lamination cores. This datasheet provides...
Journal Articles
Alloy Digest (1967) 16 (4): Ni-123.
Published: 01 April 1967
... Carpenter Vacumet HyMu 800 is a vacuum melted nickel-molybdenum-iron alloy recommended as strip for laminations or torroids with a minimum permeability of 65,000 at 40 gauss in strip 0.010-0.001 inch thick. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (1972) 21 (11): Ni-181.
Published: 01 November 1972
... BLENDALLOY 25-7904 is an 80% nickel-15% iron-5% molybdenum alloy having very high permeability and low coercive force for magnetic cores in such applications as transformer laminations, sensitive magnetic amplifiers and magnetic shielding. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1975) 24 (9): Fe-54.
Published: 01 September 1975
... MAGNESIL-O is an oriented silicon-iron alloy of exceptional magnetic qualities designed for applications involving frequencies of 400 Hertz and higher. It has pronounced directional magnetic properties in the direction of rolling. It is recommended for wound cores and stacked laminations which...
Journal Articles
Alloy Digest (1975) 24 (6): Fe-52.
Published: 01 June 1975
.... It is excellent for rotor and stator laminations, and is also a very effective magnetic shielding material. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating...
Journal Articles
Alloy Digest (1975) 24 (7): Fe-53.
Published: 01 July 1975
... MAGNESIL-N is a non-oriented silicon-iron alloy of exceptional magnetic qualities designed for applications involving frequencies of 400 Hertz and higher. It has good permeability in all directions of the rolling plane, and is designed for either punched or sheared laminations with random flux...
Journal Articles
Alloy Digest (1979) 28 (10): Bi-14.
Published: 01 October 1979
... BELMONT ALLOY 2481 is a bismuth-base, non-eutectic alloy that melts through the temperature range 218-440 F. It was developed and used originally for making punch dies to produce transformer laminations from silicon steel sheet. It is now also used to make a wide variety of punch dies and plates...
Journal Articles
Alloy Digest (1989) 38 (9): Cp-2.
Published: 01 September 1989
... K-KARB (Carbon-Carbon) is a graphitized structural graphite fabricated from a graphitized cloth precursor. The layers of graphitized cloth are laminated and bonded together with a graphitic matrix forming a light weight, high strength graphite. This datasheet provides information on physical...
Journal Articles
Alloy Digest (1983) 32 (11): Ni-294.
Published: 01 November 1983
... MAGNIFER 75 is a soft magnetic nickel-iron alloy containing about 5% copper and 2% chromium. It offers very high permeability, very low coercive force and minimum hysteresis loss. It is used primarily for transformers, tape-wound toroids, laminations, shielding and relay parts. This datasheet...
Journal Articles
Alloy Digest (1980) 29 (12): Cu-407.
Published: 01 December 1980
... foot (0.0014-inch thick) for laminating to high-temperature dielectric substrates. This datasheet provides information on composition, physical properties, and elasticity as well as fatigue. It also includes information on forming, heat treating, and machining. Filing Code: Cu-407. Producer or source...
Journal Articles
Alloy Digest (1983) 32 (3): Bi-30.
Published: 01 March 1983
... transformer laminations from silicon sheet steel. Now its many uses include filling blow holes in castings, anchoring dies and non-machinery parts, fixtures, jigs and hold-down bolts in concrete floors. This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Alloy Digest (1984) 33 (2): Ni-291.
Published: 01 February 1984
... MAGNIFER 7904 is a soft magnetic nickel-iron alloy containing about 5% molybdenum. It offers extremely high permeability, very low coercive force and minimum hysteresis loss. It is used primarily for transformers, tape-wound troids, laminations, shielding and relay parts. This datasheet provides...
Journal Articles
Alloy Digest (1987) 36 (9): TS-481.
Published: 01 September 1987
...) for die work on long production runs. It has superior depth of hardening. Its many applications include cold trimmer dies, lamination dies, plug gages, slitting cutters and blanking, stamping and cold-forming dies and punches for long runs. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1991) 40 (8): P-29.
Published: 01 August 1991
... strength, psi Tensile modulus, psi Elongation, o/t Flexural strength, psi Flexural modulus, psi Barcol hardness 1 looo-12000 4.9 x l@ 5.0-6.0 16000-18000 4.5 x 105 35 Table 2 - MECHANICAL PROPERTIES DERAKANE 41 l-35 HAND LAY-UP LAMINATES* Property Flexural strength, ksi Flexural modulus, ksi x l@ Tensile...
Journal Articles
Alloy Digest (1960) 9 (11): Ni-62.
Published: 01 November 1960
... to 0.20 oersteds 1200-1800 Permeability, initial 1500 maximum 2000 Saturation value, gausses 16,000 Retentivity, gausses Bm=200 8 Bm=lO,OOO 3500 Coercive force, oersteds Bm=200 0.005 Bm=lO,OOO 0.5 Hysteresis loss, ergs per cc. Bm=200 0.2 Bm=lO,OOO 1150 io S-rail laminations. The magnetic characteristics...