Alloy Digest (1992) 41 (1): Cer-9.
Published: 01 January 1992
..., AN-291 (Alumina [alundum] kiln furniture) Statistical process control production of these materials assures high quality, high consistency products. Chemical Characterization: The seven material types listed above are alumina (alundum) ceramics bonded with mullite (3AJO,*SiO,) PROPERTIES Table 1...
Journal Articles
Alloy Digest (1992) 41 (4): Cer-11.
Published: 01 April 1992
... ADVANCER NITRIDE BONDED SILICON CARBIDE has exceptional high-temperature strength. Its oxidation resistance assures long life. It is a low-mass ceramic that is ideally suited to kiln furniture. This datasheet provides information on composition, physical properties, elasticity, and shear strength...
Journal Articles
Alloy Digest (1997) 46 (9): SS-696.
Published: 01 September 1997
... UCI-270 is a cast, cobalt and tungsten stabilized, nickel-chromium-iron alloy having unequaled performance in high-temperature applications to 2300 F (1260 C). Among its many uses are components for heat-treating furnaces, cement kilns, petrochemical furnace tubes, and refining furnace tubes...
Journal Articles
Alloy Digest (2002) 51 (5): SS-853.
Published: 01 May 2002
... and improves weldability. Typical uses include furnace parts, heating elements, aircraft and jet engine parts, heat exchangers, carburizing-annealing boxes, sulfite liquor handling equipment, kiln liners, boiler baffles, refinery and chemical processing equipment, and auto exhaust parts. This datasheet...
Journal Articles
Alloy Digest (1967) 16 (12): SS-203.
Published: 01 December 1967
... KANTHAL-DS is a resistance alloy employed advantageously for heavily-stressed electric heating apparatus, and is particularly suitable for heating elements in industrial furnaces and ceramic kilns up to 2335 F. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1970) 19 (5): SS-238.
Published: 01 May 1970
... Kanthal A-1 is a resistance alloy employed advantageously for heavily-stressed electric heating apparatus, and is particularly suitable for heating elements in industrial furnaces and ceramic kilns. Maximum operating temperature 2505 F (1375 C). This datasheet provides information on composition...
Journal Articles
Alloy Digest (1954) 3 (7): SS-16.
Published: 01 July 1954
... KANTHAL-A is a resistance alloy employed advantageously for heavily-stressed electric heating apparatus, and is particularly suitable for heating elements in industrial furnaces and ceramic kilns. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1955) 4 (9): SS-34.
Published: 01 September 1955
... KANTHAL-D is a resistance alloy employed advantageously for heavily-stressed electric heating apparatus, and is particularly suitable for heating elements in industrial furnaces and ceramic kilns. This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (1975) 24 (12): SS-321.
Published: 01 December 1975
... RA 310 is an austenitic chromium-nickel steel with good resistance to corrosion and heat. It is recommended for high-temperature applications such as kilns, thermowells and petrochemical equipment. This datasheet provides information on composition, physical properties, microstructure, hardness...
Journal Articles
Alloy Digest (1977) 26 (10): SS-345.
Published: 01 October 1977
... ALLOY 875 is an iron-chromium-aluminum electrical-resistance alloy with excellent resistance to oxidation at elevated temperatures. It was developed primarily for use as the heating element in industrial furnaces, kilns and other equipment where continuous operating temperatures up to 2350 F may...
Journal Articles
Alloy Digest (1977) 26 (11): SS-228.
Published: 01 November 1977
... SUPERTHERM is a cast nickel-chromium-iron alloy stabilized with cobalt and tungsten. It is used worldwide in extremely high-temperature applications and has unexcelled performance to 2300 F (1260 C). Among its many uses are components for heat-treating furnaces, cement kilns, petrochemical furnace...
Journal Articles
Alloy Digest (1982) 31 (5): SS-407.
Published: 01 May 1982
... low. Among its many applications are combustion chambers, kiln linings, oil-burner components and annealing boxes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature...
Journal Articles
Alloy Digest (1980) 29 (9): SS-375.
Published: 01 September 1980
... applications are recuperators, combustion chambers, kiln linings, stack dampers and oil-burner components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance...
Journal Articles
Alloy Digest (1984) 33 (8): SS-450.
Published: 01 August 1984
... 310S, a few typical uses include annealing boxes, chemical plant equipment, fire box sheets, furnace linings, heat exchangers, oil-refining equipment, kiln linings and tube hangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1970) 19 (11): SS-245.
Published: 01 November 1970
.... Applications include a wide variety of furnace parts, kiln linings, annealing boxes, and silnilat parts. Forms Available: Plate, sheet, strip, bar, wire, seamless tube. Applications: Annealing boxes, baffle plates, burning points, glass molds, oil burner parts, pyrometer tubes, recuperators, valves...
Journal Articles
Alloy Digest (1977) 26 (9): SS-343.
Published: 01 September 1977
...- atures. With regard to applications. Alloy 815 is highly recommended ior use as heating elements in small appliances - such as hot plates, flat-irons. toasters and rhe like - as well as in electric furnaces. kilns. and various orher types of industrial equipment in which rhe maximum continuous operating...
Journal Articles
Alloy Digest (2018) 67 (6): Ni-744.
Published: 01 June 2018
... design. Applications Applications include highly stressed furnace parts, sintering and calcining muffles, cement kiln components resistant to hot abrasion, radiant tubes, and pyrolysis coils. Table 1 At high temperatures short time tests Temperature, °C (°F) Yield strength, MPa (ksi) Ultimate tensile...
Journal Articles
Alloy Digest (2018) 67 (7): Ni-745.
Published: 01 July 2018
... stressed furnace parts, sintering and calcining muffles, cement kiln components resistant to hot abrasion, radiant tubes, and pyrolysis coils. Table 1 Chart of stress-rupture properties Temperature, °C (°F) Avg initial stress for 100,000 h creep rupture, MPa (ksi) Avg stress for a creep rate of 0.0001 %/h...
Journal Articles
Alloy Digest (1992) 41 (8): Ni-408.
Published: 01 August 1992
... Specification Equivalents: DIN 17470: Cronix 80,70 ASTM B344: Cronix 80 Characterization and Typical Application: CRONIX 80E has high heat strength at elevated tem- peratures and is used for electric fnmaces and kilns; enamel ovens; unsupported heating elements; and tubu- lar elements. Heavy duty precision...
Journal Articles
Alloy Digest (1992) 41 (9): SS-534.
Published: 01 September 1992
... Specification Equivalents: ASTM B603 Aluchrom Alloy class1 0 CIZISSIIA I ChSSIIB S CbSSIIl W Characterization and Typical Application: Alucheom 0, I, S and W are ferritic stainless steels and magnetic: ail have high operating temperatures and are used in furnaces and kilns. Aluchrom 0 has the highest...