1-20 of 39 Search Results for

k monel

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1955) 4 (3): Ni-17.
Published: 01 March 1955
... K MONEL is a corrosion-resistant wrought alloy of nickel, copper and aluminum. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature...
Journal Articles
Alloy Digest (1955) 4 (4): Ni-18.
Published: 01 April 1955
... KR MONEL is a corrosion-resistant wrought alloy of nickel, copper and aluminum. It is the free-cutting grade of K Monel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as...
Journal Articles
Alloy Digest (1966) 15 (11): Ni-119.
Published: 01 November 1966
... MONEL Alloy K-500 combines the excellent corrosion resistance characteristics of the MONEL nickel-copper alloys with the added advantages of greaterr strength and hardness. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties and...
Journal Articles
Alloy Digest (1985) 34 (2): Ni-310.
Published: 01 February 1985
... MONEL Welding Electrode 190 is used for shielded-metal-are welding of MONEL Alloys 400, 404, R-405 and K-500. It also is used for surfacing of steel. Dissimilar-welding applications for Welding Electrode 190 include joints between MONEL nickel-copper alloys and carbon steel, low-alloy steel...
Journal Articles
Alloy Digest (1985) 34 (9): Ni-321.
Published: 01 September 1985
... MONEL Filler Metal 60 is a nickel-base alloy used for gas-tungsten-arc, gas-metal-arc and submerged-arc welding of MONEL. alloys 400, 400, R-405 and K-500. It also is used for surfacing of steel. The weld metal deposited by Filler Metal 60 has properties similar to those of MONEL. alloy 400. It...
Journal Articles
Alloy Digest (1970) 19 (9): Ni-157.
Published: 01 September 1970
... MONEL alloy 502, a modification of MONEL alloy K-500, provides improved machinability. It maintains high strength up to about 800 F and has good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1955) 4 (2): Ni-16.
Published: 01 February 1955
...: 900 242 358 1000 246 1 55 z2 1200 250 325 (Specimens iz? held at testing temperature ?f 5 minutes before determininze hardness.) DOI: 10.31399/asm.ad.ni0016 Copyright © ASM International® 1996 Table 6 - RESISTANCE TO GALLING IN ROTARY RUBBING CONTACT OF PLANE SURFACES Alloy Monel* K * Monel Ni-Hard...
Journal Articles
Alloy Digest (1998) 47 (6): Cu-617.
Published: 01 June 1998
... Monel Electrode 187 is an all-position copper-nickel welding electrode that meets all the requirements of applicable U.S. military specifications. The all-position electrode is of major importance in boatyards and desalination plants in resistance to pitting corrosion and avoidance of the danger...
Journal Articles
Alloy Digest (1955) 4 (12): Ni-21.
Published: 01 December 1955
... MONEL is a general purpose nickel-copper alloy having excellent combination of high strength, ductility and corrosion resistance. Cold-worked, welded and cast forms behave substantially the same under corrosive conditions. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1957) 6 (5): Ni-34.
Published: 01 May 1957
... R MONEL is a general purpose nickel-copper alloy having excellent combination of high strength, ductility and corrosion resistance. It is the free-cutting grade of Monel. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Alloy Digest (1964) 13 (7): Ni-93.
Published: 01 July 1964
... MONEL alloy 400 is a general purpose nickel-copper alloy having excellent combination of high strength, ductility, and corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep...
Journal Articles
Alloy Digest (1968) 17 (3): Cu-186.
Published: 01 March 1968
... joining. Filing Code: Cu-186. Producer or source: H. K. Porter Company Inc.. Producer or Source: H. K. Porter Company Inc. Copyright © ASM International® 1996 1996 ASM International chemical composition elasticity Excelsior hardness heat treatability joinability physical properties...
Journal Articles
Alloy Digest (1991) 40 (11): Co-82.
Published: 01 November 1991
... resists pitting and crevice corrosion. Being extremely noble, MP35N alloy cau induce galvanic corrosion in AISI Type 316 stainless or K-Monel* when coupled to those mateti- als. *K-Mancl is a uadcmark of Huntington Alloys Reduction of Area 90 60.0 59.0 57 51 47 Table 7 - CHARPY V-NOTCH IMPACT (Cold drawn...
Journal Articles
Alloy Digest (2014) 63 (12): Co-124.
Published: 01 December 2014
... crevice corrosion. As this alloy is an extremely noble alloy, this can result in galvanic corrosion when electrically coupled with more active metals such as carbon steel, type 316 stainless, or K Monel. This alloy is included in NACE MR0175 to a maximum hardness of Rockwell HRC 35 (maximum hardness of...
Journal Articles
Alloy Digest (2005) 54 (10): Cu-737.
Published: 01 October 2005
... ksi acceptability behavior resistance Marinel 230 862 125 Acceptable Good Good Monel 760 110 Acceptable Poor Poor K-500 Titanium 760 110 Acceptable Poor Poor Grade 5 Be-Cu, aged 965 140 Subject to restriction Good Good DOI: 10.31399/asm.ad.cu0737 The manufacturer offers additional ultrasonic testing...
Journal Articles
Alloy Digest (2005) 54 (9): Cu-736.
Published: 01 September 2005
... 720 104 Can be susceptible Poor Poor fastener grade Monel K-500 760 110 Susceptible Poor Poor Titanium grade 5 760 110 Can be susceptible Poor Poor Marinel 220 700 102 Immune Good Good DOI: 10.31399/asm.ad.cu0736 erosion corrosion. Strength is at least 650 MPa (94 ksi) across the entire size range...
Journal Articles
Alloy Digest (1960) 9 (12): Ni-63.
Published: 01 December 1960
... against other hardened materials such as hardened steel, against itself, or ocher age-hardenable nickel alloys such as Ioconel X , K Monel, or Duranickel. If it is used against softer materials, galling is likely to occur. Forms Available: Castings Applications: Cast parts in processing equipment for...
Journal Articles
Alloy Digest (1958) 7 (5): Ti-16.
Published: 01 May 1958
...-70 than it is for K-Monel or AISI 431 stainless Std. Forms Available: Sheet, strip, plate, tubing, billets, bars and wire. Applications: Moderately stressed aircraft parts and all types of corrosion resisting applications. Manufacturer: Rem-Cm Titanium, Inc. Midland, Pennsylvania ...
Journal Articles
Alloy Digest (1998) 47 (11): Ni-547.
Published: 01 November 1998
...: DATA ON WORLD WIDE METALS AND ALLOYS k%opynghf 199s. ASM Intemationa. All riglns reserved. Data shown are rypicai, not to be USdbrspecjficabbnOrfi~design. FUblMed by A.94 Iniema&mal Materials park. Ohio 44073-mz 440-338-5151 Fax440-33B-4634 Mem-Serv@w.ASM-lnttorg COLMONOY 730 (Nickel-Base Hard...
Journal Articles
Alloy Digest (2000) 49 (10): Cu-29.
Published: 01 October 2000
... (1780 1990) Coefficient of linear expansion, 17.6 (9.8) 10 6/K (10 6/ F) Thermal conductivity, W/m K 197 (113) (Btu/(ft h F)) Electrical conductivity, %IACS 48 Resistivity, m ( circular-mil/ft) 0.0359 (21.6) See also Tables 3 and 4. Mechanical Properties: Elastic modulus, GPa (106 psi) 117...