Alloy Digest (2007) 56 (9): Cu-751.
Published: 01 September 2007
... Wieland-BC8 is a phosphor bronze containing finely distributed lead particles. BC9 is a bronze alloy with high polishability and is often used in the jewelry industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1985) 34 (2): Ag-11.
Published: 01 February 1985
... hardener than other metals that have been considered; however, copper lowers the melting point substantially and lowers the electrical and thermal conductivities appreciably. Sterling Silver is used for flat and hollow tableware, various items of jewelry and special industrial applications. This datasheet...
Journal Articles
Alloy Digest (2000) 49 (12): Cu-646.
Published: 01 December 2000
... allergy-causing nickel-base copper alloys in the eyeglass and jewelry industries. The alloy meets the re- quirements of the rapidly expanding mobile telecommunications market. Product Forms Available: SM900R is delivered in the form of drawn round cross sections. It is delivered in small diameters as rods...
Journal Articles
Alloy Digest (2001) 50 (2): Cu-658.
Published: 01 February 2001
... as rods (0.600 in. max diameter), wire in coils (0.020 in. min diameter), and in drums (0.120 in. max). Applications: Typical applications include electronic contacts, fiber-optic connections, screws, and components for the eyeglass and jewelry industries. Table 1 Typical Mechanical Properties of Rods...
Journal Articles
Alloy Digest (2020) 69 (12): Ti-173.
Published: 01 December 2020
... or moisture) exists in the environment. Biocompatibility TiAl6V4 exhibits very good biological compatibility with human tissues and bones. For this reason, the alloy is used extensively for medical applications and in the jewelry industry. Hot Forming Conventional Forging. Heat to 980 °C (1800 °F). Wait...
Journal Articles
Alloy Digest (2021) 70 (10): Cu-925.
Published: 01 October 2021
...; costume jewelry; Industrial dials; fire extinguisher cases; lipstick containers; Wieland Rolled Products NA (formerly Olin Brass) medallions; nameplates; plaques; rouge boxes; 4801 Olympia Park Plaza, Suite 3500 Other tokens; zippers. Louisville, Kentucky 40241, USA Plumbing Tel: +1 502 873 3000 AC motors...
Journal Articles
Alloy Digest (2020) 69 (9): Ti-170.
Published: 01 September 2020
... tissues and bones. This is the reason for the increasing demand for these grades in medical applica- tions and the jewelry industry. Formability CP titanium grades have good hot and cold formability. Their capability for forming increases with decreasing content of interstitials, especially oxygen...
Journal Articles
Alloy Digest (1981) 30 (12): Cu-427.
Published: 01 December 1981
... as well as for decorative purposes. Among its many uses are slide fasteners, wire for screens of all types, electrical connectors, costume jewelry and platers bars in the manufacture of gold-plated articles. *ANACONDA is a registered trademark of Anaconda Industries. Composition: Copper zinc Nominal 87.5...
Journal Articles
Alloy Digest (1976) 25 (9): Zn-28.
Published: 01 September 1976
... NJZ Alloy No. 50 is a zinc-lead-cadmium-iron alloy characterized by high ductility with medium hardness. It can be work hardened slightly, has medium strength and an excellent surface. Its many uses include hardware and embossing jewelry. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1983) 32 (3): Cu-455.
Published: 01 March 1983
... rolls, razor handles and costume jewelry. *ANACONDA is a registered trademark of Anaconda Industries. Composition: Physical Properties: Copper Zinc Nominal 85 15 Density, lb/cu in. (At 68 F) 0.316 Specific gravity 8.75 Melting range, OF (Solidus-Liquidus) 181&1877 Specific heat, Btu/lb/ F (At 68°F) 0.09...
Journal Articles
Alloy Digest (1984) 33 (4): Cu-474.
Published: 01 April 1984
... Copper Alloy No. C40800 is brass with an addition of tin (nominally 2%). It can be machined and formed successfully. It can be joined by several methods and as good resistance to corrosion. A typical use is electrical connectors but it also can be used for bushings, washers and costume jewelry...
Journal Articles
Alloy Digest (1975) 24 (4): Cu-296.
Published: 01 April 1975
... Copper Alloy No. 411 is brass with a small addition of tin. It has good formability, weldability and corrosion resistance and is recommended for such applications as bearings, bushings, jewelry and stamped hardware. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1982) 31 (1): Cu-430.
Published: 01 January 1982
... Copper Alloy No. C41300 is brass with an addition of 1% tin. It has moderate strength and good ductility. It has a good combination of formability, joinability and resistance to corrosion. Typical uses comprise jewelry products, components for electrical switchgear, bushings and hardware...
Journal Articles
Alloy Digest (2009) 58 (6): Cu-771.
Published: 01 June 2009
... Ansonia alloy C22000 is a 10% Zn alloy with the previous trade name of Commercial Bronze. It is bronze in color and often used in costume jewelry and ornamental trim. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It also...
Journal Articles
Alloy Digest (1975) 24 (4): Zn-18.
Published: 01 April 1975
... by conventional processes including spinning and its applications include such items as deep-drawn cans and jewelry. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep and fatigue. It also includes information on corrosion resistance as well...
Journal Articles
Alloy Digest (1977) 26 (11): Ni-251.
Published: 01 November 1977
... molding where corrosion and high operating mold temperatures are factors. The fluidity and color of the alloy appeal to the jewelry trade. Manufacturer: Kawecki Berylco Industries, Inc. Reading, Pennsylvania 19603. ...
Journal Articles
Alloy Digest (1982) 31 (10): Ni-279.
Published: 01 October 1982
..., corrosion and oxidation. The applications for Berylco Alloy 42C include cast-to-shape jewelry, surgical instruments, valves, pumps and dental alloys. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (1980) 29 (11): Cu-406.
Published: 01 November 1980
... enough for use in industrial and engineering applications, yet exceptionally malleable for extensive use as the base metal for coins, costume jewelry, medallions and ornamental trim. It also provides an excellent base for coating with vitreous enamels and gold plating. Among this alloy s other noteworthy...
Journal Articles
Alloy Digest (2002) 51 (12): Cu-694.
Published: 01 December 2002
... and excellent deep-drawing properties. This makes it a popular choice for the production of metal articles and jewelry. It also has good electrical conductivity and is highly suitable for applications in the electrical industry. In sheet form this alloy can also be used for internal and external architectural...
Journal Articles
Alloy Digest (1978) 27 (5): Cu-353.
Published: 01 May 1978
... this job. The soldering alloys, brazing alloys and fluxes are conventional products available through regular sources. Corrosion Resistance: Belmont ahoy 4582 has good resistance to industrial, rural and marine atmospheres, petroleum products, alcohols, dry gases and sea water. It has fairly good...