1-20 of 87 Search Results for

jet turbine components

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (6): Ni-434.
Published: 01 June 1993
... P/M RENE 95 is a high strength, high temperature alloy used for rotating jet turbine components. Supersolvus P/M Rene 95 provides even higher temperature creep and stress-rupture resistance than standard Rene 95. Both are available as-HIP performs. A typical application is a high pressure turbine...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (4): Ni-267.
Published: 01 April 1981
... in sheet form; consequently, it is used widely for jet engine components. Other uses include turbine buckets, turbine wheels, rings and high-temperature fasteners and springs. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (5): SA-304.
Published: 01 May 1974
... range of 300 to 600 F, and components for spacecraft, jet engines and gas turbines. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on high temperature...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (10): Co-79.
Published: 01 October 1981
... and precision castings Applications: Turbine blades, rotors, aerospace parts, high-temperature hard- ware, and various component parts for jet-propulsion engines, commercial gas turbines and turbo superchargers Manufacturers: Weldability: AISI No. 671 can be welded satisfactorily by ail of the usual...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (1): Co-60.
Published: 01 January 1970
... CML-605 is a cobalt-base alloy having high strength, heat and oxidation resistance at elevated temperatures above 1600 F. It is recommended for gas turbine and jet engine components operating in the 1600 to 2000 F temperature range. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1970) 19 (5): Ni-153.
Published: 01 May 1970
... NIMONIC 93 is a nickel-base alloy having high elevated temperature strength, high oxidation resistance and good corrosion resistance. It is recommended for jet engine and gas turbine components. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1965) 14 (10): SS-173.
Published: 01 October 1965
... for turbine and jet engine components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (7): SS-196.
Published: 01 July 1967
... Allegheny Ludlum 419 is a ferritic (martensitic) type chromium-tungsten alloy recommended for high temperature applications in the temperature range of 800-1200 F, such as turbine and jet engine components. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (9): Ni-127.
Published: 01 September 1967
... CM-R41 is a vacuum-melted, precipitation hardening nickel-base alloy possessing outstanding properties in the temperature range of 1200 F to 1800 F. It is recommended for jet engine and gas turbine components operating at high temperatures. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (9): SS-200.
Published: 01 September 1967
... AISI No. 616 is a hardenable martensitic type stainless steel recommended for high temperature applications up to 1200 F. It is used for steam turbine blades and buckets, valves, jet engine components, and high temperature bolting. This datasheet provides information on composition, physical...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (2): Ni-131.
Published: 01 February 1968
... GMR-235 Alloy is a nickel-base, precipitation-hardening alloy available in investment cast form for high temperature service. It is recommended for gas turbine and jet engine components operating in excess of 1400 F. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (8): SS-212.
Published: 01 August 1968
... CMN-155 is an austenitic iron-base alloy having high oxidation and heat resistance combined with good high temperature properties. It is recommended for jet engine and gas turbine components, high temperature fasteners, and rocket chambers. This datasheet provides information on composition...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (11): SS-478.
Published: 01 November 1986
... superalloy with a relatively high ratio of strength to alloying element content. It is capable of withstanding high static and dynamic stresses through at least I 200 F. It is used for various high-temperature applications such as components for jet engines. gas turbines. turbochargers and missiles...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (2): SS-152.
Published: 01 February 1964
... strength at temperatures up co and including 1100oF. Fom s Available: Billets, hot rolled and cold finished bars, wire, cold rolled strip, and special shapes. Applications: Jet engine and steam turbine components, aircraft structural parts. Turbine blades, wheels, discs and turbine shafts. Manufacturer...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1996) 45 (12): Ni-519.
Published: 01 December 1996
.... and Metco 5P/6P Spray guns and the corresponding parameters for using the Metco Diamond Jet are available from the producer. Typical Applications: Production of Alloy 625 components in gas turbines, chemical process equipment offshore, and pulp and paper industries where exceptional corrosion resistance...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (5): Ni-404.
Published: 01 May 1992
... corrosion resistance up to 1600°F (871 C). Forms Available: Billets, bar, forgings, redraw coil. Applications: Turbine blades, turbine and compressor discs, shafts, spacers. fasteners and miscellaneous jet engine hardware. Producer: Teledyne Allvac Monroe, North Carolina 281 lo-0531 699 ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1973) 22 (11): Ni-197.
Published: 01 November 1973
... such as afterburner parts, turbine casings, wheels, buckets, and high temperature bolts and fasteners. Forms Avbilable: Billets, forgings and bars (hot rolled, annealed and heat treated). Applications: Jet engine and highspeed airframe components, afterburner parts, turbine casings, wheels, buckets, and high...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (5): Ni-124.
Published: 01 May 1967
... and forgings, wire, sheer, strip, place, ingots and ocher forms. Applications: Heavy-duty jet engine and gas turbine buckets, high temperature bolting, jet engine turbine wheels and ocher critical jet engine components. Manufacturer: Special Metals, Inc. New Hartford, New York ...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1964) 13 (9): Co-40.
Published: 01 September 1964
... strength requirements. Forms Available: Investment castings. Applications: l Ventral 523 or water soluble oil. l * Use a standard 3-flute tap; diameters smaller than 0.375 are difficult co tap. Turbine nozzle vanes in jet engines, gas turbine components requiring high strength properties in the 1000...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (4): Ni-216.
Published: 01 April 1975
..., Ti) type. Pyromet 901 is used for components in aircraft and gas turbines. such as turbine rotors, compressor discs, hubs, and shafts. This alloy is available as induction- vacuum plus vacuumarc-remelted material. Forms Available: Forging billets, hot and cold finished bars, strip and wire...