1-13 of 13 Search Results for

isotropy

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1979) 28 (4): SA-358.
Published: 01 April 1979
... Cabot ESR HY 140 is a 5Ni-Cr-Mo-V alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting (ESR) by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and toughness...
Journal Articles
Alloy Digest (1979) 28 (9): SA-364.
Published: 01 September 1979
... CABOT ESR 4330 Mod is a modified 4330 alloy steel produced by electric-furnace, melting, vacuum degassing and electroslag remelting (ESR) by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility...
Journal Articles
Alloy Digest (1980) 29 (4): SA-371.
Published: 01 April 1980
... CABOT ESR 4140 is a chromium-molybdenum alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and toughness...
Journal Articles
Alloy Digest (1983) 32 (4): SA-388.
Published: 01 April 1983
... isotropy, ductility and toughness. This steel is ideally suited for many critical applications in oil-field and power-generating equipment as well as for machinery in the metalworking, chemical-process and construction fields. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1983) 32 (6): SA-391.
Published: 01 June 1983
... INGERSOLL-RAND OILFIELD PRODUCTS ESR 4140 is a chromium-molybdenum alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility and toughness. ESR 4140...
Journal Articles
Alloy Digest (1983) 32 (9): SA-393.
Published: 01 September 1983
... INGERSOLL-RAND ESR HY 140 is a 5Ni-Cr-Mo-V alloy steel produced by electric-furnace melting, vacuum degassing and electroslag remelting (ESR) by use of small-heat-size technology. Electroslag refining improves cleanliness and lowers the sulfur content to provide improved isotropy, ductility...
Journal Articles
Alloy Digest (1987) 36 (11): Be-7.
Published: 01 November 1987
... as an optical support bench because of its high degree of isotropy and good micro-yield strength. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming...
Journal Articles
Alloy Digest (2013) 62 (9): TS-721.
Published: 01 September 2013
... and are summarized below: Good macro and microstructure with lowest levels of segregation Lowest gas contents Lowest levels of unwanted trace elements Excellent homogeneity and isotropy Highest degree of cleanliness Highest toughness Best polishability Best thermal conductivity Highest dimensional...
Journal Articles
Alloy Digest (2007) 56 (6): TS-650.
Published: 01 June 2007
... is characterized good macro- and microstructure with low levels of segregation, low gas contents, low levels of unwanted trace elements, excellent homoge- neity and isotropy, a high degree of cleanliness, high toughness, polishability, best thermal conductivity, high dimensional stability during heat treatment...
Journal Articles
Alloy Digest (1973) 22 (7): SA-291.
Published: 01 July 1973
...: 10.31399/asm.ad.sa0291 Copyright © ASM International® 1996 The similarity of transverse and longitudinal notch toughness values illustrates the relative isotropy of this oroduct. .ll LONGITUDINAL Numbers on curves are sheet thickness- es. -50 -25 0 +25 +YJ +75 +100 TEMPERATURE OF . -50 -25 0 +25 +.50 +75...
Journal Articles
Alloy Digest (2021) 70 (1): Co-132.
Published: 01 January 2021
... and 100 µm (1770 and from 1220 to 760 °C (2230 to 1400 °F) should be not more 3935 µin The limit on the minimum particle size ensures than 8 minutes. The purpose of this treatment is to dissolve safe handling of the powder. the carbides and improve the isotropy of the microstructure, thus reducing...
Journal Articles
Alloy Digest (1979) 28 (3): SA-356.
Published: 01 March 1979
... FORMABLE 50 HR and con- vantional high-strength low-alloy steel of 50.ksi yield strength. Data are based on subsizad Charpy (V-notch) specimens with the as-rolled surface intact. The similarity of longitudinal and transversa data for FORMABLE 50 HR illustrate its relative isotropy. Heat Treatment: Armco...
Journal Articles
Alloy Digest (2000) 49 (7): Cu-650.
Published: 01 July 2000
... with both longitudinal and trans- verse bends posing no forming problems. Certain mill hardenend tempers also have low directionality. Because of this isotropy, special consider- ation does not have to be given to the manner in which parts are stamped relative to the rolling direction. Corrosion Resistance...