Skip Nav Destination
Close Modal
Search Results for
isotropic properties
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 61 Search Results for
isotropic properties
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (2007) 56 (8): TS-653.
Published: 01 August 2007
... Orvar Superior is a premium Cr-Mo-V alloyed hot-work die steel with good resistance to thermal fatigue. The name “superior” is used to indicate that close control in special melting and refining has attained a high purity and very fine structure that produces isotropic properties. This datasheet...
Abstract
View article
PDF
Orvar Superior is a premium Cr-Mo-V alloyed hot-work die steel with good resistance to thermal fatigue. The name “superior” is used to indicate that close control in special melting and refining has attained a high purity and very fine structure that produces isotropic properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-653. Producer or source: Böhler-Uddeholm North America.
Journal Articles
Alloy Digest (1988) 37 (10): TS-493.
Published: 01 October 1988
... ORVAR SUPREME is a chromium-molybdenum-vanadium alloyed steel. Special processing techniques and close control are responsible for its high purity and very fine structure. It has improved isotropic properties. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
ORVAR SUPREME is a chromium-molybdenum-vanadium alloyed steel. Special processing techniques and close control are responsible for its high purity and very fine structure. It has improved isotropic properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-493. Producer or source: Uddeholm Corporation.
Journal Articles
Alloy Digest (1998) 47 (2): SS-707.
Published: 01 February 1998
... Finkl 420 Premium Quality stainless steel is a modification of AISI 420 with vacuum arc degassing and vacuum arc remelting. The modification results in a refined structure yielding cleanliness, strength, and isotropic properties. This datasheet provides information on composition, physical...
Abstract
View article
PDF
Finkl 420 Premium Quality stainless steel is a modification of AISI 420 with vacuum arc degassing and vacuum arc remelting. The modification results in a refined structure yielding cleanliness, strength, and isotropic properties. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating. Filing Code: SS-707. Producer or source: A. Finkl & Sons Company.
Journal Articles
Alloy Digest (2009) 58 (7): SA-604.
Published: 01 July 2009
... OvaX 600 is an ingot cast through-hardening steel that is specially designed for air hardening or gas quenching and for applications requiring isotropic properties and very high cleanliness levels. This datasheet provides information on composition, hardness, and tensile properties. It also...
Abstract
View article
PDF
OvaX 600 is an ingot cast through-hardening steel that is specially designed for air hardening or gas quenching and for applications requiring isotropic properties and very high cleanliness levels. This datasheet provides information on composition, hardness, and tensile properties. It also includes information on casting, forming, and heat treating. Filing Code: SA-604. Producer or source: Ovako North America Inc.
Journal Articles
Alloy Digest (1987) 36 (1): TS-469.
Published: 01 January 1987
... CARPENTER 883 PLUS is a premium quality die-casting die steel. It is electroslag remelted and this together with processing adaptations give it metallurgical consistency and improved isotropic properties. This datasheet provides information on composition, hardness, and tensile properties as well...
Abstract
View article
PDF
CARPENTER 883 PLUS is a premium quality die-casting die steel. It is electroslag remelted and this together with processing adaptations give it metallurgical consistency and improved isotropic properties. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-469. Producer or source: Carpenter. See also Alloy Digest TS-529, July 1994.
Journal Articles
Alloy Digest (2010) 59 (1): SA-612.
Published: 01 January 2010
... hardenability ensures a through hardenability of large sections. Ovako Designation 255 G. This is a premium bearing quality variant with low sulfur content and high cleanliness demands. 255 Q. This variant has isotropic properties and better fatigue strength resulting from higher cleanliness levels and a finer...
Abstract
View article
PDF
Ovako 253 is steel developed primarily for case hardening with high toughness. This datasheet provides information on composition and hardness. It also includes information on forming and heat treating. Filing Code: SA-612. Producer or source: Ovako North America Inc.
Journal Articles
Alloy Digest (2018) 67 (11): SS-1298.
Published: 01 November 2018
... Composition, wt.% (Nominal) Carbon < 0.045 Chromium 16 Nickel 5 Molybdenum 1 Iron bal Physical Properties Density, kg/m3 (lb/in.3) 7700 (0.277) Thermal expansion mean values, 20 200 °C (68 392 °F), 10 6/K (10 6/°F) 10.8 (6.0) Mechanical Properties Hot isostatic pressed components have isotropic properties...
Abstract
View article
PDF
Sandvik APM 9980 is a low-carbon martensitic stainless steel with high mechanical properties. APM 9980 is a martensitic stainless steel specially designed for those applications requiring high mechanical properties combined with improved corrosion resistance relative to traditional martensitic steels. Note: This material is made by hot isostatic pressing of components. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-1298. Producer or source: Sandvik Materials Technology and Sandvik AB Sweden.
Journal Articles
Alloy Digest (2018) 67 (12): SS-1299.
Published: 01 December 2018
..., at T/4. Hot isostatic pressed components have isotropic properties, meaning the mechanical properties are similar in all directions. See Table 1 for proof strength at temperatures. Proof strength, Rp0.2, MPa (ksi) Minimum 550 (80) Typical 620 (90) Tensile strength, Rm, MPa (ksi) Minimum 800 (116...
Abstract
View article
PDF
Sandvik APM 2327 is a powder metallurgical hot isostatic pressed product that is a super duplex stainless steel with improved mechanical properties, corrosion resistance, and superior corrosion fatigue performance over conventional duplex grades. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-1299. Producer or source: Sandvik Materials Technology.
Journal Articles
Alloy Digest (2013) 62 (10): Nd-5.
Published: 01 October 2013
... NEOQUENCH-P GRADE NP-8 is one of a series of isotropic polymer bonded magnets based on Nd-Fe-B. The raw material powder is manufactured by rapid quenching of prescribed alloys into nanocrystalline flakes that are subsequently annealed for optimum magnetic properties. This alloy is an isotropic...
Abstract
View article
PDF
NEOQUENCH-P GRADE NP-8 is one of a series of isotropic polymer bonded magnets based on Nd-Fe-B. The raw material powder is manufactured by rapid quenching of prescribed alloys into nanocrystalline flakes that are subsequently annealed for optimum magnetic properties. This alloy is an isotropic bonded magnet mixed with Sm-Fe-N powder and resin bond. This datasheet provides information on physical properties and bend strength. It also includes information on powder metal forms. Filing Code: Nd-5. Producer or source: Daido Steel (America) Inc..
Journal Articles
Alloy Digest (2019) 68 (2): SS-1302.
Published: 01 February 2019
...) Mechanical Properties Hot isostatic pressed components have isotropic properties, meaning the mechanical properties are similar in all directions. See below for mechanical properties and proof stress at 20 °C (68 °F). Minimum values according to ASTM 988. Proof strength at elevated temperatures are: Proof...
Abstract
View article
PDF
Sandvik APM 2377 is a powder metallurgical, molybdenum-alloyed, hot isostatic pressed product that is an austenitic/ferritic duplex stainless steel with improved corrosion resistance in stress-corrosion cracking over austenitic stainless steels. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-1302. Producer or source: Sandvik Steel Company.
Journal Articles
Alloy Digest (2019) 68 (1): SS-1301.
Published: 01 January 2019
... (continued) Hot isostatic pressed components have isotropic properties, meaning the mechanical properties are similar in all directions. Heat Treatment The products are delivered in the heat-treated condition. If additional heat treatment is needed due to further processing, the following is recommended...
Abstract
View article
PDF
Sandvik APM 2354 is a powder metallurgical, molybdenum alloyed, hot isostatic pressed product that is an austenitic stainless steel with improved corrosion resistance over AISI Type 304 and 304L. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on corrosion resistance as well as machining and joining. Filing Code: SS-1301. Producer or source: Sandvik Steel Company.
Journal Articles
Alloy Digest (2004) 53 (9): SS-909.
Published: 01 September 2004
... Stavax Supreme is a stainless tool steel produced by special melting techniques. The alloy has excellent polishability, isotropic mechanical properties, a unique composition, and excellent corrosion resistance. This datasheet provides information on physical properties, hardness, elasticity...
Abstract
View article
PDF
Stavax Supreme is a stainless tool steel produced by special melting techniques. The alloy has excellent polishability, isotropic mechanical properties, a unique composition, and excellent corrosion resistance. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: SS-909. Producer or source: Böhler Edelstahl GMBH, Böhler-Uddeholm N. America.
Journal Articles
Alloy Digest (1993) 42 (8): Ni-439.
Published: 01 August 1993
... P/M N690 exhibits isotropic mechanical properties and excellent corrosion resistance. Its high chromium content provides superior resistance to IGSCC. This alloy has superb weldability characteristics as well as minimal mechanical property degradation during extended exposure to elevated...
Abstract
View article
PDF
P/M N690 exhibits isotropic mechanical properties and excellent corrosion resistance. Its high chromium content provides superior resistance to IGSCC. This alloy has superb weldability characteristics as well as minimal mechanical property degradation during extended exposure to elevated temperatures. This datasheet provides information on composition, microstructuretensile properties. It also includes information on corrosion resistance. Filing Code: Ni-439. Producer or source: Crucible Compaction Metals.
Journal Articles
Alloy Digest (2013) 62 (5): Nd-4.
Published: 01 May 2013
... NEOQUENCH-P GRADE NP-7L is one of a series of isotropic polymer bonded magnets based on Nd-Fe-B. The raw material powder is manufactured by rapid quenching of prescribed alloys into nanocrystalline flakes that are subsequently annealed for optimum magnetic properties. NP-7L is made by compression...
Abstract
View article
PDF
NEOQUENCH-P GRADE NP-7L is one of a series of isotropic polymer bonded magnets based on Nd-Fe-B. The raw material powder is manufactured by rapid quenching of prescribed alloys into nanocrystalline flakes that are subsequently annealed for optimum magnetic properties. NP-7L is made by compression molding. This datasheet provides information on and physical properties. It also includes information on powder metal forms. Filing Code: Nd-4. Producer or source: Daido Steel (America) Inc..
Journal Articles
Alloy Digest (1987) 36 (11): Be-7.
Published: 01 November 1987
... BRUSH WELLMAN I-220 is an instrument grade of beryllium strengthened by a dispersion of 2.2% beryllium oxide maximum. It has a micro-yield strength of 5000 psi minimum. I-220B is manufactured from impact ground powder and therefore is more isotropic than BRUSH WELLMAN S-200E. I-220 is often used...
Abstract
View article
PDF
BRUSH WELLMAN I-220 is an instrument grade of beryllium strengthened by a dispersion of 2.2% beryllium oxide maximum. It has a micro-yield strength of 5000 psi minimum. I-220B is manufactured from impact ground powder and therefore is more isotropic than BRUSH WELLMAN S-200E. I-220 is often used as an optical support bench because of its high degree of isotropy and good micro-yield strength. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Be-7. Producer or source: Brush Wellman Inc..
Journal Articles
Alloy Digest (1989) 38 (11): Ni-376.
Published: 01 November 1989
..., the alloy has excellent isotropic properties in large billets and forgings. It resists oxidation up to 14OO F (76O C) and its corrosion resistance is similar to that of conventional austeuitic stainless steels. The alloy is rather difficult to machine (similar to super-alloys). It is fusion weldable using...
Abstract
View article
PDF
NICKEL VAC-901 is an iron-nickel base alloy with high strength and good oxidation resistance up to 1400 F (760 C). It is precipitation hardenable and is produced by vacuum induction melting followed by vacuum are remelting which greatly minimizes directionality of properties in large billets and forgings. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-376. Producer or source: Teledyne Allvac.
Journal Articles
Alloy Digest (2008) 57 (12): TS-675.
Published: 01 December 2008
... methods. Segregation-free and homogeneous metal powders of highest purity and adequate granulation are processed to homogeneous and segregation-free high-speed steels of virtually isotropic properties in a diffusion process taking place at high pressures and temperatures. The alloy is a high-speed steel...
Abstract
View article
PDF
Boehler (or Böhler) S290 Microclean is a high-speed steel made by powder metallurgy which impacts toughness and machinability. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on heat treating and powder metal forms. Filing Code: TS-675. Producer or source: Böhler-Uddeholm North America.
Journal Articles
Alloy Digest (1990) 39 (5): Cp-15.
Published: 01 May 1990
.... They have similar longitudinal and trans- verse (isotropic) properties. Corrosion resistance when compared to high-strength alloys like 7075-T6, is also very good. SXA@ materials can be fabricated, bonded, joined, anodized and plated using conventional equipment and techniques. Forms Available: Billet...
Abstract
View article
PDF
SXA is a unique group of alloy composites that provide a superior balance of strength, stiffness and fatigue resistance with low density. They are produced by powder metallurgy. This datasheet provides information on composition, tensile properties, and compressive strength. It also includes information on powder metal forms. Filing Code: Cp-15. Producer or source: Advanced Composite Materials Corporation.
Journal Articles
Alloy Digest (2005) 54 (3): TS-614.
Published: 01 March 2005
... by the patented VAD process and forged from upset ingots utilizing wide die forging techniques. This ensures sound centers and fine grain structure, giving improved isotropic properties throughout the piece. Finkl DC alloy is vacuum tested in the VAD and poured in an argon atmosphere to prevent oxidation. Finkl...
Abstract
View article
PDF
Finkl DC is a single-vacuum melted AISI H13 type material made by the vacuum arc degassing (VAD) process. The vanadium content of 1% in addition to a high chromium (Cr 5%) and molybdenum (Mo 1.4%) promotes hot strength and wear resistance. This datasheet provides information on composition. It also includes information on heat treating. Filing Code: TS-614. Producer or source: A. Finkl & Sons Company.
Journal Articles
Alloy Digest (2008) 57 (4): TS-664.
Published: 01 April 2008
... with virtually isotropic properties. Following this, the desired final dimension is achieved by hot forming. Boehler K89 Microclean, a highly ductile alloy, is a powder metallurgy cold-work tool steel with an outstanding capacity for plastic yield and a high fatigue strength. The property profile includes high...
Abstract
View article
PDF
Böhler (or Boehler) K890 Microclean is a cold-work tool steel that is highly ductile, but with a high fatigue strength. This datasheet provides information on composition, physical properties, and elasticity as well as fracture toughness. It also includes information on wear resistance as well as heat treating and powder metal forms. Filing Code: TS-664. Producer or source: Böhler-Uddeholm North America.