1-12 of 12 Search Results for

interchangeable

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2012) 61 (6): Cu-807.
Published: 01 June 2012
... Ansonia alloys C27000 and C27200 are yellow in color and sufficiently similar to those properties of C26000 to make them interchangeable. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming...
Journal Articles
Alloy Digest (2019) 68 (8): Cu-893.
Published: 01 August 2019
... Concast C89325 is a lead-free casting alloy that can be interchangeable with C937 (Alloy Digest Cu-421, August 1981). C89325 is classified as a bismuth tin bronze. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (2019) 68 (5): Cu-887.
Published: 01 May 2019
... Concast C89835 is a lead-free casting alloy that can be interchangeable with C932 (Alloy Digest Cu-387, January 1980), C836 (Alloy Digest Cu-317, August 1976), and C844 (Alloy Digest Cu-349, March 1978). This datasheet provides information on composition, physical properties, hardness, and tensile...
Journal Articles
Alloy Digest (2019) 68 (6): Cu-889.
Published: 01 June 2019
... Concast C89831 is a lead-free casting alloy that can be interchangeable with C844 (Alloy Digest Cu-349, March 1978). C89831 is classified as a bismuth tin bronze. This datasheet provides information on composition, physical properties, and elasticity. Filing Code: Cu-889. Producer or source...
Journal Articles
Alloy Digest (2019) 68 (7): Cu-891.
Published: 01 July 2019
... Concast C89833 is a lead-free casting alloy that can be interchangeable with C836 (Alloy Digest Cu-317, August 1976). C89833 is classified as a bismuth tin bronze. See also Federalloy I-844, Alloy Digest Cu-611, March 1997. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2022) 71 (12): CI-100.
Published: 01 December 2022
... Dura-Bar 202 (Type 2) Ni-Resist Iron is a flake graphite austentic cast iron that is produced by the continuous casting process. It is suitable for most applications requiring Dura-Bar 201 (Type 1) Ni-Resist Iron, and the grades are often used interchangeably. The machinability of Dura-Bar 202...
Journal Articles
Alloy Digest (1984) 33 (3): Ta-7.
Published: 01 March 1984
... with both its components. It can be used interchangeably with tantalum in numerous applications, see sections on Applications . The density of KBI-40 Alloy is about 25% lower than that of tantalum. Accordingly. KBl-40 Alloy can economically replace tantalum of equivalent surface area and gage with cost...
Journal Articles
Alloy Digest (1972) 21 (5): SS-273.
Published: 01 May 1972
... design of a conventional nature can be applied. Shrinkage and feeding characteristics are comparable to other stainless grades, and existing patterns can be used interchangeably for IS0450 and other grades of steels. Because of the somewhat low fluidity of this alloy, minimum section thickness...
Journal Articles
Alloy Digest (1972) 21 (8): SS-278.
Published: 01 August 1972
..., which allows e.xisting pattern equipment to be used interchangeably for IS040 and other stainless alloys. Composition control is of prime importance in achieving proper mechanical properties, therefore close controls must be maintained during melting operations. Most of the IS040 ahoy is melted...
Journal Articles
Alloy Digest (2023) 72 (4): Al-497.
Published: 01 April 2023
... are interchangeable, but BSI LM2 has a slightly lower density, BSI LM6 and BSI LM20 would be better than BSI LM2 in a corrosive environment, unless it can be Al-497 / 2 Table 2 Ratings of casting and other characteristics Characteristic Suitability for Sand casting Permanent mold casting Gravity die casting Low...
Journal Articles
Alloy Digest (1971) 20 (9): Ti-63.
Published: 01 September 1971
... to corrosion in many environ- ments and can frequently be used interchangeably with A-55 for such applications. Most forming operations can be performed at room temperature but warm forming reduces springback and power requirement. A-70 can be fusion welded under protective atmospheres or resistance spot...
Journal Articles
Alloy Digest (1955) 4 (7): CI-11.
Published: 01 July 1955
... are used interchangeably in many types of cormion and wear resisranr applications such as pipes, valves, pumps, cylinder liners, ea. In heat misring applicuions such as tube suppom, &box asrings, dampers, etc., Types 1 and 2 ate recommended for rempenmres up to 13OO F. and for constaut opmting temperames...