Alloy Digest (1983) 32 (4): Al-245.
Published: 01 April 1983
... for such items as cover plates and instrument cases. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat...
Journal Articles
Alloy Digest (1986) 35 (12): Al-274.
Published: 01 December 1986
... cases, gear cases, oil pans, airframe fittings and instrument housings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion...
Journal Articles
Alloy Digest (1976) 25 (5): Al-223.
Published: 01 May 1976
... ALUMINUM 356.0 is an aluminum casting alloy that normally is used only when heat-treated (aged) strengths are required. It is recommended for high strength, pressure-tight castings, intricate shapes and good resistance to corrosion. Its many applications include gear cases, instrument housings...
Journal Articles
Alloy Digest (1961) 10 (2): Al-100.
Published: 01 February 1961
... characteristics are better than those of the Al-Si alloy. Forms Available: Ingots. Applications: Automotive castings, carburetors, transmission housings, appliance castings , toys, motor housings, instrument cases, etc. Manufacturer: Apex Smelting Company Chicago, Illinois Cleveland, Ohio Long Beach, California...
Journal Articles
Alloy Digest (2005) 54 (9): W-28.
Published: 01 September 2005
... fixtures, high-durability radiation instrument casings, and radioisotope containers. SD 180 is commonly used for small, high-density balance weights. In sheet or monolithic form, it is also widely used for the shielding and/or collimation of gamma rays and high-energy x-rays in medical imaging devices. SD...
Journal Articles
Alloy Digest (1968) 17 (2): Al-172.
Published: 01 February 1968
..., instrument cases and housings, cover plates, general purpose castings. Manufacturer: Swiss Aluminium Ltd. Neuhausen am Rheinfall, Switzerland ...
Journal Articles
Alloy Digest (1961) 10 (5): Al-103.
Published: 01 May 1961
... Available: Die castings Applications: Cover plates, instrument cases, general purpose castings. Manufnciurer: Aluminum Company of America Pittsburgh, Pennsylvania ...
Journal Articles
Alloy Digest (1965) 14 (5): Al-145.
Published: 01 May 1965
... appli- cations or parts which require drastic forming can increase the applications for die castings. Forms Available: Die castings, ingots. Applications: Pressure tight castings, housings, instrument cases, centrifugal blowers. Manufacturer: Aluminum Co. of America, Pittsburgh, Pennsylvania. Reynolds...
Journal Articles
Alloy Digest (2023) 72 (8): Al-501.
Published: 01 August 2023
... motor parts, instrument cases, cover plates, a wide variety of general-purpose castings, and aircraft and marine items of many types. Information on applications sourced from 360.0 and A360.0: Al-Si-Mg General-Purpose Die-Casting Alloys, Properties and Selection of Aluminum Table 3 Ratings of casting...
Journal Articles
Alloy Digest (1967) 16 (7): Zn-10.
Published: 01 July 1967
.... instrument cases, hardware. Manufacturer: Federated Yetals Division -4merican Smelting 8: Refining Company New York, New York 10005 ...
Journal Articles
Alloy Digest (1957) 6 (8): Fe-14.
Published: 01 August 1957
... ISO-ELASTIC is an iron-nickel alloy having low temperature coefficient of the modulus of elasticity. It is suitable for precision instrument springs. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2005) 54 (11): SS-946.
Published: 01 November 2005
... Sandvik Bioline 4C27A is a hardenable 13% Cr stainless steel used in precision instruments. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating, and machining. Filing Code: SS-946. Producer...
Journal Articles
Alloy Digest (1977) 26 (9): Ni-250.
Published: 01 September 1977
... metals or alloys is zero at 320F. In the more common cases, the thermocouple only extends to a terminal block near the furnace. Extension wires are then extended to the measuring instrument. Unless the E.M.F. temperature relation of the extension wire and its thermo- element is similar, or the E.M.F...
Journal Articles
Alloy Digest (2020) 69 (8): SS-1326.
Published: 01 August 2020
... % 850 1000 123 145 650 94 10 Hardness of Surgical Instruments Conforming to ISO 71531:2016: 49 55 HRC. Modulus of Elasticity Property Unit Modulus of elasticity GPa (106 psi) At 20 °C (68 °F) Value 215 (31.2) Hot Forming Preheat slowly to 800 °C (1470 °F). Wait for equalization of the temperature. Raise...
Journal Articles
Alloy Digest (1983) 32 (3): Cu-454.
Published: 01 March 1983
... properties, Brush Alloy 3 finds widespread use in welding applications (RWMA Class 3), current-carrying springs, switch and instrument parts and similar components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fatigue...
Journal Articles
Alloy Digest (1963) 12 (2): Al-122.
Published: 01 February 1963
... copper content. Forms Available: Ingots. Applications: General die castings, instrument housings, portable tools, electrical equipment casings, motor housings, toys. Manufacturer: Apex Smelting Company, Division of American Metal Climax, Inc. Chicago 12, Illinois. Cleveland 5, Ohio. Long Beach 10...
Journal Articles
Alloy Digest (1967) 16 (6): Mg-63.
Published: 01 June 1967
... Magnesium MSR-B is a heat-treatable magnesium alloy with highest yield strength of any cast magnesium alloy up to 480 F. It is pressure tight and weldable by argon-arc. It is recommended for aircraft nose wheels, missile components, transmission cases, etc. This datasheet provides information...
Journal Articles
Alloy Digest (1974) 23 (10): Al-209.
Published: 01 October 1974
... fittings, oil pans, controls, superchargers, transmission cases, and instrument housings. Manufacturer: Federated Metals Division American Smelting and Refining Co. Somerville, NJ. 08876. ...
Journal Articles
Alloy Digest (2001) 50 (1): W-22.
Published: 01 January 2001
... with a predetermined amount of porosity. The pores are then filled with molten silver or copper to form essentially fully dense bodies. There is usually an excess of silver or copper on one of the surfaces, which, in most cases, is removed by machining. With the PSI process, the refractory content of the materials can...
Journal Articles
Alloy Digest (2001) 50 (6): W-26.
Published: 01 June 2001
... of copper on one of the surfaces, which, in most cases, is removed by machining. With the PSI process, the refractory content of the materials can range from about 35 90 wt The materials made by the PSI process normally have the greatest resistance to arc erosion. They are used for almost all of the larger...