Alloy Digest (2010) 59 (1): Cu-778.
Published: 01 January 2010
... an alloy safe for humans and the environment, particularly potable water. ECO BRASS® (Lead-Free Silicon Brass Rod and Ingot) ECO BRASS® Chemical Composition, wt See Table 1. Table 1 Chemical composition, wt.% Sand casting Nominal Permanent mold casting Nominal Wrought alloy Copper 74 78 76 74 78 77 73.0...
Journal Articles
Alloy Digest (1963) 12 (1): Fe-10.
Published: 01 January 1963
... ARMCO MAGNETIC INGOT IRON is a grade of commercially pure iron recommended for magnetic purposes. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on high...
Journal Articles
Alloy Digest (1978) 27 (2): SA-343.
Published: 01 February 1978
... LESCALLOY HP 9-4-30 VAC-ARC is a low-alloy, high-strength steel with a high nickel content to promote toughness. It was designated for high hardenability and good weldability. It is produced by the vacuum-consumable-electrode process to insure cleanliness and provide a preferred ingot structure...
Journal Articles
Alloy Digest (1989) 38 (9): Al-299.
Published: 01 September 1989
... ALCOA Alloy 2090 is an aluminum-lithium alloy with 8% lower density and 12% higher elastic modulus than 7075-T6, a major high-strength alloy used in aircarft structures. Special facilities and practices required for casting commercial size aluminum-lithium ingots have been developed to cope...
Journal Articles
Alloy Digest (1991) 40 (12): TS-144.
Published: 01 December 1991
... DYNAFLEX VAC-ARC steel is a medium alloyed, air hardening ultra high strength grade. It is produced by consumable electrode vacuum melting which provides superior cleanliness, elimination of dissolved gases and preferred ingot structure. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1992) 41 (3): SA-314.
Published: 01 March 1992
... LESCALLOY 4330 + V VAC-ARC steel is a vanadium modified 4330 having improved hardenability and mechanical properties. It is produced by consumable electrode vacuum are remelting providing optimum cleanliness and preferred ingot structure. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1992) 41 (4): Mo-16.
Published: 01 April 1992
... ARC-CAST LOW CARBON MOLYBDENUM is a carbon-deoxidized molybdenum alloy produced from ingots consolidated by a consummable electrode vacuum-arc-casting process. This datasheet provides information on composition, hardness, and tensile properties. Filing Code: Mo-16. Producer or source: Climax...
Journal Articles
Alloy Digest (1977) 26 (7): SA-335.
Published: 01 July 1977
... as 210 F in impact tests. It is produced by the vacuum consumable electrode melting process to provide optimum cleanliness and preferred ingot structure. Its uses include fasteners, shafting and aircraft components. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2021) 70 (3): Al-474.
Published: 01 March 2021
... Rio Tinto 319.2 is a heat-treatable, Al-Si-Cu casting alloy (3xx.x series). It is available in the form of ingots for remelting, for the production of sand and permanent mold castings. Alloy 319.0 exhibits very good castability and pressure tightness, moderate strength, and good high-temperature...
Journal Articles
Alloy Digest (2021) 70 (4): Al-475.
Published: 01 April 2021
... Raffmetal EN AB-Al Si7Mg (EN AB-42000) is a heat-treatable, aluminum-silicon-magnesium casting alloy in ingot form for remelting. It is used extensively for producing sand and permanent mold castings for applications requiring a combination of good strength and ductility, and good corrosion...
Journal Articles
Alloy Digest (2021) 70 (8): Al-479.
Published: 01 August 2021
... Rio Tinto 354.2 is a heat-treatable, aluminum-silicon-copper-magnesium casting alloy (3xx.x series). It is available in the form of ingots for remelting to be used for the production of sand and permanent mold castings. Alloy 354.0 was developed especially for premium engineered casting...
Journal Articles
Alloy Digest (2021) 70 (9): Al-480.
Published: 01 September 2021
... Raffmetal EN AB-Al Si7Mg0.3 (EN AB-42100) is a heat-treatable, Al-Si-Mg casting alloy in ingot form for remelting. It is used extensively for producing sand, permanent mold and investment castings for applications requiring a combination of excellent casting characteristics, high strength...
Journal Articles
Alloy Digest (2021) 70 (12): Al-483.
Published: 01 December 2021
... Raffmetal EN AB-Al Si7Mg0.6 (EN AB-42200) is a heat-treatable, Al-Si-Mg casting alloy in ingot form for remelting. It is used extensively for producing sand, permanent mold, and investment castings for applications requiring a combination of excellent casting characteristics, high strength...
Journal Articles
Alloy Digest (2009) 58 (6): SA-601.
Published: 01 June 2009
... Ovako 146S is an ingot cast case-hardening steel with good dimensional stability and high toughness. This datasheet provides information on composition as well as fatigue. It also includes information on casting, heat treating, and machining. Filing Code: SA-601. Producer or source: Ovako North...
Journal Articles
Alloy Digest (2009) 58 (7): SA-604.
Published: 01 July 2009
... OvaX 600 is an ingot cast through-hardening steel that is specially designed for air hardening or gas quenching and for applications requiring isotropic properties and very high cleanliness levels. This datasheet provides information on composition, hardness, and tensile properties. It also...
Journal Articles
Alloy Digest (1993) 42 (2): SA-321.
Published: 01 February 1993
... optimum cleanliness and preferred ingot structure. Its applications include aircraft components, pressure vessels and fasteners. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information...
Journal Articles
Alloy Digest (1959) 8 (1): Al-75.
Published: 01 January 1959
... APEX 39 is an aluminum die casting alloy ingot containing copper and silicon. It has excellent castability and improved machinability. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1979) 28 (7): SA-361.
Published: 01 July 1979
... LESCALLOY 4340 VAC-ARC is a low-alloy steel that can be heat treated to high strength levels. It has a good combination of strength, ductility and toughness along with high hardenability. It is produced by the vacuum-consumable-electrode process to provide optimum cleanliness and preferred ingot...
Journal Articles
Alloy Digest (1979) 28 (6): Bi-12.
Published: 01 June 1979
... BELMONT ALLOY 2431 is a bismuth-base alloy that can be melted easily. This non-eutectic alloy melts through the temperature range 160-190 F. It was originally developed as an ingot alloy and sold in a kit to be used by children for casting soldiers and other small objects. It has the unique...
Journal Articles
Alloy Digest (1981) 30 (8): Cu-421.
Published: 01 August 1981
... Copper Alloy No. C93700 is a cast bronze with relatively low strength, good machinability and good corrosion resistance. Commercial names formerly used (not recommended) are (1) High-Leaded Tin Bronze, (2) Ingot No. 305, (3) Bushing and Bearing Bronze and (4) 80-10-10. Its many applications...