... AlSiMag 222 is a porous ceramic material. It has excellent electrical insulating properties at elevated temperatures. For high frequency applications as an insulator, impregnation with a moisture repellant substance is required. AlSiMag 222 is well suited to prototype model making. This datasheet...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1971) 20 (12): Cu-246.
Published: 01 December 1971
... COMPO H is an oil-impregnated sintered bronze, produced by powder metallurgy techniques, which is widely used in automotive, applicance, farm equipment, and aircraft industry applications. This datasheet provides information on composition, physical properties, tensile properties, and compressive...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (6): Cp-9.
Published: 01 June 1990
... VERTON OF-700-10 is a long glass fiber reinforced polyphenylene sulfide. It has been engineered to maximize the benefits of long fiber reinforcement while maintaining the ease of processing and good fiber despersion associated with conventional short fiber reinforced compounds. Impregnation...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (9): Cp-2.
Published: 01 September 1989
... weight, high strength graphite. *K-KARB is a trademark of Kaiser Aerospace and Electronic Co. Components: Graphite fiber (from virgin rayon, pan acrylic nitrile, coal tar pitch, woven into cloth precursor). Resin (phenolic) The impregnated precursor constitutes the pre-preg. Physical Constants:* specific...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1957) 6 (9): Al-55.
Published: 01 September 1957
.... For the sevaest conditions this resistance can be further in- creased by anodic tramxnt, supplemenrd by a di- chromate impregnation of the oxide film While mildly less resistant to marine atmosphere and to mildly alka- line solutions than are the aluminum-magnesium alloys, it is mu& superior in mildly acid...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1975) 24 (3): Al-214.
Published: 01 March 1975
... conditions this resistance ~311 be further increased by anodic treatment. supplemented by a dichromate impregnation of the oxide film. While mildly less resistant to marine atmosplrere and to mildly alkuline solutions tlran are the 3lulilinuiii-nlagnesiurii alloys. 11 is much superior in mildly acid...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (8): Al-270.
Published: 01 August 1986
... increased by anodic treatment, supplemented by a dichromate impregnation of the oxide film. While mildly less resistant to marine atmosphere and to mildly alkaline solutions than are the aluminum-magnesium alloys, it is much superior in mildly acid solutions such as are encountered in the textile industry...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (12): SS-947.
Published: 01 December 2005
... is the result of the fine grain size, small carbides, and the cleanliness of the powder metallurgy (PM) microstructure. The alloy also has excellent edge retention. See Table 1 and Fig. 3. Product Forms Available: Contact the producer for the bar products and shapes available. Applications: DuraTech 20CV excels...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1992) 41 (12): TS-514.
Published: 01 December 1992
... Thyroplast 2311 tool steel is an AISI P20 modified grade, electric are melted and vacuum degassed, applicable to large plastic molds. It has good abrasion resistance and high impact strength This datasheet provides information on composition, physical properties, hardness, and tensile properties...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (2): TS-523.
Published: 01 February 1994
... wheels with plenty of coolant. Restrict peripheral speed c. Polishing: Thyssen P20 SUPER (P20 Modified) has excellent polishability. The recommended technique after grinding to 600 grit is to finally polish with diamond paste or aluminum oxide power impregnated cloths.75,6O,45.30,15,9,6,3...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1990) 39 (11): Cp-11.
Published: 01 November 1990
.../in. Width, in Cured ply thickness, vacuum bag, mils Impregnated fabric Resin content Volatiles 10.7 21.0 33.5 14.0 25.0 37.0 Plain 4HS 4HS 12 x 12 12 x 12 10x 10 50 50 50 8.0 15.0 26.0 4.0 38-40 3840 38-40 3840 13-15 13-15 13-15 13-15 *FD1048 designed entirely for tool surfacing. **Plain weave style: one...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1994) 43 (7): TS-528.
Published: 01 July 1994
.... The recommended technique af- ter grind& to 600 grit is to final polish with diamond paste or aluminum oxide powder impregnated cloths. 75,60,45, 30, 15, 9, 6, 3 micron paste or powder is recommended. Inclusion of all the above steps to required finish is recom- mended to reduce overall polishing time. Excessive...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1955) 4 (7): Al-29.
Published: 01 July 1955
.... welding process. Corrosion Resistance: Exhibits excellent resistance to corrosion under ordi- nary a:mospheric marine and domestic conditions. For the severest conditions this resistance can be further increased by anodic treatment, supplemented by a di- chromate impregnation of the oxide film. While mild...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1989) 38 (11): Cp-3.
Published: 01 November 1989
... and molding conditions, it is recommended that prototype molds be utilized to determine exact shrinkage General Characteristics: The injection moldable pellets from which VERTON composites are processed are made by pultrusion which provides a high level of impregnation by the resin with no fiber damage...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1993) 42 (6): TS-518.
Published: 01 June 1993
... with diamond paste or aluminum oxide powder impregnated cloths. 75. 60,45, 30, 15, 9,6, 3 micron paste or powder is recommended. Inclusion of all the above steps to required finish is recommended to reduce overall polishing time. Excessive polishing could result in pitting or orange peel effect. Polish only...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2003) 52 (9): SS-891.
Published: 01 September 2003
... Trades Research Associations) test machine performs a standard cutting operation and measures the number of silica impregnated cards that are cut (TCC = total cards cut). It is considered a measure of relative wear resistance. CATRA testing relative to 440C shows edge retention of 440C at 100%, 154CM...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2011) 60 (6): SS-1093.
Published: 01 June 2011
... or more times that of 440C and 154CM. The higher transverse toughness results indicate that CPM S35VN and CPM S30V are much more resistant to chipping and breaking in applications which may encounter side loading. In knife making, the higher transverse toughness makes CPM especially good for bigger blades...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2005) 54 (2): SS-918.
Published: 01 February 2005
... Polmax was developed to be both highly polishable and corrosion resistant for extreme surface finishes such as in lens molds. Polmax has excellent polishability, good corrosion resistance, good wear resistance, good machinability, and good stability in hardening. It is used for applications where...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (8): SS-367.
Published: 01 August 1979
... corrosive plastics, and (3) Corrosion problems when molds are used in hot, humid climates. In addition to resisting the above corrosive conditions, users have found that this steel has many other cost-reducing advantages for applications where corrosion is not involved. This datasheet provides information...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1999) 48 (8): SS-759.
Published: 01 August 1999
... impregnated with paste and improve with use. Hands and workpieces should be cleaned carefully between each change of paste grade. Workpieces should be cleaned with a grease solvent, and hands should be cleaned with soap. Paste should be applied to the polishing tool in manual polish- ing. When machine...