Alloy Digest (1977) 26 (11): Ni-251.
Published: 01 November 1977
... beryllium-nickel casting alloy that has been in use for over 40 years. Its many uses include tooling for plastics, glass-mold tooling, fuel-pump impellers, cores for Teflon molding and deep sour-well drilling components. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1978) 27 (5): Cu-354.
Published: 01 May 1978
... Copper Alloy No. 858 is a copper-zinc-tin-lead (yellow brass) alloy for die castings. It is a low-cost, general-purpose alloy with good machinability and soldering characteristics. Its many uses include general and marine hardware, pump, impellers, plumbing parts and gears. This datasheet provides...
Journal Articles
Alloy Digest (1968) 17 (7): SS-211.
Published: 01 July 1968
... AISI Type 502 is a corrosion and heat resisting 5% chromium alloy steel. It is generally used in the annealed condition only. It is recommended for oil refinery and chemical plant equipment, oil pump impellers, etc. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1968) 17 (9): Ni-138.
Published: 01 September 1968
... Brush Alloy 260-C is a beryllium nickel casting alloy having high strength, hardness and good corrosion resistance. It is recommended for fuel pump impellers, turbines, non-sparking tools, molds for plastics and glass. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1968) 17 (10): Cu-192.
Published: 01 October 1968
... PROMET No. 3 is a leaded tin bronze possessing a good combination of physical properties and corrosion resistance. It is recommended for bearings, gears, pump bodies and impellers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1969) 18 (2): Ni-142.
Published: 01 February 1969
... BRUSII Alloy 200C is a beryllium-nickel casting alloy having high resistance to wear, corrosion, thermal shock and oxidation. It is recommended for fuel pump impellers, turbines, non-sparking tools, molds for plastics and glass. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (1995) 44 (5): SS-595.
Published: 01 May 1995
... SOLEIL C5 is a 13% chromium 4% nickel martensitic stainless steel with improved toughness and good corrosion resistance to fresh water. Shafts and compressor impellers for hydraulic applications is the area of primary usage. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1978) 27 (6): Cu-355.
Published: 01 June 1978
... Copper Alloy No. 923 is a cast copper-tin-zinc-lead alloy known also as Leaded G Bronze or 87-8-1-4 alloy. This alloy possesses a good combination of strength, resistance to corrosion and machinability. It is a good alloy to withstand gas or liquid pressures. Applications include pump impellers...
Journal Articles
Alloy Digest (1979) 28 (10): Cu-382.
Published: 01 October 1979
... uses include valves, piston rings and pump impellers. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness, creep, and fatigue. It also includes information on high temperature...
Journal Articles
Alloy Digest (1979) 28 (12): Cu-386.
Published: 01 December 1979
.... Its many applications include tools, pump impellers, gears and marine hardware. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting...
Journal Articles
Alloy Digest (1979) 28 (4): Al-234.
Published: 01 April 1979
... for military aircraft and missiles, and impellers for gas turbine engines. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion...
Journal Articles
Alloy Digest (1980) 29 (8): Cu-401.
Published: 01 August 1980
... impellers and corrosion-resistant castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat...
Journal Articles
Alloy Digest (1963) 12 (1): Cu-124.
Published: 01 January 1963
... Ni-Bral nickel-aluminum bronze is a material having high strength and good corrosion resistance. It is recommended for marine propellers, impellers, valves, gears, and shafting. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties...
Journal Articles
Alloy Digest (1969) 18 (6): SS-225.
Published: 01 June 1969
... Duraloy CB 30 is a cast chromium steel having good corrosion resistance. It cannot be hardened by heat treatment. It is recommended for food processing and oil services at high temperatures, valve bodies, impellers and heat treating equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1981) 30 (8): Cu-421.
Published: 01 August 1981
... include bearings, bushings, impellers and pressure-tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness, creep, and fatigue. It also includes information...
Journal Articles
Alloy Digest (1983) 32 (10): Cu-464.
Published: 01 October 1983
... many applications include bearings, bushings, pump impellers and corrosion-resistant castings. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (1986) 35 (2): Cu-506.
Published: 01 February 1986
... for numerous applications such as bearings, gears, impellers and valve stems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat...
Journal Articles
Alloy Digest (1997) 46 (3): Cu-611.
Published: 01 March 1997
... Federalloy I-844 (C89831) is a lead-free bronze casting alloy that is machinable by alloying additions of bismuth. Applications include bearings (high speed and heavy pressure), pumps, impellers, and corrosion-resistant and pressure-tight castings. This datasheet provides information...
Journal Articles
Alloy Digest (1984) 33 (4): Cu-475.
Published: 01 April 1984
... in the form of continuous castings and its uses include bearings, pump bodies and impellers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as casting, heat treating, machining...
Journal Articles
Alloy Digest (1984) 33 (5): Cu-477.
Published: 01 May 1984
... Copper Alloy No. C92700 is a cast copper-base alloy; it formerly was known as 88-10-2-0 alloy. It is characterized by a good combination of machinability, strength and resistance to corrosion. Among its many uses are bearings, pump impellers, piston rings and valve parts that are subject to liquid...