Skip Nav Destination
Close Modal
Search Results for
impact resistance
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 2261
Search Results for impact resistance
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
GRIVORY G 355 NZ: High Impact Resistant Thermoplastic
Available to Purchase
Alloy Digest (1989) 38 (6): P-4.
Published: 01 June 1989
... GRIVORY G 355 NZ is an unreinforced, amorphous, high-impact resistant engineering thermoplastic. It is opaque and has a natural ivory color. It can be processed by injection molding, extrusion and blow molding. This datasheet provides information on physical properties, hardness, elasticity...
Abstract
View articletitled, GRIVORY G 355 NZ: High <span class="search-highlight">Impact</span> <span class="search-highlight">Resistant</span> Thermoplastic
View
PDF
for article titled, GRIVORY G 355 NZ: High <span class="search-highlight">Impact</span> <span class="search-highlight">Resistant</span> Thermoplastic
GRIVORY G 355 NZ is an unreinforced, amorphous, high-impact resistant engineering thermoplastic. It is opaque and has a natural ivory color. It can be processed by injection molding, extrusion and blow molding. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on casting. Filing Code: P-4. Producer or source: EMS-American Grilon Inc..
Journal Articles
RMI 6Al-2Cb-1Ta-0.8Mo: High Impact Resistant Alloy
Available to Purchase
Alloy Digest (1967) 16 (12): Ti-53.
Published: 01 December 1967
... RMI-6A1-2Cb-1Ta-0.8Mo is a titanium-base alloy recommended for parts requiring high impact strength along with good corrosion resistance, especially for deep diving under sea vehicles. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Abstract
View articletitled, RMI 6Al-2Cb-1Ta-0.8Mo: High <span class="search-highlight">Impact</span> <span class="search-highlight">Resistant</span> Alloy
View
PDF
for article titled, RMI 6Al-2Cb-1Ta-0.8Mo: High <span class="search-highlight">Impact</span> <span class="search-highlight">Resistant</span> Alloy
RMI-6A1-2Cb-1Ta-0.8Mo is a titanium-base alloy recommended for parts requiring high impact strength along with good corrosion resistance, especially for deep diving under sea vehicles. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ti-53. Producer or source: Reactive Metals Inc..
Journal Articles
HAYNES ALLOY No. 273: Hard Facing Alloy Resistant to Heat and Heavy Impact
Available to Purchase
Alloy Digest (1974) 23 (9): Ni-208.
Published: 01 September 1974
...+ Alloy No. 273 (Hard-Facing Alloy Resistant to Heat and Heavy Impact) HAYNES Alloy No. 273 is a nickel-base, hard-facing alloy developed to provide extra life for hot-working equipment such as hot-forging dies, hot-shear blades and hotextrusion dies. It is deposited by using a composite electrode...
Abstract
View articletitled, HAYNES ALLOY No. 273: Hard Facing Alloy <span class="search-highlight">Resistant</span> to Heat and Heavy <span class="search-highlight">Impact</span>
View
PDF
for article titled, HAYNES ALLOY No. 273: Hard Facing Alloy <span class="search-highlight">Resistant</span> to Heat and Heavy <span class="search-highlight">Impact</span>
HAYNES Alloy No. 273 is a nickel-base, hard-facing alloy developed to provide extra life for hot-working equipment such as hot-forging dies, hot-shear blades and hot-extrusion dies. It is deposited by using a composite electrode with nickel-base core and the balance of the alloying elements in the flux coating. Deposits retain their hardness up to 1200 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-208. Producer or source: Cabot Corporation.
Journal Articles
DELORO N-6 PM: Wear and Corrosion Resistant Alloy with Impact Strength
Available to Purchase
Alloy Digest (1993) 42 (2): Ni-422.
Published: 01 February 1993
... properties tensile properties wear resistance - DIGEST& DATA ON WORLD WIDE METALS AND ALLOYS DELORO N-6 PM Filing Code: Nickel Alloy Ni-422 FEBRUARY 1993 -6y: Alq &ja6l, Irr1201-677-6161 2? Car&Id SIrea, Orat&ja. N.J. ORXOI USA DELORO N-6 PM (Wear and Corroskm Resistant Alloy with impact Strength...
Abstract
View articletitled, DELORO N-6 PM: Wear and Corrosion <span class="search-highlight">Resistant</span> Alloy with <span class="search-highlight">Impact</span> Strength
View
PDF
for article titled, DELORO N-6 PM: Wear and Corrosion <span class="search-highlight">Resistant</span> Alloy with <span class="search-highlight">Impact</span> Strength
DELORO N-6 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on wear resistance as well as machining and joining. Filing Code: Ni-422. Producer or source: Deloro Stellite Inc.
Journal Articles
DELORO 208 PM: Wear and Corrosion Resistant Alloy with Impact Strength
Available to Purchase
Alloy Digest (1993) 42 (3): Ni-424.
Published: 01 March 1993
... L7pEJctm w fnaldL%p. DELORO 208 PM (Wear and Corrosion Resistant Alloy with impact Strength) DELORO@ 208 PM is a nickel-base alloy recommended for handling conditions of wear, erosion. heat and corrosion when Filing Code: Ni-424 YLLVI IV LVV PM Nickel Alloy impact is also a consideration. DELORO...
Abstract
View articletitled, DELORO 208 PM: Wear and Corrosion <span class="search-highlight">Resistant</span> Alloy with <span class="search-highlight">Impact</span> Strength
View
PDF
for article titled, DELORO 208 PM: Wear and Corrosion <span class="search-highlight">Resistant</span> Alloy with <span class="search-highlight">Impact</span> Strength
DELORO 208 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on wear resistance as well as machining and joining. Filing Code: Ni-424. Producer or source: Deloro Stellite Inc.
Journal Articles
DELORO 711 PM: Wear and Corrosion Resistant Alloy with Impact Strength
Available to Purchase
Alloy Digest (1993) 42 (5): Ni-431.
Published: 01 May 1993
... and Corrosion Resistant Alloy with impact Strength) DELORO@ 711 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. DELORO@ is a registered trademark. Composition, Nominal Wt., %: cobalt 12 Iron 23 Chromium 27 Molybdenum 7...
Abstract
View articletitled, DELORO 711 PM: Wear and Corrosion <span class="search-highlight">Resistant</span> Alloy with <span class="search-highlight">Impact</span> Strength
View
PDF
for article titled, DELORO 711 PM: Wear and Corrosion <span class="search-highlight">Resistant</span> Alloy with <span class="search-highlight">Impact</span> Strength
DELORO 711 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on high temperature performance as well as machining and joining. Filing Code: Ni-431. Producer or source: Deloro Stellite Inc.
Journal Articles
DELORO 716 PM: Wear and Corrosion Resistant Alloy with Impact Strength
Available to Purchase
Alloy Digest (1993) 42 (7): Ni-435.
Published: 01 July 1993
... or fma/ design. 27 Canlield SItwI. Orange. N.J. 07060 / U.S.A DELORO 716 PM (Wear and Corrosion Resistant Alloy with Impact Strength) DELORO@ 716 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. DELOROe is a registered...
Abstract
View articletitled, DELORO 716 PM: Wear and Corrosion <span class="search-highlight">Resistant</span> Alloy with <span class="search-highlight">Impact</span> Strength
View
PDF
for article titled, DELORO 716 PM: Wear and Corrosion <span class="search-highlight">Resistant</span> Alloy with <span class="search-highlight">Impact</span> Strength
DELORO 716 PM is a nickel-base alloy recommended for handling conditions of wear, erosion, heat and corrosion when impact is also a consideration. This datasheet provides information on composition, physical properties, and hardness. It also includes information on high temperature performance and wear resistance as well as machining and joining. Filing Code: Ni-435. Producer or source: Deloro Stellite Inc.
Journal Articles
DILLIDUR IMPACT: Wear Resistant Steel
Available to Purchase
Alloy Digest (2013) 62 (9): SA-681.
Published: 01 September 2013
... Dillidur 500V is a water hardened wear-resistant steel with surface hardness at room temperature of 310-370 HB. It has a high resistance to abrasion and impact wear in combination with good welding performance. This steel is used in the production of excavator buckets, stone crushers, and loading...
Abstract
View articletitled, DILLIDUR <span class="search-highlight">IMPACT</span>: Wear <span class="search-highlight">Resistant</span> Steel
View
PDF
for article titled, DILLIDUR <span class="search-highlight">IMPACT</span>: Wear <span class="search-highlight">Resistant</span> Steel
Dillidur 500V is a water hardened wear-resistant steel with surface hardness at room temperature of 310-370 HB. It has a high resistance to abrasion and impact wear in combination with good welding performance. This steel is used in the production of excavator buckets, stone crushers, and loading machines. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on wear resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-681. Producer or source: Dillinger Hütte GTS.
Journal Articles
ISO1083/JS/400-18-LT: Ferritic Ductile Iron
Available to Purchase
Alloy Digest (2023) 72 (4): CI-104.
Published: 01 April 2023
... grade of gray cast iron, together with much higher elongation and impact resistance. It is specifically designed to provide good impact properties at low temperature. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Abstract
View articletitled, ISO1083/JS/400-18-LT: Ferritic Ductile Iron
View
PDF
for article titled, ISO1083/JS/400-18-LT: Ferritic Ductile Iron
ISO1083/JS/400-18-LT is a ferritic spheroidal graphite cast iron that has a minimum tensile strength of 400 MPa (58 ksi) and a minimum elongation of 18%, when measured on test pieces machined from separately cast samples. It has a tensile strength exceeding that of the highest-tensile-strength grade of gray cast iron, together with much higher elongation and impact resistance. It is specifically designed to provide good impact properties at low temperature. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength as well as fatigue. It also includes information on casting and heat treating. Filing Code: CI-104. Producer or source: International Organization for Standardization.
Journal Articles
ACO EUROBAR EN-GJS-400-18C-LT (5.3123): Continuous Cast Spheroidal Graphite Cast Iron
Available to Purchase
Alloy Digest (2024) 73 (2): CI-109.
Published: 01 June 2024
... of gray cast iron, together with much higher elongation and impact resistance. It is specifically designed to provide good impact properties at low temperature. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Abstract
View articletitled, ACO EUROBAR EN-GJS-400-18C-LT (5.3123): Continuous Cast Spheroidal Graphite Cast Iron
View
PDF
for article titled, ACO EUROBAR EN-GJS-400-18C-LT (5.3123): Continuous Cast Spheroidal Graphite Cast Iron
ACO Eurobar EN-GJS-400-18C-LT is a ferritic spheroidal graphite cast iron that is produced by the continuous casting process. It has a minimum tensile strength of 400 MPa (58 ksi) and a minimum elongation of 18%. It has a tensile strength exceeding that of the highest-tensile-strength grade of gray cast iron, together with much higher elongation and impact resistance. It is specifically designed to provide good impact properties at low temperature. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on low temperature performance as well as casting, heat treating, and machining. Filing Code: CI-109. Producer or source: ACO Eurobar GmbH.
Journal Articles
CROLOY 9M: Chromium Molybdenum Alloy Steel
Available to Purchase
Alloy Digest (1953) 2 (4): SA-9.
Published: 01 April 1953
... CROLOY 9M is a chromium-molybdenum alloy steel having very good corrosion resistance with good high temperature strength. It has good resistance to steam oxidation up to 1200 F and good atmospheric oxidation resistance up to 1300 F maximum . It is also tough and impact resistant. This datasheet...
Abstract
View articletitled, CROLOY 9M: Chromium Molybdenum Alloy Steel
View
PDF
for article titled, CROLOY 9M: Chromium Molybdenum Alloy Steel
CROLOY 9M is a chromium-molybdenum alloy steel having very good corrosion resistance with good high temperature strength. It has good resistance to steam oxidation up to 1200 F and good atmospheric oxidation resistance up to 1300 F maximum . It is also tough and impact resistant. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-9. Producer or source: Babcock & Wilcox Company.
Journal Articles
CARLSON ALLOY NITRONIC 60: High-Manganese Austenitic Stainless Steel
Available to Purchase
Alloy Digest (2009) 58 (2): SS-1029.
Published: 01 February 2009
.... Possesses excellent high-temperature oxidation resistance and low-temperature impact resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion and wear resistance as well as forming. Filing Code: SS-1029...
Abstract
View articletitled, CARLSON ALLOY NITRONIC 60: High-Manganese Austenitic Stainless Steel
View
PDF
for article titled, CARLSON ALLOY NITRONIC 60: High-Manganese Austenitic Stainless Steel
CARLSON ALLOY NITRONIC 60 is a galling- and wear-resistant austenitic stainless steel that provides a significantly lower-cost alternative to cobalt-bearing and high-nickel alloys. Corrosion resistance is superior to 304 in most media. Approximately twice the yield strength of 340 and 316. Possesses excellent high-temperature oxidation resistance and low-temperature impact resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion and wear resistance as well as forming. Filing Code: SS-1029. Producer or source: G.O. Carlson Inc.
Journal Articles
ARMCO NITRONIC 60: High Temperature Galling Resistant Stainless Steel
Available to Purchase
Alloy Digest (1990) 39 (7): SS-308.
Published: 01 July 1990
... ARMCO NITRONIC 60 Stainless Steel provides outstanding galling and wear resistance. It also has excellent high-temperature oxidation resistance and low-temperature impact resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Abstract
View articletitled, ARMCO NITRONIC 60: High Temperature Galling <span class="search-highlight">Resistant</span> Stainless Steel
View
PDF
for article titled, ARMCO NITRONIC 60: High Temperature Galling <span class="search-highlight">Resistant</span> Stainless Steel
ARMCO NITRONIC 60 Stainless Steel provides outstanding galling and wear resistance. It also has excellent high-temperature oxidation resistance and low-temperature impact resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-308. Producer or source: Baltimore Specialty Steels Corporation. Originally published as Nitronic 60, March 1975, revised July 1990.
Journal Articles
ARMCO 410 Cb: Corrosion Resistant Steel
Available to Purchase
Alloy Digest (1963) 12 (7): SS-145.
Published: 01 July 1963
... Armco 410 Cb is a modified Type 410 corrosion resistant steel by the addition of columbium. It is extremely tough and impact resistant. It is a hardenable grade but less sensitive to tempering variables than Type 410. This datasheet provides information on composition, physical properties...
Abstract
View articletitled, ARMCO 410 Cb: Corrosion <span class="search-highlight">Resistant</span> Steel
View
PDF
for article titled, ARMCO 410 Cb: Corrosion <span class="search-highlight">Resistant</span> Steel
Armco 410 Cb is a modified Type 410 corrosion resistant steel by the addition of columbium. It is extremely tough and impact resistant. It is a hardenable grade but less sensitive to tempering variables than Type 410. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-145. Producer or source: Armco Inc., Eastern Steel Division. See also Alloy Digest SS-261, October 1971.
Journal Articles
AMPCO METAL-12: Aluminum Bronze
Available to Purchase
Alloy Digest (1955) 4 (5): Cu-26.
Published: 01 May 1955
... AMPCO METAL 12 is a cast aluminum bronze having good impact resistance, moderate strength and good wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness...
Abstract
View articletitled, AMPCO METAL-12: Aluminum Bronze
View
PDF
for article titled, AMPCO METAL-12: Aluminum Bronze
AMPCO METAL 12 is a cast aluminum bronze having good impact resistance, moderate strength and good wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as machining and joining. Filing Code: Cu-26. Producer or source: Ampco Metal Inc..
Journal Articles
ALLEGHENY STAINLESS TYPE 410: High Strength Corrosion and Heat Resistant Steel
Available to Purchase
Alloy Digest (1981) 30 (7): SS-388.
Published: 01 July 1981
... and it may be tempered at temperature up to 1350 F to produce high impact resistance. Among its many applications are knives, mechanical blades and other miscellaneous cutting tools for numerous corrosive environments. This datasheet provides information on composition, physical properties, microstructure...
Abstract
View articletitled, ALLEGHENY STAINLESS TYPE 410: High Strength Corrosion and Heat <span class="search-highlight">Resistant</span> Steel
View
PDF
for article titled, ALLEGHENY STAINLESS TYPE 410: High Strength Corrosion and Heat <span class="search-highlight">Resistant</span> Steel
ALLEGHENY STAINLESS TYPE 410 is a hardenable 12% chromium type of stainless steel. It has good resistance to corrosion and oxidation and offers a wide range of mechanical properties obtainable by heat treatment. It has such a high hardenability that it can be hardened readily by air cooling and it may be tempered at temperature up to 1350 F to produce high impact resistance. Among its many applications are knives, mechanical blades and other miscellaneous cutting tools for numerous corrosive environments. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: SS-388. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
NAK 55: Age-Hardenable Plastic Mold Steel
Available to Purchase
Alloy Digest (1994) 43 (12): SA-481.
Published: 01 December 1994
... NAK 55 is a very clean steel for use in plastic and rubber molds were impact resistance is not critical in design. Its age-hardening gives very high strength and good wear resistance. Tight tolerance are obtained with consistent expansion and contraction properties. This datasheet provides...
Abstract
View articletitled, NAK 55: Age-Hardenable Plastic Mold Steel
View
PDF
for article titled, NAK 55: Age-Hardenable Plastic Mold Steel
NAK 55 is a very clean steel for use in plastic and rubber molds were impact resistance is not critical in design. Its age-hardening gives very high strength and good wear resistance. Tight tolerance are obtained with consistent expansion and contraction properties. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on heat treating, machining, and joining. Filing Code: SA-481. Producer or source: International Mold Steels.
Journal Articles
REPUBLIC M: High Strength Low Alloy Construction Steel
Available to Purchase
Alloy Digest (1963) 12 (7): SA-149.
Published: 01 July 1963
... Republic-M is a low carbon, manganese type structural steel having high notch-impact resistance and high ductility at subzero temperatures. It is recommended for structural applications where weight reduction is important. This datasheet provides information on composition, physical properties...
Abstract
View articletitled, REPUBLIC M: High Strength Low Alloy Construction Steel
View
PDF
for article titled, REPUBLIC M: High Strength Low Alloy Construction Steel
Republic-M is a low carbon, manganese type structural steel having high notch-impact resistance and high ductility at subzero temperatures. It is recommended for structural applications where weight reduction is important. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-149. Producer or source: Republic Steel Corporation.
Journal Articles
NICLOY 9: Tough Nickel Alloy Steel
Available to Purchase
Alloy Digest (1952) 1 (2): SA-2.
Published: 01 October 1952
... Nicloy 9 is a tough, impact resistant nickel alloy steel applicable to sub-zero temperature uses. It has high physical properties with excellent ductility. Its toughness is very high at low temperatures. At room temperature it is only slightly sensitive to temper brittleness. This datasheet...
Abstract
View articletitled, NICLOY 9: Tough Nickel Alloy Steel
View
PDF
for article titled, NICLOY 9: Tough Nickel Alloy Steel
Nicloy 9 is a tough, impact resistant nickel alloy steel applicable to sub-zero temperature uses. It has high physical properties with excellent ductility. Its toughness is very high at low temperatures. At room temperature it is only slightly sensitive to temper brittleness. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and fatigue. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: SA-2. Producer or source: Babcock & Wilcox Company.
Journal Articles
AISI 6150: Chromium Vanadium Steel
Available to Purchase
Alloy Digest (1955) 4 (1): SA-26.
Published: 01 January 1955
... AISI 6150 is a tough, shock resisting, shallow-hardening chromium-vanadium steel. It has high fatigue and impact resistance in the heat treated condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture...
Abstract
View articletitled, AISI 6150: Chromium Vanadium Steel
View
PDF
for article titled, AISI 6150: Chromium Vanadium Steel
AISI 6150 is a tough, shock resisting, shallow-hardening chromium-vanadium steel. It has high fatigue and impact resistance in the heat treated condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-26. Producer or source: Alloy steel mills and foundries.