1-20 of 2479

Search Results for impact properties

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2023) 72 (4): CI-104.
Published: 01 April 2023
... grade of gray cast iron, together with much higher elongation and impact resistance. It is specifically designed to provide good impact properties at low temperature. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear strength...
Journal Articles
Alloy Digest (1979) 28 (2): SA-355.
Published: 01 February 1979
... UNIFLUX V90 is a continuous flux-cored welding electrode (wire) developed to weld high-strength low-alloy steels, but it may be used to weld other low-alloy steels and carbon steels. It is used to deposit typically 2.40% nickel steel weld metal with good low-temperature impact properties. Welding...
Journal Articles
Alloy Digest (1979) 28 (6): TS-350.
Published: 01 June 1979
... UHB-S7 is a tool steel characterized by its high hardenability and excellent impact properties. At Rockwell C 59 it has a compressive strength of over 600,000 psi, a tensile strength of 340,000 psi, and a Charpy (no notch, smooth) impact value of more that 140 foot-pounds. It is suitable...
Journal Articles
Alloy Digest (1979) 28 (7): SA-362.
Published: 01 July 1979
.... It is used to deposit typically 2.40% nickel steel weld metal with good low-temperature impact properties. Uniflux 90 is used widely in shipbuilding and other fabricating industries. It provides around 85,000 psi tensile strength and around 25 foot-pounds Charpy V-notch impact at -60 F. This datasheet...
Journal Articles
Alloy Digest (2024) 73 (2): CI-109.
Published: 01 June 2024
... of gray cast iron, together with much higher elongation and impact resistance. It is specifically designed to provide good impact properties at low temperature. This datasheet provides information on physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (2022) 71 (2): CI-90.
Published: 01 February 2022
... Meehanite SFF350 is a ferritic ductile iron with a minimum tensile strength of 350 MPa (51 ksi) and a minimum elongation of 24%, when measured on test pieces machined from separately cast samples. It is specifically designed to provide good impact properties at low temperature. This fully ferritic...
Journal Articles
Alloy Digest (2022) 71 (5): CI-93.
Published: 01 May 2022
... Meehanite SFF400 is a ferritic ductile iron with a minimum tensile strength of 400 MPa (58 ksi) and a minimum elongation of 20%, when measured on test pieces machined from separately cast samples. It is specifically designed to provide good impact properties at low temperature. This fully ferritic...
Journal Articles
Alloy Digest (1973) 22 (7): Zn-16.
Published: 01 July 1973
... KORLOY 2570 and 2573 are zinc-base alloys possessing superior strength and good low-temperature impact properties down to -60 F. They are easily forged, extruded and machined for wrought applications and alloy 2570 can be used in the cast condition. They have excellent bearing properties and can...
Journal Articles
Alloy Digest (2006) 55 (3): Cu-741.
Published: 01 March 2006
... Hidurax 7 is a nickel and silicon hardened bronze grade with tensile properties slightly lower than Hidurax 1 (see Alloy Digest Cu-740, February 2006). The alloy has high impact properties and low magnetic permeability. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2015) 64 (1): SS-1196.
Published: 01 January 2015
... Kubota CA-6NM is a hardenable Fe-Cr-Ni-Mo alloy based on the 13% chromium stainless steel alloy CA-15. Ductility, impact properties, and resistance to salt water corrosion are raised by the addition of nickel and molybdenum. Castability in thick or intricate sections is better than that of the 13...
Journal Articles
Alloy Digest (1961) 10 (1): SA-109.
Published: 01 January 1961
... Vascojet 1000-5 Temper is an ultra high-strength steel designed for applications requiring between 300,000 and 325,000 psi ultimate tensile strength, and 260,000-270,000 psi yield strength, with good fatigue and impact properties. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2023) 72 (1): CI-101.
Published: 01 January 2023
... ACO Eurobar EN-GJS-350-22C-LT is a ferritic spheroidal graphite cast iron that is produced by the continuous casting process. It has a minimum tensile strength of 350 MPa (51 ksi) and a minimum elongation of 22%, and it is specifically designed to provide good impact properties at low temperature...
Journal Articles
Alloy Digest (1979) 28 (8): Ti-72.
Published: 01 August 1979
... RMI 40 is a grade of commercially pure unalloyed titanium. It has a guaranteed minimum yield strength of 40,000 psi with good ductility and formability. Its strength is about the same as that of the annealed austenitic stainless steels. It has good impact properties at low temperatures...
Journal Articles
Alloy Digest (1981) 30 (1): Ti-81.
Published: 01 January 1981
... RMI 55 is a grade of commercially pure unalloyed titanium. It has good ductility and formability with a guaranteed minimum yield strength of 55,000 psi. It has good impact properties at room temperatures and excellent resistance to corrosion by marine atmospheres and seawater. Among its uses...
Journal Articles
Alloy Digest (1983) 32 (4): SA-389.
Published: 01 April 1983
...-grained steels with low-temperature toughness. Tri-Mark TM-811N2 is used to deposit typically 2.35% nickel steel weld metal with good low-temperature impact properties. It is used for shipbuilding, oil rigs and similar structures. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1983) 32 (8): SA-392.
Published: 01 August 1983
... for single and multiple-pass welding. It has outstanding low-temperature impact properties. Its applications including mining equipment, large vehicles and similar items. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1984) 33 (6): SS-448.
Published: 01 June 1984
... cracking. It has good strength and impact properties over a wide range of temperatures. JS800H also exhibits very good creep strength up to at least 1500 F. Uses include the chemical process industry and equipment of heat treating. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1970) 19 (9): Cu-220.
Published: 01 September 1970
... MUELLER 6246 is a high-strength copper-aluminum-iron (Aluminum Bronze) alloy possessing a tensile strength greater than 100,000 psi. It has excellent impact properties, wear characteristics and corrosion resistance. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1963) 12 (12): CS-20.
Published: 01 December 1963
... Lukens LT-75 is a carbon-manganese-silicon steel of flange and firebox quality having good impact properties for low temperature applications. It is supplied in two grades; LT-75N and LT-75QT. This datasheet provides information on composition, physical properties, elasticity, and tensile...
Journal Articles
Alloy Digest (1976) 25 (10): Co-74.
Published: 01 October 1976
... WALLEX No. 40 is a self-fluxing, cobalt-base hard-surfacing alloy with excellent resistance to a combination of corrosion and abrasion and relatively good impact properties. It has excellent red hardness and weldability. It is supplied only as atomized powder for application with Wall Colmonoy's...