1-20 of 49 Search Results for

hydraulic valve parts

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1977) 26 (6): Cu-334.
Published: 01 June 1977
... AMPCOLOY C-3 is a copper-aluminum-iron alloy with high strength and hardness, good toughness, good resistance to fatigue and wear, and good corrosion resistance. It is used for heavy loads in such applications as bearings, gears and hydraulic valve parts. It is suited for service up to 750 F...
Journal Articles
Alloy Digest (1966) 15 (9): Cu-169.
Published: 01 September 1966
... Bohnolloy R-60L is a leaded Naval Brass having good corrosion resistance and improved machinability. It is recommended for marine hardware, hydraulic valve stems, screw machine products, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1999) 48 (1): Al-357.
Published: 01 January 1999
... Kaiser Aluminum Alloy 2024 has good machinability and good mechanical properties. The alloy is typically used in aircraft structures, rivets, connectors, hydraulic valve bodies, and miscellaneous structural applications. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1966) 15 (8): Cu-167.
Published: 01 August 1966
..., spur gears, cams, bridge parts, gears, screw-down nuts, bearings (slow speed, heavy load), hydraulic cylinder parts, screw machine products, rotors, rollers, gun parts. Manufacturer: Mueller Brass Company Port Huron, hlichigan ...
Journal Articles
Alloy Digest (1976) 25 (1): Cu-307.
Published: 01 January 1976
... ATLANTIC 13B Alloy is a silicon bronze casting alloy offering excellent castability and corrosion resistance, good machinability and medium-high strength. It is an all-purpose alloy that is suitable for gears, valve parts and marine fittings. It is especially useful in stress-corrosion...
Journal Articles
Alloy Digest (1976) 25 (10): Cu-320.
Published: 01 October 1976
... Copper Alloy No. 875 is a copper-base casting alloy for applications requiring a combination of high strength and good resistance to corrosion. It cannot be hardened or strengthened by heat treatment. Its many applications include valve parts, small propellers, gears and marine components...
Journal Articles
Alloy Digest (2018) 67 (3): SS-1281.
Published: 01 March 2018
... welding, Ferro-Titanit is particularly used in forming and cutting tools, hydraulic jacks for polymer production, and pelletizing and granulating cutter blades. This datasheet provides information on composition, physical properties, microstructure, and hardness. It also includes information on heat...
Journal Articles
Alloy Digest (1970) 19 (2): SS-234.
Published: 01 February 1970
... components, chemical processing equipment, valve and pump parts, marine hardware, sporting goods. Manufacturer: Allegheny Ludlum Steel Corp. Pittsburgh & Brackenridge. Pennsylvania ...
Journal Articles
Alloy Digest (1998) 47 (5): Al-348.
Published: 01 May 1998
... is exp ected to evaluate and test the alloy, temp er, and finishing method. Products Available: Cold-finished rectangles, rounds and hexes, bar, rod, shap es Applications: ABS braking systems, hydraulic applications, valves, machined parts, roller blade parts. munitions Producer: ALCOA Wire. Rod and Bar...
Journal Articles
Alloy Digest (1977) 26 (9): Zn-31.
Published: 01 September 1977
... or slower turning applications. Where aluminum is too soft, or tends to seize or gall, ZA-12 is an ideal substitute. Available data suggest ZA-12 has excellent potential in many bearing markets. Thrust bearings, hydraulic cylinder parts, high wear pulley parts, flange and bushing bearings are a few areas...
Journal Articles
Alloy Digest (1998) 47 (3): Al-346.
Published: 01 March 1998
... and test the alloy, temper, and finishing method. Applications: Typical applications include aircraft fittings, hydraulics, hinge pins, valves and valve parts, and brake pistons. The T6 and T85 1 tempers offer both an increase in strength and improved stress- DOI: 10.31399/asm.ad.al0346 2024-T351 - 2024-T6...
Journal Articles
Alloy Digest (2021) 70 (5): CI-81.
Published: 01 May 2021
... produced parts for automobiles as well as for small hydraulic bodies that must be pressure tight. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on low and high temperature performance as well as casting, heat treating...
Journal Articles
Alloy Digest (1986) 35 (2): Cu-506.
Published: 01 February 1986
... for numerous applications such as bearings, gears, impellers and valve stems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat...
Journal Articles
Alloy Digest (1988) 37 (7): Zn-43.
Published: 01 July 1988
... or gall, UNS NO. 235630 is an ideal substitute. Thrust bearings, hydraulic cylinder parts, high wear pulley pans, flange and bushing bearings are a few areas where the alloy may be considered. Corrosion Resistance: UNS NO. 235630 has good corrosion resistance and proven reliability in various aqueous...
Journal Articles
Alloy Digest (2023) 72 (4): CI-104.
Published: 01 April 2023
... such as gear box, hub and nacelle; applications in hydraulic and pneumatic systems for parts such as high pressure hydraulic housings; brackets; couplings; pressure vessels; valves. Information on applications sourced from Meehanite Specification Handbook, Meehanite Metal Corp, 2013, p 37, and Low Temperature...
Journal Articles
Alloy Digest (1988) 37 (11): Zn-44.
Published: 01 November 1988
... in corrosion protection for UNS 235840. (See zinc anodizing section.) Bearing and Wear Characteristics: UNS 235840 is a strong material with bearing properties which can often replace bronze and brass for sliding and rotating bearings. Thrust bearings, spacers, bearing flanges and bushings, and hydraulic...
Journal Articles
Alloy Digest (1962) 11 (6): Cu-118.
Published: 01 June 1962
... Available: Castings Applications: Spurs, gears, gibs, cams, machine parts, large valve stems, bridge parts, screw-down nuts, hydraulic cylinder parts, bearings. Manufacturer: Lumen Bearing Company Buffalo, New York ...
Journal Articles
Alloy Digest (1960) 9 (1): Mg-44.
Published: 01 January 1960
... and pump bodies, hydraulic cylinders, supercharger parts, control lev- ers, fittings, hardware engine mountings, screw ma- chine parts from extruded bars and rods. Manufacturer: Aluminum Company of America Pittsburgh, Pennsylvania (forgings) Dow Chemical Company Midland, Michigan (for,&g billets) ...
Journal Articles
Alloy Digest (1996) 45 (12): Al-340.
Published: 01 December 1996
... higher overall productivity. Typical applications are for aluminum screw machine parts and include A-rot4 hated master cylinder brake pistons, connectors, transmission valves. and various hydraulic parts commonly used in the automotive. fluid power. and electronic industries. Products Available: Extruded...
Journal Articles
Alloy Digest (1959) 8 (12): Cu-84.
Published: 01 December 1959
... to Leaded Commercial Bronze or Tellurium Copper. Leaded Naval Brass is readily hot forged, for which purpose the slugs must be sawed to length. Forms Available: Rods, bars, extruded or extruded and drawn shapes, forgings. Applications: Forgings, matine hardware, screw machine products, hydraulic valve stems...