1-4 of 4 Search Results for

hydraulic jacks

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2018) 67 (3): SS-1281.
Published: 01 March 2018
... welding, Ferro-Titanit is particularly used in forming and cutting tools, hydraulic jacks for polymer production, and pelletizing and granulating cutter blades. This datasheet provides information on composition, physical properties, microstructure, and hardness. It also includes information on heat...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2018) 67 (5): Fe-168.
Published: 01 May 2018
... resistance and low tendency toward cold welding, Ferro-Titanit is particularly used in forming and cutting tools, hydraulic jacks for polymer production, and pelletizing and granulating cutter blades. This datasheet provides information on composition, physical properties, hardness, elasticity...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2018) 67 (4): SS-1283.
Published: 01 April 2018
... groups. Depending on application, Ferro-Titanit contains up to 45% titanium carbide, one of the hardest and most resistant carbides. Because of its high wear resistance and low tendency toward cold welding, Ferro-Titanit is particularly used in forming and cutting tools, hydraulic jacks for polymer...
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (9): SA-230.
Published: 01 September 1968
... strength is 60-70~ of its tensile strength. Forms Available: Annealed hot-tolled rounds, squares and flats. Heat treated, machined straightened, and stress-relieved rounds, squares and flats. Cold-finished rounds. Applications: Gears, pinions, bolts, shafts. adapters, sleeves, set screws, hydraulic...