1-20 of 2383 Search Results for

hot work tool steel

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1984) 33 (1): TS-420.
Published: 01 January 1984
... W.W. HOT WORK is a chromium-tungsten hot-work tool and die steel containing nominally 1.05% vanadium. It is characterized by high strength and hardness at elevated temperature and good resistance to heat checking. It has high hardenability and can be hardened by quenching in salt or oil. Its many...
Journal Articles
Alloy Digest (2020) 69 (3): TS-789.
Published: 01 March 2020
... Finkl Steel Durodi is a nickel-chromium-molybdenum-vanadium, alloy hot work tool steel that hardens deeply and uniformly to a high hardness that holds up exceedingly well under impact and thermal shock. It is designed to provide maximum abrasion and heat resistance over a full range of service...
Journal Articles
Alloy Digest (2022) 71 (3): TS-825.
Published: 01 March 2022
... Uddeholm QRO 90 Supreme is a high-performance chromium-molybdenum-vanadium alloy hot-work tool steel. The combination of high temperature strength, temper resistance and thermal conductivity exhibited by Uddeholm QRO 90 Supreme is unparalleled. Thus Uddeholm QRO 90 Supreme exhibits improved...
Journal Articles
Alloy Digest (2022) 71 (4): TS-826.
Published: 01 April 2022
... Uddeholm Unimax is a high-hardness chromium-molybdenum-vanadium alloy hot-work tool steel that provides high wear resistance at elevated temperatures. It performs very well in precision forging and hot stamping. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1994) 43 (3): TS-524.
Published: 01 March 1994
... THYROTHERM 2344 EFS is an electric arc melted, vacuum degassed hot work tool steel with good resistance to thermal shock and the capability to be polished to lens quality. This datasheet provides information on composition, physical properties, and hardness as well as fracture toughness. It also...
Journal Articles
Alloy Digest (1994) 43 (6): TS-527.
Published: 01 June 1994
... righlsraserved. Pldrlirhedby: Alloy Dii. Inc. I201-677-9161 &uashmarerypu.Mnloteusedtor 27CanfiildSlmt.Orange. N.J.070501lJ.S.A s&x3&l Q fd &e#7. THYROTHERM 2344 SUPRA ESR (Chromium hot-work tool steel ) THYROTHERM 2344 SUPRA ESR is a premium quality AISI H13 work tool steel with consistent and uniform...
Journal Articles
Alloy Digest (1994) 43 (11): TS-533.
Published: 01 November 1994
...-6161 ~?lpiIIWbsd~ 27 CardbW strecn. Orpnge. NJ. 07060 I USA AISI Type H22 (Tungsten hot work tool steel) H22 is a tungsten hot work steel with the principal alloying elements of carbon, tungsten, chromium and vanadium. It resists softening at elevated temperatures. Nominal Composition, Wt, %: Carbon...
Journal Articles
Alloy Digest (1961) 10 (11): TS-111.
Published: 01 November 1961
... Milne CMV is a 5% chromium, medium-carbon hot work tool steel, having high compression strength, wear resistance, and corrosion resistance. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness and creep. It also includes information...
Journal Articles
Alloy Digest (1962) 11 (7): TS-120.
Published: 01 July 1962
... Pvblisbad by HEPPENSTALL V3 (Hot Work Tool Steel, Type H21) Engineering Alloys Digest. Inc. Upper Montclair. New Jersey Al1 O! DIGEST Heppenorall T73 is a low carbon, medium tungsten, hot work steel which has excellent red hardness properties. It is recan- mended for forging and extrusion dies. Composition...
Journal Articles
Alloy Digest (1966) 15 (3): TS-177.
Published: 01 March 1966
... Filing Code: TS-177 Tool Steel MARCH 1966 -DATA ON WORLD WIDE METALS AND ALLOYS CALMAX (Hot Work Tool Steel) Pvblisbrd by Engineering Alloys Digest. Inc. Upper Montclair, New Jm UHD CALMAX is a chromium-tungsten-cobalt hot work steel recommended for the most severe applications. lt has an extremely...
Journal Articles
Alloy Digest (2020) 69 (2): TS-787.
Published: 01 February 2020
... Uddeholm Vidar 1 ESR is a medium-carbon, chromium-molybdenum-vanadium, hot-work tool steel that is produced using the electroslag remelting (ESR) process. Its good toughness in combination with very good polishability and texturing properties makes it a suitable steel in plastic mold applications...
Journal Articles
Alloy Digest (2020) 69 (7): TS-796.
Published: 01 July 2020
... Crucible Nu-Die V (Type H13) is a medium-carbon, chromium-molybdenum-vanadium, alloy hot work tool steel that provides a good balance of toughness, heat check resistance, and temper resistance, along with moderate wear resistance. It is used for tool temperatures up to about 540 °C (1000 °F...
Journal Articles
Alloy Digest (2023) 72 (6): TS-835.
Published: 01 June 2023
... Böhler K300 Isobloc is a chromium-molybdenum-vanadium alloy hot-work tool steel. It is characterized by good hot strength properties, very high toughness, and good polishability. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Alloy Digest (2023) 72 (7): TS-836.
Published: 01 July 2023
... Böhler K300 Isodisc is a chromium-molybdenum-vanadium alloy hot-work tool steel. It is characterized by outstanding air hardenability, excellent hot tensile properties, high impact strength, and good polishability. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (2023) 72 (8): TS-837.
Published: 01 August 2023
... Böhler K302 Isodisc is a chromium-molybdenum-vanadium alloy hot-work tool steel. It is characterized by good toughness, high hot hardness, and high wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also...
Journal Articles
Alloy Digest (1954) 3 (10): TS-25.
Published: 01 October 1954
... hardness heat treatability machinability Seneca workability Filing Code: TS-25 Tool Steel 1 SENECA 1 OCTOBER, 1954 DIGESTd - DATA ON WORLD WIDE METALS AND ALLOYS SENECA (Hot Work Tool Steel) SENECA is a tungsten-chromium type of hot work steel having good red hardness and resistance to abrasion...
Journal Articles
Alloy Digest (1955) 4 (3): TS-31.
Published: 01 March 1955
... treatability joinability machinability Ultimo-6 workability Filing Code: TS-31 Tool steel - DATA ON WORLD WIDE METALS AND ALLOYS ULTIMO-6 (Hot Work Tool Steel) WI IMO-6 is a chromium-nickel-molybdenum tool and die steel applicable where resistance to shock is important and where water cooling may...
Journal Articles
Alloy Digest (2000) 49 (8): TS-579.
Published: 01 August 2000
... treatability high-temperature alloys joinability machinability physical properties temperature resistance BÖHLER W302 ISOBLOC® (Hot-Work Tool Steel) Böhler W302 ISOBLOC is a premium grade H13 tool steel with a good combination of toughness, heat-checking resistance, temperature resistance, and high...
Journal Articles
Alloy Digest (2000) 49 (10): TS-581.
Published: 01 October 2000
... Boehler W302 VMR is a hot tool steel that is manufactured and certified to meet an average impact toughness of 20 J (15 ft·lbf) minimum in Charpy V-notch testing. This die steel achieves that toughness by vacuum melting and remelting. Applications include dies, die holders, liners, and stems...
Journal Articles
Alloy Digest (2001) 50 (6): TS-588.
Published: 01 June 2001
..., thermomechanical processing, and care in annealing treatments. TLSTM H13 PQ (Hot Work Tool Steel) Filing Code: TS-588 Tool Steel June 2001 TLSTM H13 PQ Chemical Composition, wt (Typical) Carbon 0.40 Manganese 0.40 Sulfur 0.001 Silicon 1.00 Chromium 5.25 Molybdenum 1.35 Vanadium 1.00 Iron bal Physical Properties...