Skip Nav Destination
Close Modal
Search Results for
hot work punches
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 477 Search Results for
hot work punches
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
1
Sort by
Journal Articles
Alloy Digest (1964) 13 (7): TS-149.
Published: 01 July 1964
... Peerless 56 was designed as an improved low-alloy hot-work steel possessing a combination of high tensile strength and hardness with roughness. It is recommended for extrusion dies, hot billet shears and hot work punches. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
Peerless 56 was designed as an improved low-alloy hot-work steel possessing a combination of high tensile strength and hardness with roughness. It is recommended for extrusion dies, hot billet shears and hot work punches. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-149. Producer or source: Crucible Steel Company of America.
Journal Articles
Alloy Digest (1985) 34 (6): TS-442.
Published: 01 June 1985
... a combination of high tensile strength and hardness with excellent toughness. Typical hot work applications include forging dies, extrusion dies, hot header dies, mandrels, punches and piercing tools. Consult the manufacturer for specific recommendations. Composition: Carbon Manganese Silicon Chromium Vanadium...
Abstract
View article
PDF
AISI Type H10 is a hot-work tool steel of the chromium type, although it contains a substantial amount of molybdenum. It is a high-hardenability steel and possesses a combination of high tensile strength and hardness with excellent toughness. Typical hot work applications include forging dies, extrusion dies, hot header dies, mandrels, punches and piercing tools. Consult the manufacturer for specific recommendations. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-442. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1984) 33 (1): TS-421.
Published: 01 January 1984
... AL TECH NAVAHO is an air-hardening punch and die steel with lower carbon than most cold-work steels; this provides an optimum combination of wear resistance and toughness for difficult cold-work applications. It also is used for abrasive hot-work requirements. This steel offers relatively...
Abstract
View article
PDF
AL TECH NAVAHO is an air-hardening punch and die steel with lower carbon than most cold-work steels; this provides an optimum combination of wear resistance and toughness for difficult cold-work applications. It also is used for abrasive hot-work requirements. This steel offers relatively favorable size stability and exceptional secondary hardness characteristics. NAVAHO has a broad application range from shear blades and punches to molds for plastics ad hot-work tooling. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-421. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Alloy Digest (1981) 30 (4): TS-381.
Published: 01 April 1981
... be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides information...
Abstract
View article
PDF
AISI Type H12 is a general-purpose, low-carbon, chromium-molybdenum-tungsten hot-work steel for tools and dies that require high toughness. It has high hardenability and offers high resistance to softening in service at elevated temperatures. It also offers good resistance to heat checking and may be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-381. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1986) 35 (1): TS-453.
Published: 01 January 1986
... checking and may be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides...
Abstract
View article
PDF
UNS No. T20812 is a low-carbon chromium-molybdenum-tungsten hot-work steel for general purposers. It is used for dies and tools that require high toughness. It has high hardenability and offers high resistance to softening in service at elevated temperatures. It also offers good resistance to heat checking and may be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-453. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1984) 33 (1): TS-420.
Published: 01 January 1984
... hot-work applications include extrusion dies for copper and brass, long-running die-casting dies, piercer points and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing...
Abstract
View article
PDF
W.W. HOT WORK is a chromium-tungsten hot-work tool and die steel containing nominally 1.05% vanadium. It is characterized by high strength and hardness at elevated temperature and good resistance to heat checking. It has high hardenability and can be hardened by quenching in salt or oil. Its many hot-work applications include extrusion dies for copper and brass, long-running die-casting dies, piercer points and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-420. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1968) 17 (10): TS-211.
Published: 01 October 1968
... CROMO-W is a general purpose hot work tool and die steel having excellent resistance to wear, shock, and drastic changes in temperature. It is recommended for hot shear blades, forging and bolt heading dies, punches and other types of hot work tools. This datasheet provides information...
Abstract
View article
PDF
CROMO-W is a general purpose hot work tool and die steel having excellent resistance to wear, shock, and drastic changes in temperature. It is recommended for hot shear blades, forging and bolt heading dies, punches and other types of hot work tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-211. Producer or source: Bethlehem Steel Corporation.
Journal Articles
Alloy Digest (1986) 35 (11): TS-465.
Published: 01 November 1986
...-work applications. Another feature of this versatile die steel is its outstanding secondary hardness associated with remarkable tempering resistance up to 900 F. Typical applications comprise blanking dies, swaging dies, hot and cold-piercing punches, forming rolls, shear blades and coining dies...
Abstract
View article
PDF
AL TECH CHEROKEE is a high-carbon, high-chromium die steel containing nominally 3.25% cobalt. The cobalt provides effective resistance to galling and pickup as well as improved hot hardness. The cobalt enables this steel to perform exceptionally well on both extended cold-work and moderate hot-work applications. Another feature of this versatile die steel is its outstanding secondary hardness associated with remarkable tempering resistance up to 900 F. Typical applications comprise blanking dies, swaging dies, hot and cold-piercing punches, forming rolls, shear blades and coining dies. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-465. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Alloy Digest (1983) 32 (6): TS-414.
Published: 01 June 1983
..., good wear resistance., excellent toughness and easy machining are important. These properties make it suitable for many hot-work and cold- work applications. Among its many uses are blanking dies. shear blades. punches and chisels. l GUTERL is a registered trademark of Guterl Special Steel Corporation...
Abstract
View article
PDF
GUTERL S-7 is a chromium-molybdenum, general-purpose, air-hardening tool steel recommended for uses where shock resistance, good hot-work properties, good wear resistance, excellent toughness and easy machining are important. These properties make it suitable for many hot-work and cold-work applications. Among its many uses are blanking dies, shear blades, punches and chisels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and surface treatment. Filing Code: TS-414. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Alloy Digest (1967) 16 (2): TS-189.
Published: 01 February 1967
... Jessop-Saville H.50 is an air or oil hardening hot work tool steel recommended for die casting dies, hot punches, shear blades and pressing tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Abstract
View article
PDF
Jessop-Saville H.50 is an air or oil hardening hot work tool steel recommended for die casting dies, hot punches, shear blades and pressing tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-189. Producer or source: Jessop-Saville Ltd, Brightside Works.
Journal Articles
Alloy Digest (1981) 30 (9): TS-386.
Published: 01 September 1981
..., cold-work die steel. It also is used in some applications as a hot-work tool and die steel. An excellent combination of high hardenability, good wear resistance and toughnessmakes Hotform No. 3 useful for special tools. Typical applications are blanking dies, cold-forming dies, punches and cold and hot...
Abstract
View article
PDF
HOTFORM No. 3 is a medium-carbon, air-hardening, cold-work die steel. It also is used in some applications as a hot-work tool and die steel. An excellent combination of high hardenability, good wear resistance and toughness makes Hotform No. 3 useful for special tools. Typical applications are blanking dies, cold-forming dies, punches and cold and hot shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-386. Producer or source: Teledyne Vasco.
Journal Articles
Alloy Digest (1967) 16 (4): TS-192.
Published: 01 April 1967
... Mustang-LC is a tungsten-molybdenum high-speed steel specially developed for hot work applications requiring long die life. It is recommended for hot forming and swaging dies, hot extrusion dies, hot punches, etc. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
Mustang-LC is a tungsten-molybdenum high-speed steel specially developed for hot work applications requiring long die life. It is recommended for hot forming and swaging dies, hot extrusion dies, hot punches, etc. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-192. Producer or source: Jessop Steel Company.
Journal Articles
Alloy Digest (1985) 34 (11): TS-450.
Published: 01 November 1985
... FIREDIE 9 is a chromium-molybdenum-cobalt hot-work steel. It has outstanding resistance to softening in elevated-temperature service; the cobalt gives this steel its superior heat resistance. Firedie 9 has excellent resistance to thermal shock; in fact, dies can be water cooled durin operation...
Abstract
View article
PDF
FIREDIE 9 is a chromium-molybdenum-cobalt hot-work steel. It has outstanding resistance to softening in elevated-temperature service; the cobalt gives this steel its superior heat resistance. Firedie 9 has excellent resistance to thermal shock; in fact, dies can be water cooled durin operation without fear of cracking. Among its many applications are forging dies, hot-extrusion mandrels, hot-shear blades, die-casting dies and hot punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-450. Producer or source: Columbia Tool Steel Company.
Journal Articles
Alloy Digest (1986) 35 (9): TS-462.
Published: 01 September 1986
... FIREDIE 13 is the standard 5% chromium hot-work tool steel with increased vanadium for improved wear resistance and toughness. In addition, this steel possesses excellent hot-hardness properties. Its many applications include die-casting tools (for Al, Mg and Zn), extrusion tools (for Al and Mg...
Abstract
View article
PDF
FIREDIE 13 is the standard 5% chromium hot-work tool steel with increased vanadium for improved wear resistance and toughness. In addition, this steel possesses excellent hot-hardness properties. Its many applications include die-casting tools (for Al, Mg and Zn), extrusion tools (for Al and Mg), hot-heading dies, forging dies, hot punches and heavy shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-462. Producer or source: Columbia Tool Steel Company.
Journal Articles
Alloy Digest (1987) 36 (11): TS-484.
Published: 01 November 1987
... AL TECH B-47 is a chromium-tungsten-cobalt-vanadium steel with excellent resistance to shock and abrasion at elevated temperatures. Its good hot hardness enables it to handle many hot-work jobs without washing out or changing size. B-47 has very good mechanical properties at elevated temperatures...
Abstract
View article
PDF
AL TECH B-47 is a chromium-tungsten-cobalt-vanadium steel with excellent resistance to shock and abrasion at elevated temperatures. Its good hot hardness enables it to handle many hot-work jobs without washing out or changing size. B-47 has very good mechanical properties at elevated temperatures where typical applications include extrusion dies for brass, hot-punch tools and forging-die inserts. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-484. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Alloy Digest (1989) 38 (2): TS-496.
Published: 01 February 1989
... dummy blocks for copper or brass. permanent molds for brass casting, hot-forging-die inserts. hot-work dies. hot-press dies for both steel and brass, hot-punch tools, valve extrusion die rings and inserts. forging dia. hotcxtrusicm die inserrsforstecL Manufacturers: Tool steel milLs. ...
Abstract
View article
PDF
UNS T20819 is a hot-work tool and die steel that is characterized by excellent resistance to shock and abrasion at elevated temperatures. This steel provides relatively high toughness and outstanding resistance to heat checking and softening at elevated temperatures. Among its many applications are hot-punch tools, forging dies and inserts, brass extrusion dies, permanent molds for brass casting and hot-extrusion die inserts for steel. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-496. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1974) 23 (12): TS-280.
Published: 01 December 1974
... POTOMAC 2V punches wear resistance workability POTOMAC 2V Filing Code: l-s-290 Tool Steel DECEMBER 1974 AlI 07 DIGEST d - DATA ON WORLD WIDE METALS AND ALLOYS Pnblisbd by POTOMAC* 2V Enginecr~ Alloys Die Inc. Upper Moncchir. New Jersey (Hot-Work Tool Steel) POTOMAC 2V is a high-carbon. high-vanadium...
Abstract
View article
PDF
POTOMAC 2V is a high-carbon, high-vanadium modification of the well-known 5% chromium hot-work tool steel. It has improved wear resistance and the necessary toughness for severe forming applications. It is recommended for such applications as hot dies for extrusions and forgings, piercing points and hot punches. This datasheet provides information on composition, physical properties, and hardness as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-280. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Alloy Digest (1982) 31 (7): TS-401.
Published: 01 July 1982
... molds for brass casting, hot-forging-die inserts. hot-work dies, hot-press dies for both steel and brass, hot-punch tools, valve ex- trusion die rings and inserts. forging dies, hot-extrusion die inserts for steel. Manufacturers: Tool steel mills. ...
Abstract
View article
PDF
AISI Type H19 is a hot-work tool and die steel that is characterized by excellent resistance to shock and abrasion at elevated temperatures. This steel provides relatively high toughness and outstanding resistance to heat checking and softening at elevated temperatures. Among its many applications are hot-punch tools, forging dies and inserts, brass extrusion dies, permanent molds for brass casting and hot-extrusion die inserts for steel. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-401. Producer or source: Tool steel mills.
Journal Articles
Alloy Digest (1968) 17 (2): TS-202.
Published: 01 February 1968
... FAGERSTA-D66 is a 9% tungsten type hot-work tool and die steel having excellent combination of abrasion resistance, red-hardness and toughness at high operating temperatures. It is recommended for hot extrusion and forming dies, punches, rivet sets, shear blades, etc. This datasheet provides...
Abstract
View article
PDF
FAGERSTA-D66 is a 9% tungsten type hot-work tool and die steel having excellent combination of abrasion resistance, red-hardness and toughness at high operating temperatures. It is recommended for hot extrusion and forming dies, punches, rivet sets, shear blades, etc. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-202. Producer or source: Fagersta Steels Inc..
Journal Articles
Alloy Digest (1968) 17 (8): TS-209.
Published: 01 August 1968
... Thermold-H10 is a chromium-molybdenum hot work steel that exhibits excellent resistance to softening at elevated temperatures. It is recommended for hot punches and shears, mandrels, and aluminum die casting dies. This datasheet provides information on composition, physical properties, hardness...
Abstract
View article
PDF
Thermold-H10 is a chromium-molybdenum hot work steel that exhibits excellent resistance to softening at elevated temperatures. It is recommended for hot punches and shears, mandrels, and aluminum die casting dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-209. Producer or source: Cyclops Corporation.
1