Skip Nav Destination
Close Modal
Search Results for
hot shear blades
Update search
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
Filter
- Title
- Authors
- Author Affiliations
- Full Text
- Abstract
- Keywords
- DOI
- ISBN
- EISBN
- Issue
- ISSN
- EISSN
- Volume
- References
NARROW
Format
Topics
Subjects
Journal
Article Type
Date
Availability
1-20 of 288 Search Results for
hot shear blades
Follow your search
Access your saved searches in your account
Would you like to receive an alert when new items match your search?
Sort by
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (4): TS-381.
Published: 01 April 1981
... be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides information...
Abstract
View article
PDF
AISI Type H12 is a general-purpose, low-carbon, chromium-molybdenum-tungsten hot-work steel for tools and dies that require high toughness. It has high hardenability and offers high resistance to softening in service at elevated temperatures. It also offers good resistance to heat checking and may be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-381. Producer or source: Tool steel mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1985) 34 (11): TS-450.
Published: 01 November 1985
... without fear of cracking. Among its many applications are forging dies, hot-extrusion mandrels, hot-shear blades, die-casting dies and hot punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating...
Abstract
View article
PDF
FIREDIE 9 is a chromium-molybdenum-cobalt hot-work steel. It has outstanding resistance to softening in elevated-temperature service; the cobalt gives this steel its superior heat resistance. Firedie 9 has excellent resistance to thermal shock; in fact, dies can be water cooled durin operation without fear of cracking. Among its many applications are forging dies, hot-extrusion mandrels, hot-shear blades, die-casting dies and hot punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-450. Producer or source: Columbia Tool Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (1): TS-453.
Published: 01 January 1986
... checking and may be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides...
Abstract
View article
PDF
UNS No. T20812 is a low-carbon chromium-molybdenum-tungsten hot-work steel for general purposers. It is used for dies and tools that require high toughness. It has high hardenability and offers high resistance to softening in service at elevated temperatures. It also offers good resistance to heat checking and may be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-453. Producer or source: Tool steel mills.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1974) 23 (9): Ni-208.
Published: 01 September 1974
... HAYNES Alloy No. 273 is a nickel-base, hard-facing alloy developed to provide extra life for hot-working equipment such as hot-forging dies, hot-shear blades and hot-extrusion dies. It is deposited by using a composite electrode with nickel-base core and the balance of the alloying elements...
Abstract
View article
PDF
HAYNES Alloy No. 273 is a nickel-base, hard-facing alloy developed to provide extra life for hot-working equipment such as hot-forging dies, hot-shear blades and hot-extrusion dies. It is deposited by using a composite electrode with nickel-base core and the balance of the alloying elements in the flux coating. Deposits retain their hardness up to 1200 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-208. Producer or source: Cabot Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (10): TS-211.
Published: 01 October 1968
... CROMO-W is a general purpose hot work tool and die steel having excellent resistance to wear, shock, and drastic changes in temperature. It is recommended for hot shear blades, forging and bolt heading dies, punches and other types of hot work tools. This datasheet provides information...
Abstract
View article
PDF
CROMO-W is a general purpose hot work tool and die steel having excellent resistance to wear, shock, and drastic changes in temperature. It is recommended for hot shear blades, forging and bolt heading dies, punches and other types of hot work tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-211. Producer or source: Bethlehem Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (5): TS-219.
Published: 01 May 1969
... Carpenter T-K is a tungsten-chromium type hot-work steel having good red-hardness and resistance to abrasion. It will withstand high operating temperatures up to 1000 F for long periods. It is recommended for hot shear blades, forging and extrusion dies, hot compression tools, and similar...
Abstract
View article
PDF
Carpenter T-K is a tungsten-chromium type hot-work steel having good red-hardness and resistance to abrasion. It will withstand high operating temperatures up to 1000 F for long periods. It is recommended for hot shear blades, forging and extrusion dies, hot compression tools, and similar applications where high compressive strength and wear resistance at elevated temperatures are required. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-219. Producer or source: Carpenter.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1981) 30 (9): TS-386.
Published: 01 September 1981
... are blanking dies, cold-forming dies, punches and cold and hot shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-386. Producer or source...
Abstract
View article
PDF
HOTFORM No. 3 is a medium-carbon, air-hardening, cold-work die steel. It also is used in some applications as a hot-work tool and die steel. An excellent combination of high hardenability, good wear resistance and toughness makes Hotform No. 3 useful for special tools. Typical applications are blanking dies, cold-forming dies, punches and cold and hot shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-386. Producer or source: Teledyne Vasco.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (2010) 59 (11): TS-694.
Published: 01 November 2010
... Thermodur 2714 is a tough die steel with high tempering resistance and good through hardening. Typical applications include forging dies, mandrels, die holders, armored trim dies, and hot-shear blades. This datasheet provides information on composition, physical properties, and hardness. It also...
Abstract
View article
PDF
Thermodur 2714 is a tough die steel with high tempering resistance and good through hardening. Typical applications include forging dies, mandrels, die holders, armored trim dies, and hot-shear blades. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming and heat treating. Filing Code: TS-694. Producer or source: Schmolz + Bickenbach USA Inc.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1969) 18 (4): TS-217.
Published: 01 April 1969
... EB alloy is a high-carbon chromium alloy steel for general hot-work applications. It possesses good compressive strength and hot mechanical properties. It is recommended for hot header and gripper dies, shear blades, hot rivet sets, forging dies, cold forming and embossing dies. This datasheet...
Abstract
View article
PDF
EB alloy is a high-carbon chromium alloy steel for general hot-work applications. It possesses good compressive strength and hot mechanical properties. It is recommended for hot header and gripper dies, shear blades, hot rivet sets, forging dies, cold forming and embossing dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-217. Producer or source: Allegheny Ludlum Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (9): TS-462.
Published: 01 September 1986
...), hot-heading dies, forging dies, hot punches and heavy shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-462. Producer or source: Columbia Tool Steel...
Abstract
View article
PDF
FIREDIE 13 is the standard 5% chromium hot-work tool steel with increased vanadium for improved wear resistance and toughness. In addition, this steel possesses excellent hot-hardness properties. Its many applications include die-casting tools (for Al, Mg and Zn), extrusion tools (for Al and Mg), hot-heading dies, forging dies, hot punches and heavy shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-462. Producer or source: Columbia Tool Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (11): TS-465.
Published: 01 November 1986
...-work applications. Another feature of this versatile die steel is its outstanding secondary hardness associated with remarkable tempering resistance up to 900 F. Typical applications comprise blanking dies, swaging dies, hot and cold-piercing punches, forming rolls, shear blades and coining dies...
Abstract
View article
PDF
AL TECH CHEROKEE is a high-carbon, high-chromium die steel containing nominally 3.25% cobalt. The cobalt provides effective resistance to galling and pickup as well as improved hot hardness. The cobalt enables this steel to perform exceptionally well on both extended cold-work and moderate hot-work applications. Another feature of this versatile die steel is its outstanding secondary hardness associated with remarkable tempering resistance up to 900 F. Typical applications comprise blanking dies, swaging dies, hot and cold-piercing punches, forming rolls, shear blades and coining dies. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-465. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (6): TS-414.
Published: 01 June 1983
..., good wear resistance., excellent toughness and easy machining are important. These properties make it suitable for many hot-work and cold- work applications. Among its many uses are blanking dies. shear blades. punches and chisels. l GUTERL is a registered trademark of Guterl Special Steel Corporation...
Abstract
View article
PDF
GUTERL S-7 is a chromium-molybdenum, general-purpose, air-hardening tool steel recommended for uses where shock resistance, good hot-work properties, good wear resistance, excellent toughness and easy machining are important. These properties make it suitable for many hot-work and cold-work applications. Among its many uses are blanking dies, shear blades, punches and chisels. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, machining, and surface treatment. Filing Code: TS-414. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1984) 33 (1): TS-421.
Published: 01 January 1984
... favorable size stability and exceptional secondary hardness characteristics. NAVAHO has a broad application range from shear blades and punches to molds for plastics ad hot-work tooling. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Abstract
View article
PDF
AL TECH NAVAHO is an air-hardening punch and die steel with lower carbon than most cold-work steels; this provides an optimum combination of wear resistance and toughness for difficult cold-work applications. It also is used for abrasive hot-work requirements. This steel offers relatively favorable size stability and exceptional secondary hardness characteristics. NAVAHO has a broad application range from shear blades and punches to molds for plastics ad hot-work tooling. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: TS-421. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1967) 16 (2): TS-189.
Published: 01 February 1967
... Jessop-Saville H.50 is an air or oil hardening hot work tool steel recommended for die casting dies, hot punches, shear blades and pressing tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Abstract
View article
PDF
Jessop-Saville H.50 is an air or oil hardening hot work tool steel recommended for die casting dies, hot punches, shear blades and pressing tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-189. Producer or source: Jessop-Saville Ltd, Brightside Works.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1968) 17 (2): TS-202.
Published: 01 February 1968
... FAGERSTA-D66 is a 9% tungsten type hot-work tool and die steel having excellent combination of abrasion resistance, red-hardness and toughness at high operating temperatures. It is recommended for hot extrusion and forming dies, punches, rivet sets, shear blades, etc. This datasheet provides...
Abstract
View article
PDF
FAGERSTA-D66 is a 9% tungsten type hot-work tool and die steel having excellent combination of abrasion resistance, red-hardness and toughness at high operating temperatures. It is recommended for hot extrusion and forming dies, punches, rivet sets, shear blades, etc. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-202. Producer or source: Fagersta Steels Inc..
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1986) 35 (3): TS-455.
Published: 01 March 1986
... will withstand repeated heating to 700-800 F, when used in lower temperature hot-work applications. Among its many uses are shear blades, hand chisels, pneumatic tools, coining dies, hot-heading dies, forging dies and machine parts. This datasheet provides information on composition, physical properties...
Abstract
View article
PDF
BUSTER ALLOY 60 is a widely accepted tungsten shock-resisting tool steel. Its performance is unequalled in most shock and impact tools used under very demanding conditions. It is deep hardening and combines this quality with excellent wear resistance and good toughness. Buster Alloy 60 will withstand repeated heating to 700-800 F, when used in lower temperature hot-work applications. Among its many uses are shear blades, hand chisels, pneumatic tools, coining dies, hot-heading dies, forging dies and machine parts. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-455. Producer or source: Columbia Tool Steel Company.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1979) 28 (7): TS-352.
Published: 01 July 1979
... factors. It may be carburized for those applications where high wear resistance and great core strength are required. Its many applications include shear blades, rivet busters and forging dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also...
Abstract
View article
PDF
CYCLOPS S1 (formerly Alco M) was originally developed for chisel and pneumatic tool purposes. It is now used for many other cold and hot work applications because of its outstanding toughness and resistance to fatigue. It gives excellent results in those instances where shock and impact are major factors. It may be carburized for those applications where high wear resistance and great core strength are required. Its many applications include shear blades, rivet busters and forging dies. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-352. Producer or source: Cyclops Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1980) 29 (11): TS-372.
Published: 01 November 1980
... strength than ordinary high-carbon, high-chromium die steels. It is used for many types of dies, hot-piercing punches and shear blades. This datasheet provides information on composition, physical properties, and hardness as well as fracture toughness. It also includes information on forming, heat treating...
Abstract
View article
PDF
AL Tech D-5 is a high-carbon, high-chromium tool and die steel; it contains cobalt (3.30%) and is air-hardening and nondeforming. The cobalt impacts a pronounced secondary hardening effect in tempering and a non-galling effect. AL Tech D-5 has both superior abrasion resistance and greater edge strength than ordinary high-carbon, high-chromium die steels. It is used for many types of dies, hot-piercing punches and shear blades. This datasheet provides information on composition, physical properties, and hardness as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-372. Producer or source: AL Tech Specialty Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1982) 31 (3): TS-396.
Published: 01 March 1982
... boilermaker's tools, cold-battering hand and pneumatic tools, punches, shear blades and concrete drills and breakers. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment...
Abstract
View article
PDF
GUTERL S-1 is a chromium-tungsten steel for general use for chisels and other cold-battering tools. It also is used for numerous other cold and hot-work applications because of its excellent toughness, high hardness and strength, and resistance to fatigue. Its many applications include boilermaker's tools, cold-battering hand and pneumatic tools, punches, shear blades and concrete drills and breakers. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-396. Producer or source: Guterl Special Steel Corporation.
Journal Articles
Publisher: Journals Gateway
Alloy Digest (1983) 32 (7): TS-416.
Published: 01 July 1983
... for resistance to abrasion, fatigue and wear. It is used for both hot-work and cold-work applications. Among its many uses are automotive gears, forgings, gun barrels, shafts, wrenches, chisels, punches, lathe spindles, axes, shear blades, dies, files, reamers and drills. This datasheet provides information...
Abstract
View article
PDF
AISI Type 1.2 is a chromium-vanadium tool steel of modest hardenability and variable carbon content (nominally 0.50-1.10% carbon). At its lower carbon levels, it is used for tools requiring toughness and resistance to shock and vibration. At its higher carbon levels, it is recommended for resistance to abrasion, fatigue and wear. It is used for both hot-work and cold-work applications. Among its many uses are automotive gears, forgings, gun barrels, shafts, wrenches, chisels, punches, lathe spindles, axes, shear blades, dies, files, reamers and drills. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-416. Producer or source: Tool steel mills.