1-20 of 531 Search Results for

hot punches

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1985) 34 (11): TS-450.
Published: 01 November 1985
... without fear of cracking. Among its many applications are forging dies, hot-extrusion mandrels, hot-shear blades, die-casting dies and hot punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating...
Journal Articles
Alloy Digest (1986) 35 (9): TS-462.
Published: 01 September 1986
...), hot-heading dies, forging dies, hot punches and heavy shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-462. Producer or source: Columbia Tool Steel...
Journal Articles
Alloy Digest (1967) 16 (4): TS-192.
Published: 01 April 1967
... Mustang-LC is a tungsten-molybdenum high-speed steel specially developed for hot work applications requiring long die life. It is recommended for hot forming and swaging dies, hot extrusion dies, hot punches, etc. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1989) 38 (2): TS-496.
Published: 01 February 1989
... are hot-punch tools, forging dies and inserts, brass extrusion dies, permanent molds for brass casting and hot-extrusion die inserts for steel. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on high...
Journal Articles
Alloy Digest (1974) 23 (12): TS-280.
Published: 01 December 1974
... and hot punches. This datasheet provides information on composition, physical properties, and hardness as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: TS-280. Producer...
Journal Articles
Alloy Digest (1982) 31 (7): TS-401.
Published: 01 July 1982
... are hot-punch tools, forging dies and inserts, brass extrusion dies, permanent molds for brass casting and hot-extrusion die inserts for steel. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat...
Journal Articles
Alloy Digest (1987) 36 (11): TS-484.
Published: 01 November 1987
... where typical applications include extrusion dies for brass, hot-punch tools and forging-die inserts. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on high temperature performance as well...
Journal Articles
Alloy Digest (1968) 17 (8): TS-209.
Published: 01 August 1968
... Thermold-H10 is a chromium-molybdenum hot work steel that exhibits excellent resistance to softening at elevated temperatures. It is recommended for hot punches and shears, mandrels, and aluminum die casting dies. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1969) 18 (9): TS-223.
Published: 01 September 1969
... HALCOMB 425 is a hot work tool steel having excellent resistance to shock and abrasion at elevated temperatures. It is recommended for brass and copper extrusion dies, forging dies and inserts, and hot punches. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1967) 16 (2): TS-189.
Published: 01 February 1967
... Jessop-Saville H.50 is an air or oil hardening hot work tool steel recommended for die casting dies, hot punches, shear blades and pressing tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness...
Journal Articles
Alloy Digest (1984) 33 (1): TS-421.
Published: 01 January 1984
... AL TECH NAVAHO is an air-hardening punch and die steel with lower carbon than most cold-work steels; this provides an optimum combination of wear resistance and toughness for difficult cold-work applications. It also is used for abrasive hot-work requirements. This steel offers relatively...
Journal Articles
Alloy Digest (1986) 35 (1): TS-453.
Published: 01 January 1986
... checking and may be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides...
Journal Articles
Alloy Digest (1981) 30 (4): TS-381.
Published: 01 April 1981
... be water cooled in service. It is suitable for hot-work applications involving severe conditions of shock and sudden temperature changes. Its many applications include hot shear blades, forging dies, extrusion dies, punches and other types of hot-work tools. This datasheet provides information...
Journal Articles
Alloy Digest (1985) 34 (6): TS-442.
Published: 01 June 1985
..., extrusion dies, hot header dies, mandrels, punches and piercing tools. Consult the manufacturer for specific recommendations. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on high temperature...
Journal Articles
Alloy Digest (1986) 35 (11): TS-465.
Published: 01 November 1986
...-work applications. Another feature of this versatile die steel is its outstanding secondary hardness associated with remarkable tempering resistance up to 900 F. Typical applications comprise blanking dies, swaging dies, hot and cold-piercing punches, forming rolls, shear blades and coining dies...
Journal Articles
Alloy Digest (1968) 17 (10): TS-211.
Published: 01 October 1968
... CROMO-W is a general purpose hot work tool and die steel having excellent resistance to wear, shock, and drastic changes in temperature. It is recommended for hot shear blades, forging and bolt heading dies, punches and other types of hot work tools. This datasheet provides information...
Journal Articles
Alloy Digest (1964) 13 (7): TS-149.
Published: 01 July 1964
... Peerless 56 was designed as an improved low-alloy hot-work steel possessing a combination of high tensile strength and hardness with roughness. It is recommended for extrusion dies, hot billet shears and hot work punches. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1984) 33 (1): TS-420.
Published: 01 January 1984
... hot-work applications include extrusion dies for copper and brass, long-running die-casting dies, piercer points and punches. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing...
Journal Articles
Alloy Digest (1999) 48 (1): TS-566.
Published: 01 January 1999
... Vanadis 30 is cobalt alloyed high-performance, high-speed steel made by powder metallurgy. The cobalt addition of approximately 8.5% has a positive influence on the hot strength, hot hardness, temper resistance, and modulus of elasticity. Punches are a suitable application for this alloy...
Journal Articles
Alloy Digest (1968) 17 (2): TS-202.
Published: 01 February 1968
... FAGERSTA-D66 is a 9% tungsten type hot-work tool and die steel having excellent combination of abrasion resistance, red-hardness and toughness at high operating temperatures. It is recommended for hot extrusion and forming dies, punches, rivet sets, shear blades, etc. This datasheet provides...