Alloy Digest (1957) 6 (8): Mg-33.
Published: 01 August 1957
... ECLIPSALOY 130 is a magnesium die casting alloy having improved ductility, high corrosion, and impact resistance. The alloy was developed primarily to obtain an alloy of magnesium for die casting with less hot cracking tendency than those in use at the time of its development. This datasheet...
Journal Articles
Alloy Digest (1984) 33 (1): TS-420.
Published: 01 January 1984
... temperature should be about 2 hours per inch of greatest cross section. Distortion: W. W. Hot Work has medium distortion when quenched in oil. It has high safety (against cracking) in hardening. Decarburization: W. W. Hot Work steel will not decarburize provided the user follows the standard precautions for...
Journal Articles
Alloy Digest (1971) 20 (5): CS-40.
Published: 01 May 1971
... properties workability SUPERFORM Filing Code: cs40 Carbon Steel MAY 1971 DIGEST fl - DATA ON WORLD WIDE METALS AND ALLOYS Pnblisbsd by Engineering Alloys Digest, Inc. Upper Montclair, New Jersey SUPERFORM (Hot-Rolled Steel for Cold Forming) SUPERFORM is produced in two grades: SUPERFORM 30 is recommended...
Journal Articles
Alloy Digest (1960) 9 (7): TS-95.
Published: 01 July 1960
... that it may become quite hot in opera- tion without sinking. It will withstand water cool- ing while in operation without danger of checking or cracking. Choice No. 1 can be satisfactorily heat treated over a wide temperature range, and for many types of dies it can be given a heat treatment which will...
Journal Articles
Alloy Digest (2012) 61 (7): TS-705.
Published: 01 July 2012
... Böhler (or Boehler) W303 is a hot work tool steel featuring excellent hot tensile properties with retention of hardness. This datasheet provides information on composition, physical properties, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS...
Journal Articles
Alloy Digest (1961) 10 (2): TS-102.
Published: 01 February 1961
... Type H13 JIG No H6 General Characteristics: Because of its composition Drvsr has the following properries which are of great vslue for hot work sppli- cations in general and particularly for aluminum die- csstiug dies: ability to harden sstisbcrorily in air, miuirsum tendency ro scale on sir cooling...
Journal Articles
Alloy Digest (1964) 13 (1): TS-142.
Published: 01 January 1964
... Characteristics: CROMO-N is a low carbon, high chromium hot work tool and die steel, developed specifi- cally to combat heat-checking and resultant cracking. To insure development of the re- quired hardness, the alloy few-ures an addition of nitrogen. Forms Available: Billets, bars and forgings Applications...
Journal Articles
Alloy Digest (1986) 35 (5): SA-419.
Published: 01 May 1986
... elasticity, psi (Tension) Modulus of rigidity, psi (Torsion) PROPERTIES Table 1 - TYPICAL ROOM-TEMPERATURE MECHANICAL PROPERTIES (l-in. Dia Bar) Property Hot Rolled Annealed Normalized - - Tensile strength, psi 144000 103000 148000 Yield point, psi 115000 73000 120000 Elongation (2 in % 15 21 15 Reduction of...
Journal Articles
Alloy Digest (1979) 28 (12): SA-366.
Published: 01 December 1979
...) 28-30 x 106 Modulus of rigidity, psi (Torsion) 12 x 106 PROPERTIES Table 1 - TYPICAL ROOM-TEMPERATURE MECHANICAL PROPERTIES (l-in. Dia Bar) Hot Roww Rolled Annealed Normalized Tensile strength, psi 123000 90000 125000 Yield point, psi 85000 59000 89000 Elongation (2 in % 18 26 20 Reduction of area...
Journal Articles
Alloy Digest (1980) 29 (3): SA-370.
Published: 01 March 1980
... (Torsion) 12~ 106 PROPERTIES Table 1 - TYPICAL ROOM-TEMPERATURE MECHANICAL PROPERTIES (l-in. Dia Bar) Hot Property Rolled Annealed Tensile strength, psi 129000 95000 Yield point, psi 90000 64000 Elongation (2 in % 17 25 Reduction of area. E 45 51 BrineU hardness 263 195 Normalized 132000 93000 19 50 270...
Journal Articles
Alloy Digest (1980) 29 (8): SA-375.
Published: 01 August 1980
... resistivity, microhm-cm Modulus of elasticity, psi (Tension) Modulus of rigidity, psi (Torsion) PROPERTIES Table 1 - TYPICAL ROOM-TEMPERATURE MECHANICAL PROPERTIES Property Hot Rolled Annealed Normalized - - Tensile strength, psi 144000 103000 148000 Yield poinr, psi 115000 73000 120000 Elongation (2 in L c...
Journal Articles
Alloy Digest (1985) 34 (7): SS-461.
Published: 01 July 1985
... elongation less than 2OTc. Table 2 - EFFECT OF HEAT TREATMENT (Data are from standard 0.505-in. tensile specimens machined from bars) Tensile Yield Strength Strength (0.2ce Offset) Heat Treatment psi psi As hot rolled 89000- IO0000 78000-88000 1450 F-l hr-air cool 69000 37700 1450 F-l hr-furnace cool 70000...
Journal Articles
Alloy Digest (2002) 51 (11): SS-867.
Published: 01 November 2002
... weldable by the common fusion and resistance techniques. Special consideration is required to avoid weld hot cracking by assuring formation of ferrite in the weld deposit. This particular alloy is gen- erally considered to have comparable weldability to Types 304 and 304L, but autogenous arc welding...
Journal Articles
Alloy Digest (1984) 33 (2): SA-397.
Published: 01 February 1984
... 7.84 0. I2 6.4 x lO-6 6.8 x IO-6 7.2 x IO-6 0. IO 22 29-30 x lo6 12x lo6 Table 1 - TYPICAL ROOM-TEMPERATURE MECHANICAL PROPERTIES (l-in. Dia Bar) Property Tensile strength, psi Yield point, psi Elongation (2 in B Reduction of area, $ Brinell hardness Hot Rolled I66000 120000 IO 25 335 Annealed...
Journal Articles
Alloy Digest (1969) 18 (1): Al-183.
Published: 01 January 1969
... resistance to hot cracking, fair resistance to pressure tightness, good fluidity, and fair solidification shrinkage tendency. It does not respond to a strengthening heat treatment. The alloy has good strength at elevated temperatures. Forms Available: Ingots and sand castings. Applications: Ornamental...
Journal Articles
Alloy Digest (1965) 14 (12): Al-150.
Published: 01 December 1965
... Silafont-7 is an aluminum piston alloy for sand, permanent mold and die castings. It has high strength, particularly good hot-crack resistance and limited corrosion resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also...
Journal Articles
Alloy Digest (1966) 15 (5): Ni-113.
Published: 01 May 1966
... HASTELLOY Alloy G is a nickel-base alloy recommended for tough environmental applications. It resists hot sulfuric and phosphoric acid service, and is also resistant to stress-corrosion cracking. This alloy is covered by U.S. Pat. No. 2,777,766. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1955) 4 (9): Mg-19.
Published: 01 September 1955
... ELEKTRON ZW3 is a high strength wrought magnesium alloy. It shows improved hot formability; it is free from stress-corrosion cracking in service and is readily weldable by the argonarc and heliarc machine processes and by the manual method for simple joints. This datasheet provides information on...
Journal Articles
Alloy Digest (2003) 52 (1): Ni-600.
Published: 01 January 2003
... and base metal/filler material should take place with no tendency towards crater cracking or hot crack- ing. No deleterious second-phase precipitation occurs in the heat- affected zone. See also Table 1. ALLCORR® Filing Code: Ni-600 Nickel January 2003 ALLCORR® (Corrosion-Resistant Nickel-Base Alloy...
Journal Articles
Alloy Digest (1977) 26 (5): Al-226.
Published: 01 May 1977
... to the stability of its chemical analysis on melting and remelting, and the relative ease of pouring dross-free castings. Likewise, it has good castability with respect to mold-filling properties, rel- ative freedom from cracking and hot-shortness, ease of feeding and tendency toward low shrinkage...