1-20 of 208 Search Results for

hot billet shears

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1964) 13 (7): TS-149.
Published: 01 July 1964
... Peerless 56 was designed as an improved low-alloy hot-work steel possessing a combination of high tensile strength and hardness with roughness. It is recommended for extrusion dies, hot billet shears and hot work punches. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1958) 7 (2): TS-67.
Published: 01 February 1958
... and magnesium extrusion, gripper and header dies, hot work punches, hot billet shears, shell piercing tools, inserts for forging dies and upsetters, extrusion shape dies and rams for low temperature brass extrusion. Manufacturer: Crucible Steel Co. ·of America Pittsburgh, Pennsylvania - - - ...
Journal Articles
Alloy Digest (1960) 9 (1): Mg-44.
Published: 01 January 1960
... MAGNESIUM ALLOY-TA54A is a general purpose hammer-forging alloy having intermediate strength. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information...
Journal Articles
Alloy Digest (2004) 53 (2): Co-95.
Published: 01 February 2004
... properties, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: CO-95. Producer or source: Special Metals Corporation. Originally published January 1995, revised February 2004. Producer...
Journal Articles
Alloy Digest (1985) 34 (11): TS-450.
Published: 01 November 1985
...) High red hardness. Forms Available: Billets, bars and forgings. Applications: Firedie 9 is used widely for forging dies, forging-die inserts. extrusion dies, hot-extrusion mandrels, hot- shear blades, die-casting dies, hot-trim dies, hot- gripper dies and hot punches. Manufacturer: Columbia Tool Steel...
Journal Articles
Alloy Digest (2002) 51 (7): Ti-129.
Published: 01 July 2002
... properties, and compressive, shear, and bearing strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TI-129. Producer or source: Carpenter Technology Corporation. Producer or Source: Carpenter Technology...
Journal Articles
Alloy Digest (1960) 9 (12): SS-111.
Published: 01 December 1960
... that work hardens very slowly. This steel work hardens more slowly than conventional 18-8 stainless steel and will remain non-magnetic after severe cold forming operations. Forms Available: Forging billets, hot rolled bars and forgings, cold drawn and ground bars, wire and wire rods, strip. Applications...
Journal Articles
Alloy Digest (2005) 54 (7): Ni-626.
Published: 01 July 2005
... Nimonic alloy PK33 is a nickel-base aerospace alloy developed to produce sheet with ultrahigh strength and good formability. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength as well as creep. It also includes information...
Journal Articles
Alloy Digest (1978) 27 (1): SS-346.
Published: 01 January 1978
..., tensile properties, and shear strength as well as fracture toughness. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-346. Producer or source: Carpenter. Producer or Source: Carpenter Copyright © ASM...
Journal Articles
Alloy Digest (1987) 36 (7): Be-5.
Published: 01 July 1987
...* Sonic velocity, ft/s (m/s) 41300 (12600) Modulus of elasticity, psi 44 x 106 MPa 305 x 103 *Seventeen times better than an equal thickness of aluminum. PROPERTIES Table 1 - MECHANICAL PROPERTIES (Sheet hot rolled from steel-enclosed billets of vacuum hot-pressed block) Tensile strength, psi (MPa...
Journal Articles
Alloy Digest (1986) 35 (9): TS-462.
Published: 01 September 1986
...), hot-heading dies, forging dies, hot punches and heavy shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, and machining. Filing Code: TS-462. Producer or source: Columbia Tool Steel...
Journal Articles
Alloy Digest (1985) 34 (3): TS-437.
Published: 01 March 1985
... of chromium and molybdenum. It is used for both cold and hot tooling applications. Its many uses include shear blades, swaging dies, chisels and dies for molding plastics below 1000 F (538 C). This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes...
Journal Articles
Alloy Digest (1986) 35 (3): TS-455.
Published: 01 March 1986
... very demanding conditions. This steel will withstand repeated heating to 700 to 800°F when used in lower temperature hot-work applica- tions. Forms Available: Billets. bars and forgings. Castings. Applications: The many applications for Buster Alloy 60 include shear blades. heavy punches, hand chisels...
Journal Articles
Alloy Digest (1981) 30 (9): TS-386.
Published: 01 September 1981
... are blanking dies, cold-forming dies, punches and cold and hot shear blades. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and surface treatment. Filing Code: TS-386. Producer or source...
Journal Articles
Alloy Digest (1955) 4 (3): TS-31.
Published: 01 March 1955
... where the more expensive hot work steels become uneco- nomicaL This grade has unusually good toughness at its highest obtainable hardness and as such is useful for certain cold work applications such as sheat blades. High transverse strength is also a property of this grade. Forms Available: Billets...
Journal Articles
Alloy Digest (1981) 30 (3): Cu-414.
Published: 01 March 1981
... working is excellent and it is suitable for fabrication by hot forging and pressing, hot heading and upsetting, and by cold blanking, drawing, forming, bending, heading, upsetting and shearing. It can be joined readily by soldering and brazing. Its suitability for welding by several convention- al...
Journal Articles
Alloy Digest (1992) 41 (10): Ti-80.
Published: 01 October 1992
...-3Al faces no known producibility barriersIndeed, slightvariationsincompositiondonotmarkedly affect the mechanical property response or the fabrication char- acteristics of Ti-6Al4V scrap. Maximum yield has been realized horn ingot to billet to forging because of Ti-lOV-2Fe-3Al s excellent hot...
Journal Articles
Alloy Digest (1979) 28 (7): TS-352.
Published: 01 July 1979
... CYCLOPS S1 (formerly Alco M) was originally developed for chisel and pneumatic tool purposes. It is now used for many other cold and hot work applications because of its outstanding toughness and resistance to fatigue. It gives excellent results in those instances where shock and impact are major...
Journal Articles
Alloy Digest (1981) 30 (8): TS-385.
Published: 01 August 1981
... but with normal precautions this gives no problems. It can be hot forged and hot rolled readily. In the annealed condition it has medium- togood ma&inability. Forms Available: Billets, bars, rods, plates and forgings. Applications: Bending dies, blanking dies, block and ring gages, broaches, coining dies, cold...
Journal Articles
Alloy Digest (1978) 27 (8): TS-337.
Published: 01 August 1978
... tools, end mills, extrusion dies, form tools, gear cutters, hobs, lathe tools, milling cutters, nail dies, paper knives, planer tools, piercing tools, punches - hot and cold, reamers, shear blades, slitting tools, slotting cutters, taps, threading tools, twist drills and wood-working tools. Manufacturer...