Alloy Digest (1999) 48 (7): Ni-555.
Published: 01 July 1999
... Crucible P/M N625 is a powder metallurgical nickel-base alloy with excellent corrosion resistance, high strength, chemical homogeneity, and thermal stability. Applications include use for highly corrosive situations in the marine, nuclear power, pulp and paper, and chemical process industries...
Journal Articles
Alloy Digest (2000) 49 (2): TS-572.
Published: 01 February 2000
... Compax Supreme is a further improvement of Compax (see Alloy Digest TS-488, March 1988). The alloy is extremely clean with a homogeneous microstructure. Sulfur is very low. Carbon is held to the high end of the range to consistently achieve high hardness for molds with larger cross sections...
Journal Articles
Alloy Digest (1953) 2 (4): Cu-7.
Published: 01 April 1953
... HY-TEN-SL No. 1 is a close-grained, tough, homogeneous metal, having the non-corrosive properties of bronze and the strength of alloy steel. It has good wear resisting qualities under heavy or shock loads. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1983) 32 (11): Cu-467.
Published: 01 November 1983
... PFINODAL C72900 is a copper-base alloy that derives its strength from spinodal hardening. It is produced by the manufacturer's wrought powder-metallurgy process for strip metal. This process provides the homogeneity and uniformity needed to achieve fully the available properties of the alloy...
Journal Articles
Alloy Digest (1985) 34 (4): TS-438.
Published: 01 April 1985
..., is an improved quality product with homogeneous macro and micro sections exhibiting a finer grain size, better toughness and superior grindability in the heat-treated condition than conventionally produced M42. This datasheet provides information on composition, physical properties, hardness, and elasticity...
Journal Articles
Alloy Digest (1993) 42 (7): SS-547.
Published: 01 July 1993
... surface finish; less distortion problems; more homogeneity in microstructures; and marginally increased resistance to corrosion. This datasheet provides information on composition and physical properties. It also includes information on machining. Filing Code: SS-547. Producer or source: Avesta Sheffield...
Journal Articles
Alloy Digest (1993) 42 (9): SS-549.
Published: 01 September 1993
... surface finish; less distortion problems; more homogeneity in microstructures; and marginally increased resistance to corrosion. This datasheet provides information on composition and physical properties. It also includes information on machining. Filing Code: SS-549. Producer or source: Avesta Sheffield...
Journal Articles
Alloy Digest (1993) 42 (11): SS-553.
Published: 01 November 1993
...; better surface finish; less distortion problems; more homogeneity in microstructures; and marginally increased resistance to corrosion. This datasheet provides information on composition and physical properties. It also includes information on machining. Filing Code: SS-553. Producer or source: Avesta...
Journal Articles
Alloy Digest (1993) 42 (12): TS-522.
Published: 01 December 1993
... PYROTOUGH 78 is a hot work die steel possessing a high degree of purity, homogeneity and microstructural integrity that produces a good combination of toughness and temper resistance. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well...
Journal Articles
Alloy Digest (1993) 42 (12): SS-557.
Published: 01 December 1993
...; better surface finish; less distortion problems; more homogeneity in microstructures; and marginally increased resistance to corrosion. This datasheet provides information on composition and physical properties. It also includes information on machining. Filing Code: SS-557. Producer or source: Avesta...
Journal Articles
Alloy Digest (1994) 43 (6): Cu-598.
Published: 01 June 1994
... Powder production of copper alloy C72650 achieves 100% density after a series of anneals and cold rolling operations. The technique prevents segregation in high tin alloys, produces a fine grain and homogeneity which favors the decomposition (spinoidal) reaction. Applications include springs...
Journal Articles
Alloy Digest (1994) 43 (7): TS-529.
Published: 01 July 1994
... CARPENTER 883 PLUS is a 5% Chromium hot work die steel designed for applications requiring both toughness and good red-hardness. It achieves this with higher purity, homogeneity and greater structural integrity than standard AISI type H13. This datasheet provides information on composition...
Journal Articles
Alloy Digest (2001) 50 (12): TS-595.
Published: 01 December 2001
... Crucible CPM REX M35HCHS is a modification of the AISI M2 high-speed steel by an addition of cobalt and produced by powder metallurgy to be homogeneous with good toughness. This datasheet provides information on composition, physical properties, microstructure, hardness, and elasticity. It also...
Journal Articles
Alloy Digest (2004) 53 (10): TS-607.
Published: 01 October 2004
... Boehler K390 Microclean is a cold work tool steel with an extremely good wear resistance combined with good toughness and a high compressive strength. This alloy is of powder metallurgical origins and is very homogeneous. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (2006) 55 (7): SS-967.
Published: 01 July 2006
... tool life, better surface finish, less distortion problems, more homogeneity in microstructures, and marginally increased resistance to corrosion. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information...
Journal Articles
Alloy Digest (2013) 62 (12): TS-724.
Published: 01 December 2013
... Böhler (or Boehler) W303 ISODISC is a hot work tool steel with outstanding hot tensile properties, high retention of hardness, good toughness, and resistance to heat checking. W303 ISODISC is a special grade with improved homogeneity and increased toughness. This datasheet provides information...
Journal Articles
Alloy Digest (2010) 59 (7): CS-154.
Published: 01 July 2010
... Ancorsteel 150 HP is a good base powder for a wide range of hybrid alloy systems. In the powder production process used to make Ancorsteel, molten steel is atomized into irregular, homogeneous particles which are then annealed to produce uniform, dependable steel powders. Ancorsteel grades...
Journal Articles
Alloy Digest (2010) 59 (8): CS-155.
Published: 01 August 2010
... Ancorsteel 721 SH is a water atomized, prealloyed steel powder specifically developed for sinter hardenings. In the powder production process used to make Ancorsteel, molten steel is atomized into irregular, homogeneous particles which are then annealed to produce uniform, dependable steel powders...
Journal Articles
Alloy Digest (2010) 59 (9): CS-156.
Published: 01 September 2010
... Ancorsteel 737SH is water atomized, prealloyed steel powder specifically developed for heat treatment by either the sinter-hardening process or conventional quenching and tempering. In the powder production process used to make Ancorsteel, molten steel is atomized into irregular, homogeneous...
Journal Articles
Alloy Digest (2010) 59 (10): CS-157.
Published: 01 October 2010
... Ancorsteel 2000 is a water atomized low-alloy powder metal containing Ni, Mo, and Mn and is useful in powder metal parts requiring greater hardenability. In the powder production process used to make Ancorsteel, molten steel is atomized into irregular, homogeneous particles which are then annealed...