1-9 of 9 Search Results for

highway trailers

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (1984) 33 (12): Al-254.
Published: 01 December 1984
... ALUMINUM 535.0 is a high-purity aluminum alloy of the aluminum-magnesium type. It possesses a high and stable combination of strength, shock resistance and ductility in the cast condition. Among its many applications are armament, hardware, cooking utensils, highway trailers, textile machinery and...
Journal Articles
Alloy Digest (2004) 53 (5): CS-143.
Published: 01 May 2004
... Algoma 130 is a cost-effective choice for applications that require high strength, improved notch toughness, weldability, and good formability. It is one in a full range of heat treated plate products for highway trailers, mining, manufacturing, and military applications. This datasheet provides...
Journal Articles
Alloy Digest (2003) 52 (12): Al-275.
Published: 01 December 2003
... Alcoa alloy 5454 was developed specifically for use in the manufacture of aluminum tank trailer and dump bodies. This revision of the original Alloy Digest data sheet is also specific to road transport products and adds additional coverage to alloy 5454 H34. This datasheet provides information on...
Journal Articles
Alloy Digest (1962) 11 (3): Al-4.
Published: 01 March 1962
... implements, highway trailers, machine tool parts, textile machinery, gasoiine fuel gages and meters. Manufacturer: William F. Jobbins. Incorporated Aurora, Illinois ...
Journal Articles
Alloy Digest (2004) 53 (4): CS-142.
Published: 01 April 2004
...). Applications: Typical applications include highway trailers, forestry and min- ing equipment, and other uses where weight is a critical factor. The improved surface capabilities make this product particularly suited for exposed off-highway applications. Producer: Algoma Steel, Inc. Burlington, Ontario, Canada...
Journal Articles
Alloy Digest (1974) 23 (7): SS-297.
Published: 01 July 1974
.... highway trailers. water-well casings, trans- former base plates. lightning standard base plates, radio and television towers. Manufacturer: Allegheny Ludlum Industries. Inc. Pittsburgh. Pennsylvania 15222. ...
Journal Articles
Alloy Digest (1995) 44 (10): SS-616.
Published: 01 October 1995
... uses are structural members, siding and roofing for railway cars and highway trailers, and severe stretch-forming applications such as auto wheelcovers. Producer: Allegheny Ludlum Steel Corp. Pittsburgh, PA 152225479 412-394-2800 SS616.S ...
Journal Articles
Alloy Digest (1953) 2 (1): SA-5.
Published: 01 January 1953
... ~_ Low .30 - - - Mild Steel 14 Trace - - - - 0. H. Iron 24 LOW .30 - - .50 Cu Bearing Steel 24 Low .30 .06 1.00 SO Yoloy ACR 83+ Low .30 - 2.00 1.00 Yoloy HSX 83+ General Characteristics: YOLOY is used where light weight and high strength are desirable such as in busses, trucks, trailers, street cars...
Journal Articles
Alloy Digest (1971) 20 (4): SA-264.
Published: 01 April 1971
... light plate. It is available in thicknesses from 0.071 to 0.312 inches. Maximum widths vary from 48 to 72 inches, depending oil thickness. Railroad equipment, utility trucks, giant transportation trucks, construction machinery, bridge and building structures, mining machinery, trailer parts, pre-shaped...