1-20 of 23 Search Results for

highway applications

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
Alloy Digest (2001) 50 (1): SS-815.
Published: 01 January 2001
... UNS S41003 is a low-cost utilitarian martensitic stainless steel to be used for highway and other applications. It is used in the tempered condition at several strength levels. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear...
Journal Articles
Alloy Digest (2004) 53 (5): CS-143.
Published: 01 May 2004
... Algoma 130 is a cost-effective choice for applications that require high strength, improved notch toughness, weldability, and good formability. It is one in a full range of heat treated plate products for highway trailers, mining, manufacturing, and military applications. This datasheet provides...
Journal Articles
Alloy Digest (2003) 52 (10): SA-522.
Published: 01 October 2003
... by being one of a family of alloy that can be fabricated readily. Applications include weight-sensitive components subject to high stress such as frames for large off-highway equipment. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile...
Journal Articles
Alloy Digest (1984) 33 (12): Al-254.
Published: 01 December 1984
... ALUMINUM 535.0 is a high-purity aluminum alloy of the aluminum-magnesium type. It possesses a high and stable combination of strength, shock resistance and ductility in the cast condition. Among its many applications are armament, hardware, cooking utensils, highway trailers, textile machinery...
Journal Articles
Alloy Digest (1986) 35 (8): SA-421.
Published: 01 August 1986
... be fabricated readily. Applications include weight-sensitive components subject to high stress such as frames for large off-highway haulers. This datasheet provides information on composition, physical properties, microstructure, elasticity, and tensile properties as well as fracture toughness. It also includes...
Journal Articles
Alloy Digest (2004) 53 (4): CS-142.
Published: 01 April 2004
...). Applications: Typical applications include highway trailers, forestry and min- ing equipment, and other uses where weight is a critical factor. The improved surface capabilities make this product particularly suited for exposed off-highway applications. Producer: Algoma Steel, Inc. Burlington, Ontario, Canada...
Journal Articles
Alloy Digest (2000) 49 (12): SA-506.
Published: 01 December 2000
... BETHLEHEM LUKENS PLATE HPS-70W is a high-performance steel (HPS) developed through a cooperative agreement among the Federal Highway Administration (FHWA), the American Iron and Steel Institute (AISI), and the Department of the Navy. This steel is an improved version of ASTM A 709 grade 70W...
Journal Articles
Alloy Digest (2003) 52 (9): SA-520.
Published: 01 September 2003
... BethStar 50 steel plate is a high-strength product with a 345 MPa (50 ksi) minimum yield strength. It contains low carbon and low sulfur and has outstanding toughness, weldability, and formability. It provides options for off-highway equipment. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1983) 32 (3): SS-422.
Published: 01 March 1983
...) shows improved resistance to pitting attack from various de-icing chemicals. In addition, the color of Uniloy 434, when buffed, closely resembles that of bright chromium plate. Hence a popular application for Uniloy 434 is automotive trim. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2006) 55 (2): SA-555.
Published: 01 February 2006
..., with membership including the American Iron and Steel Institute (AISI), Federal Highway Administration (FHWA), and U.S. Naval Surface Warfare Center (NSWC), developed a new steel grade, designated HPS 100W, for 690 MPa (100 ksi) minimum yield strength applications in bridges. This developmental grade has been...
Journal Articles
Alloy Digest (1962) 11 (3): Al-4.
Published: 01 March 1962
... Available: Ingots for sand castings. AISO modifications of this sand casting aIIoy composition for permanent mold and die castings, are available. Applications: Armament, automotive and marine castings, hardware, sporting goods, architectural ornaments, cooking uten- sils, agricultural implements, highway...
Journal Articles
Alloy Digest (1966) 15 (7): SA-198.
Published: 01 July 1966
.... Applications: Bridges, transportation equipment including marine, railway and highway, buildings and general constructional use. Particularly advantageous where high strength for thick sections is required arid als 0 when exposed unpainted exterior structures are contemplated. Manufacturer: The Steel Company...
Journal Articles
Alloy Digest (2020) 69 (12): Al-471.
Published: 01 December 2020
...- standing corrosion resistance. Field tests included pre- stressing samples at 240 MPa (35 ksi) and placing them underneath trucks that routinely traveled along the heav- ily salted winter highways between Alcoa s Massena, New York, and Cleveland, Ohio, plants. In addition, samples were placed at a seaside...
Journal Articles
Alloy Digest (1985) 34 (12): Al-262.
Published: 01 December 1985
... performance on salted streets and highways. In salt fog tests 6009-T4 and T6 outperformed 2036-T4. Alloy 6009 is essentially immune to stress-corrosion cracking and exfoliation. When coupled with steel, aluminum alloys are subject to galvanic corrosion. Proper protection of the steel is essential and joints...
Journal Articles
Alloy Digest (1995) 44 (4): Al-333.
Published: 01 April 1995
... for 4 hrs with a 12.S-lb load at 36 pm. SNo measurable wear. DOI: 10.31399/asm.ad.al0333 Copyright ┬ę ASM International┬« 1996 Table 5 - PROPERTIES VS. CAST IRON FOR CYLJNDER LINER APPLICATIONS DURALCAN DLJRALCAN GRAY CAST IRON W6A. 1OA F3S.lOS Grade 30/35 Wear-ASTM G77 BloCkoflRillg 1.6 1.5 4.9 Volume...
Journal Articles
Alloy Digest (1973) 22 (7): SA-291.
Published: 01 July 1973
... these ranges are subject to inquiry. Applications: Transportation eqUipTEnt, construction machinery, mining machinery, highway equipment, and automotive equipment Manufacturer: Bethlehem Steel Corporation Bethlehem, Pennsylvania 18016. ...
Journal Articles
Alloy Digest (2003) 52 (12): Al-275.
Published: 01 December 2003
.... Workability: This alloy has good hot working characteristics. It also has good cold-forming characteristics in the thicker sheet applications for which it is intended. Stiffening ribs may be pressed into brackets and support arms. Bending information is given in Table 3. Weldability: This alloy has good...
Journal Articles
Alloy Digest (1978) 27 (7): SA-348.
Published: 01 July 1978
... low temperatures such as drilling units, structural members for off-highway trucks, transportation and construction equipment. This steel should be considered for any application where high strength, toughness, formability and ease of welding are desired. Manufacturer: hnco Inc. Western Steel Division...
Journal Articles
Alloy Digest (1982) 31 (7): SA-385.
Published: 01 July 1982
... with quenched-and-tempered steel plate. BethStar 80 plate can be machined, formed and welded readily. It is used in several constructional applications and has the potential for many more applications. This datasheet provides information on composition, physical properties, microstructure, elasticity...
Journal Articles
Alloy Digest (1971) 20 (9): SA-268.
Published: 01 September 1971
...- ation of strength and low-temperature toughness, Table 3 and Figure 1, for non-carburizing applications. Naturally. the core of carburized material also has this high toughness. Forms Available: Rods, bars, forgings and billets. Applications: Carburized rock-bit bodies, carburized heavyduty gears in oil...