Alloy Digest (1974) 23 (4): SS-295.
Published: 01 April 1974
... alloy is also used in high-strength non-magnetic applications because it remains essentially non-magnetic even after severe cold working. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also...
Journal Articles
Alloy Digest (1974) 23 (1): SS-290.
Published: 01 January 1974
... CROLOY 299 is a chromium-manganese austenitic steel which can be cold worked to high levels of strength and hardness without becoming magnetic. It exhibits permeability of less than 1.01 Mu as measured with a Severn tester. This datasheet provides information on composition, physical properties...
Journal Articles
Alloy Digest (1995) 44 (5): Co-97.
Published: 01 May 1995
... composition hardness machinability orthopedic industry physical properties tensile properties workability thermal properties BIO-DURTM CCM PLUSM ALLOY g=t=; co-97 - DIGEST- MAY 1995 DATA ON WORLD WIDE METALS AND ALLOYS (Non-magnetic, cobaltchromlum-molybdenum alloy) This alloy is a high carbon...
Journal Articles
Alloy Digest (1957) 6 (8): SS-59.
Published: 01 August 1957
... WIDE METALS AND ALLOYS Psblkbed by Engineering Alloys Digest, Inc. Upper Montclair, New Jeemp ENDURO HCN (Heat Resistant, High Strength Steel, Type 309) ENDURO is an austenitic, non-magnetic chromium-nickel stainless steel having high creep and oxidation resistance at elevated temperatures. Composition...
Journal Articles
Alloy Digest (1963) 12 (6): Co-16.
Published: 01 June 1963
... DYNAVAR is a corrosion resistant, non-magnetic, age-hardening type cobalt-base alloy with good hot and cold working properties. It is characterized principally by its high fatigue resistance, tensile strength, torque values and corrosion resistance. This datasheet provides information on...
Journal Articles
Alloy Digest (1967) 16 (8): Cu-179.
Published: 01 August 1967
... EVERDUR-651 is a high-strength, corrosion-resistant copper-silicon alloy having good fabricating properties. It is non-magnetic and fatigue resistant. It is used for cold-headed bolts, hardware, marine fittings, etc. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1953) 2 (6): SS-8.
Published: 01 June 1953
... CYCLOPS 17A corrosion-resistant alloys heat resistance chemical composition compressive strength elasticity fatigue properties fracture toughness hardness tensile properties workability heat treatability machinability joinability physical properties high-temperature alloys low-temperature...
Journal Articles
Alloy Digest (1976) 25 (3): Ni-224.
Published: 01 March 1976
... Electrical and Electronic Applications) NIMAG 100 is wrought nickel combining excellent mechanical properties with good corrosion resistance. It retains its strength to a high degree at elevated temperatures. Nimag 100 is produced by vacuum melting to provide close control of composition. It is used in a...
Journal Articles
Alloy Digest (1984) 33 (2): Cu-472.
Published: 01 February 1984
... telecommunications or high- strength aircraft hook-up wire, CR 155 is an ideal material. CR 155 needs only small amounts (0. I9cor less) of magnesium and phosphorus. Both elements are non-strategic, non-magnetic, non- toxic and readily removed on subsequent remelting of the scrap. Thus CR 155 offers an attractive...
Journal Articles
Alloy Digest (1959) 8 (5): SS-87.
Published: 01 May 1959
... steam turbines. These include turbine wheels, couplings, shafts, valve stems, bolts, etc. Also, the alloy s non-magnetic and high yield strength char- acteristics make it highly desirable for low temperature usage as retaining rings and wedges for electrical apparatus. RAanufacturer: Westinghouse...
Journal Articles
Alloy Digest (1971) 20 (3): SS-252.
Published: 01 March 1971
... Engineering Alloys Digest, Inc. Upper Moncchir, New Jersey ARMCO 22-13-5* (High-Strength, Corrosion-Resistant Austenitic Stainless Steel) ARMCO 22-13-5 provides an unusually good combination of corrosion resistance and strength for an austenitic stainless steel. It is nonmag- netic even after severe cold work...
Journal Articles
Alloy Digest (1975) 24 (5): SS-311.
Published: 01 May 1975
... USS TENELON is a completely austenitic, nickel-free stainless steel with exceptionally high strength which is retained at elevated temperatures. It has excellent corrosion resistance in atmospheric and mild acid exposures and maintains nonmagnetic characteristics even when 60% cold reduced. It...
Journal Articles
Alloy Digest (1961) 10 (12): SS-125.
Published: 01 December 1961
... in the heat affected zone. Forms Available: Sheet and cold rolled strip, bar, wire and plate. Applications: Automobile anti-smog devices, high temperature springs, non-magnetic parts. Manufacturer: .4rmco Steel Corporation Middletown, Ohio ...
Journal Articles
Alloy Digest (1979) 28 (1): Ni-259.
Published: 01 January 1979
... Initial permeability, gauss 200 Residual induction, gauss 3500 Coercive force, oersted 3.3 Table 2 - NOMINAL TENSILE AND HARDNESS PROPERTIES Tensile Yield Strength Elongation Form and Strength (0.2% Offset) (2;J Rockwell Condition psi Psi Hardness Sheet and Strip (Sheet is cut from strip) Annealed 55000...
Journal Articles
Alloy Digest (1977) 26 (11): SS-228.
Published: 01 November 1977
... design and pattern equipment. Weldability: Supertherm weldability is very good for a high-strength, high- temperature alloy. Several processes can be utilized, Including manual shielded metal arc, automatic gas metal arc (MIG) and automatic gas tungsten (TIG) arc. Welding rod and wire with matching...
Journal Articles
Alloy Digest (1956) 5 (3): Ni-24.
Published: 01 March 1956
... than standard Duranickel, and is recom- mended for special applications requiring optimum machin- ability. In Duranickel R the design engineer has a wrought, non-ferrous, slightly magnetic alloy which has the high strength found in the hear treated alloy steels. In the soft condition, it is very...
Journal Articles
Alloy Digest (1964) 13 (3): Cu-139.
Published: 01 March 1964
.... Machinability: Mallory 150 Metal in the fully heat treated con- dition can be readily turned, drilled or tapped, using either high speed or carbide tools. In gener- al, the machining characteristics of this alloy can be classed with such non-leaded materials as high strength phosphor and silicon bronzes...
Journal Articles
Alloy Digest (1963) 12 (6): Ni-83.
Published: 01 June 1963
... 301 the design engineer has a wrought, non-ferrous, slightly magnetic alloy which bas the high saengtb found in the beat aeated alloy steels. Wire can be cold-drawn and age-hardened subsequently w develop tensile saengths of tbe order of 200,000 w 240,000 psi. In tbe soft condition, it is very...
Journal Articles
Alloy Digest (1953) 2 (1): Ni-2.
Published: 01 January 1953
... DURANICKEL, formerly known as Z-Nickel, is an age-hardenable nickel alloy having high strength and high corrosion resistance in addition to high heat resistance. It is magnetic at room temperature in all conditions. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1970) 19 (7): SS-241.
Published: 01 July 1970
... UNILOY 326 is a two-phase, ferromagnetic stainless steel characterized by high strength and very good general and stress corrosion resistance. It has distinct advantage for the fastener industry. This datasheet provides information on composition, physical properties, hardness, elasticity, and...