Alloy Digest (1975) 24 (8): Zn-21.
Published: 01 August 1975
... NJZ ALLOY No. 15 is a high-strength alloy with high stiffness and limited bending characteristics. It is produced from high-grade zinc base with additions of lead, copper, cadmium and magnesium. It can be severely work hardened and its applications include weather-stripping and hardware. This...
Journal Articles
Alloy Digest (1976) 25 (1): Zn-25.
Published: 01 January 1976
... NJZ Alloy No. 45 is a zinc-copper alloy characterized by high hardness and strength, good ductility and high stiffness. It work hardens easily. Among its many applications are hardware, sporting-equipment components, cable wrappings and watch cases. This datasheet provides information on...
Journal Articles
Alloy Digest (1976) 25 (12): Zn-30.
Published: 01 December 1976
... NJZ Alloy No. 55 is a zinc-cadmium alloy characterized by high tensile strength and hardness but low ductility. It has high stiffness and resiliency but low drawing and forming characteristics. Its applications include hardware and medallions. This datasheet provides information on composition...
Journal Articles
Alloy Digest (1989) 38 (9): Al-299.
Published: 01 September 1989
... the highly reactive nature of lithium in molten aluminum. In general, the alloy should be considered for use in light-weight structures requiring high strength and stiffness. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes...
Journal Articles
Alloy Digest (1959) 8 (1): CI-25.
Published: 01 January 1959
... MEEHANITE type GM is a high strength iron which may be cast uniformly solid regardless of casting size or sectional deviation. This particular engineering material possesses true elastic properties, conferring both controlled stiffness and resilience which provides good impact strength and shock...
Journal Articles
Alloy Digest (1990) 39 (8): Cp-10.
Published: 01 August 1990
... KEVLAR 49 is a high-modulus para-aramid reinforcing fiber. It is a widely used organic reinforcing fiber in advanced composites. It has exceptional strength and stiffness and is a low density material. This datasheet provides information on physical properties, tensile properties, and compressive...
Journal Articles
Alloy Digest (1997) 46 (12): Ti-111.
Published: 01 December 1997
... 3M TITANIUM MATRIX COMPOSITES are produced by electron-beam evaporation to apply Ti-6Al-4V coating to high-strength, high-modulus silicon carbon fibers. The resulting composite has increased strength and stiffness over monolithic titanium/titanium alloy parts. This datasheet provides information...
Journal Articles
Alloy Digest (2017) 66 (4): SA-780.
Published: 01 April 2017
... Strenx Section 700 is a cold-formed steel section made of hot-rolled, high-strength steel with a minimum yield strength of 700 MPa (102 ksi). Its high strength combined with naturally stiff form enables construction of stronger and lighter structures. The common shape is a U-bend channel. This...
Journal Articles
Alloy Digest (2017) 66 (6): SA-788.
Published: 01 June 2017
... Strenx Section 650 is a cold-formed steel section made of hot-rolled, high-strength steel with a minimum yield strength of 650 MPa (94 ksi). Its high strength combined with naturally stiff form enables construction of stronger and lighter structures. The common shape is a U-bend channel. This...
Journal Articles
Alloy Digest (2017) 66 (7): SA-792.
Published: 01 July 2017
... Strenx Section 900 is a cold-formed steel section made of hot-rolled, high-strength steel with a minimum yield strength of 900 MPa (131 ksi). Its high strength combined with naturally stiff form enables construction of stronger and lighter structures. The common shape is a U-bend channel. This...
Journal Articles
Alloy Digest (1975) 24 (7): Zn-20.
Published: 01 July 1975
... NJZ ALLOY No. 10 is an alloy with medium tensile strength and elongation. It is produced from a high-grade zinc base by additions of cadmium, iron, and lead. It combines good ductility with stiffness and its applications include hardware and laundry tags. This datasheet provides information on...
Journal Articles
Alloy Digest (1990) 39 (4): Cp-7.
Published: 01 April 1990
... KEVLAR 49 is a high-modulus para-aramid reinforcing fiber. It is the dominant organic reinforcing fiber in advanced composites today. It has exceptional strength and stiffness and it is a low density material. This datasheet provides information on composition, physical properties, elasticity...
Journal Articles
Alloy Digest (2019) 68 (6): Cu-890.
Published: 01 June 2019
... Olin Brass Alloy C77000 combines high strength with excellent stiffness, formability, corrosion resistance, and solderability. These characteristics make it extremely adaptable to a range of spring applications including flat and slightly formed springs. It is also used for switches, jacks, and...
Journal Articles
Alloy Digest (2020) 69 (2): Cu-905.
Published: 01 February 2020
... and electronic industries. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming and joining. Filing Code: Cu-905. Producer or source: Olin...
Journal Articles
Alloy Digest (1990) 39 (5): Cp-15.
Published: 01 May 1990
... alloys. They have similar longitudinal and trans- verse (isotropic) properties. Corrosion resistance when compared to high-strength alloys like 7075-T6, is also very good. SXA@ materials can be fabricated, bonded, joined, anodized and plated using conventional equipment and techniques. Forms Available...
Journal Articles
Alloy Digest (2005) 54 (12): Al-398.
Published: 01 December 2005
... alloys. General Characteristics: Alcoa developed aluminum-lithium alloy 2099, also designated as C460, for use in aerospace and high-strength applications requiring low density, high stiffness, superior damage tolerance, excellent corrosion resistance, and weldability. Lithium additions increase the...
Journal Articles
Alloy Digest (2012) 61 (9): Al-439.
Published: 01 September 2012
... strength applications requiring low density, high stiffness, superior damage tolerance, excellent corrosion resistance, and weldability. Li additions increase the strength and modulus of Al alloys while lowering their density. EXCO rating SCC (LT direction), min MPa (ksi) in ASTM G47 2099-T83 P/EA 330 (48...
Journal Articles
Alloy Digest (1978) 27 (2): Zn-33.
Published: 01 February 1978
... strength, psi 4300047000 Table 2 - RELATNE PROPERTIES fiwerty Rating Stiffness A+ Tensile strength A+ Hardness A+ Elongation (Tensile) D Bending E Forming (Stretching) E Drawing E Code: A+ = Excellent. A =High. B = Good. C = Medium. D = Fair. E = Not Recommended. 0.226 6.25 693-747 0.11 143 x 10-6 67.5 28...
Journal Articles
Alloy Digest (1966) 15 (5): SS-181.
Published: 01 May 1966
... or scraping. Slow feeds, deep cuts and powerful, rigid machines are necessary for best results. Work should be firmly mounted and sup- ported,and tool mountings should provide maximum stiffness. Both high speed steel and carbide tools may be used successfully. Good lubrication and cooling are...
Journal Articles
Alloy Digest (1966) 15 (10): SS-187.
Published: 01 October 1966
... in all cases that the tool be kept continually entering into the metal. Slow feeds, deep cuts and powerful, rigid machines are necessary for best results. Work should be firmly mounted and supported, and tool mounc- ings should provide maximum stiffness. Both high speed steel and carbide tools may be...