1-20 of 647 Search Results for

heavy-impact tools

Sort by
Journal Articles
Alloy Digest (1975) 24 (2): TS-284.
Published: 01 February 1975
... FERRO-TIC SK is a cemented carbide comprising titanium carbide in a matrix of 5% chromium tool steel. It can be heat treated and machined by conventional means and is recommended for cold and hot-working dies and heavy-impact tools. This datasheet provides information on composition, physical...
Journal Articles
Alloy Digest (2005) 54 (4): TS-562.
Published: 01 April 2005
... to conventional S7. Typical applications include plastic injection molds, punches and dies by wire EDM, and heavy impact tools. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on wear resistance as well...
Journal Articles
Alloy Digest (1984) 33 (2): SA-397.
Published: 01 February 1984
... AISI 4161 is a low-alloy steel of the chromium-molybdenum type; it contains nominally 0.61% carbon. It has relatively high hardenability and good resistance to abrasion, impact and fatigue. It is an oil-hardening grade and is recommended for moderately heavy-duty service. This steel has...
Journal Articles
Alloy Digest (1956) 5 (2): TS-43.
Published: 01 February 1956
... C. Y. W. CHOICE steel is a chromium hot work steel developed for applications where dies or tools are subjected to heavy pressure or impact while in contact with hot metal. It is an ASM Class IV A-2 tool steel. This datasheet provides information on composition, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1962) 11 (4): TS-117.
Published: 01 April 1962
... HWD No. 1 is a chromium-molybdenum-tungsten alloy hot work steel developed for applications where dies or tools are subject to heavy pressure or impact while in contact with hot metal. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile...
Journal Articles
Alloy Digest (1964) 13 (9): SA-167.
Published: 01 September 1964
... AISI 9260 is an oil-hardening type of spring steel and tool steel recommended for repeated and severe impact service. It is also used for heavy duty, shock resistant machine parts. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties...
Journal Articles
Alloy Digest (1964) 13 (11): SA-170.
Published: 01 November 1964
... Republic HP150 is an alloy steel designed to give 150,000 psi yield strength with exceptional toughness. The alloy is intended for fabrication in the heat treated condition principally for heavy plate sections. This datasheet provides information on composition, physical properties, hardness...
Journal Articles
Alloy Digest (1964) 13 (11): TS-154.
Published: 01 November 1964
... Lo-Air is a high-carbon alloy steel having air hardening characteristics. It is a deep hardening steel producing a combination of high strength, toughness and wear resistance. It is recommended for precision tools and heavy duty blanking and forming dies. This datasheet provides information...
Journal Articles
Alloy Digest (1962) 11 (8): Co-34.
Published: 01 August 1962
... Tantung 144 is a cast nonferrous alloy recommended for cutting tools where resistance to abrasion is paramount and where there is little or no shock or impact. This datasheet provides information on composition, physical properties, and hardness as well as creep. It also includes information...
Journal Articles
Alloy Digest (1974) 23 (9): Ni-208.
Published: 01 September 1974
...+ Alloy No. 273 (Hard-Facing Alloy Resistant to Heat and Heavy Impact) HAYNES Alloy No. 273 is a nickel-base, hard-facing alloy developed to provide extra life for hot-working equipment such as hot-forging dies, hot-shear blades and hotextrusion dies. It is deposited by using a composite electrode...
Journal Articles
Alloy Digest (1982) 31 (6): TS-400.
Published: 01 June 1982
... hardness heat treatability heavy-duty punches joinability MOSIL physical properties rivet sets workability UNS T41905 All Filing Code: TS400 MOSIL Tool Steel Or JUNE 1962 DIGEDT - DATA ON WORLD WIDE METAW AND ALLOYS @ Copyright 1960. Engineering Publications, 1% A41 rights reserved. Plddih?dby...
Journal Articles
Alloy Digest (1953) 2 (7): TS-8.
Published: 01 July 1953
... composition fracture toughness hardness workability heat treatability machinability JULY 1963 DATA ON WORLD WIDE METALS AND ALLOYS COMOKUT (HIoH SPEED TOOL STEEL) COMOKUT is a tungsten-molybdenum-chromium-vanadium&t type of high speed stccI. continuo heavy liogging cuts where high cutting-edge...
Journal Articles
Alloy Digest (1957) 6 (2): Cu-47.
Published: 01 February 1957
... Shear strength, psi 58000 60000 55000 60000 Charpy impact (keyhole), ft. lbs. 2 4 6 8 Izod impact, ft. lbs. 6 10 14 DOI: 10.31399/asm.ad.cu0047 Copyright ┬ę ASM International┬« 1996 Machinability: Readily machinable. High speed steel tools are re- commended for roughing operations and carbide tools...
Journal Articles
Alloy Digest (1962) 11 (3): SA-126.
Published: 01 March 1962
... ESCO Alloy 12M is a low alloy, medium carbon content, hard, shock and impact-resisting steel recommended for heavy duty cast parts. Minor chemical composition variations and heat treatment are employed in order to develop specific properties. This alloy possesses exceptional toughness at low...
Journal Articles
Alloy Digest (1975) 24 (9): CS-57.
Published: 01 September 1975
... and small hand tools to heavy components for machinery. Forms Available: Biiets, rods, bars, hot-rolled strip, cold-rolled strip, wire, and heavy rolled and forged shapes. Applications: Hand tools, music wire, control rods, braces, shafts, heavy machinery parts, wrenches, hammers. pliers, screwdrivers...
Journal Articles
Alloy Digest (1973) 22 (4): CS-51.
Published: 01 April 1973
... AISI 1070 is a high-carbon water or oil-hardening tool and spring steel of low hardenability. It is used for railroad and street railway rails, heavy machinery parts, shafts, springs and a wide variety of hand and machine tools requiring strength and wear resistance. This datasheet provides...
Journal Articles
Alloy Digest (1961) 10 (9): Cu-107.
Published: 01 September 1961
.../30) 331 Compression elasticity limit, psi 65000 Compression ultimate strength, psi 171000 Shear stress, psi 60000 Charpy impact, ft.lbs. (Keyhole) 2 Izod impact, ft. lbs. 2 Sand Cast Centrifugal Cast 85000 70000 0.5 0 331 65000 171000 70000 2 2 Table 3 - ELEVATED TEMPERATURE PROPERTIES Test...
Journal Articles
Alloy Digest (1986) 35 (8): CS-112.
Published: 01 August 1986
.... relatively tough (pearlitic) core; this combination is highly suitable for many hand and machine tools. No. Gl0860 enjoys an extremely wide range of applicarions from music wire and small hand tools to heavy components for machinery. Forms Available: Billets. rods, bars, hot-rolled strip, cold-roiled strip...
Journal Articles
Alloy Digest (1980) 29 (1): CI-49.
Published: 01 January 1980
... liner applications involving heavy sections. **PAC is heat treated to provide additional resistance to breakage needed in wearing applications such as coal crusher parts, lifter bars and segmental concaves. Table 2 - ABRASION RESISTANCE, IMPACT AND HARDNESS (Simulated 5inch section properties of Grades...
Journal Articles
Alloy Digest (1971) 20 (8): TS-237.
Published: 01 August 1971
... in tempering but are based on 3/4-in. diameter specimens; therefore, tools of heavy section may be several points lower in Rockwell hardness for a given treatment) Tempering Temperature OF As quenched 300 400 500 600 700 800 900 1000 1100 1200 1300 Rockwell C Hardness Oil Quench Water Quench from 1625OF from...