Alloy Digest (1953) 2 (7): TS-8.
Published: 01 July 1953
... COMOKUT is a tungsten-molybdenum-chromium-vanadium-cobalt type of high-speed steel. It is particularly suitable for continuous heavy hogging cuts where high cutting-edge temperatures and pressures are developed. This datasheet provides information on composition and hardness as well as fracture...
Journal Articles
Alloy Digest (1982) 31 (3): TS-395.
Published: 01 March 1982
... the other alloying elements form carbides. Thus the cobalt in- teases the hot or red hardness, thereby enabling the tool to maintain a higher hardness at elevated temperatures. Type T4 is recommended for hogging cuts with heavy-duty lathe, planer and boring tools, or where the temperature of the...
Journal Articles
Alloy Digest (1955) 4 (6): Cu-27.
Published: 01 June 1955
.... Machinability: Machinabiliy raring is 20% of Free-Cutting Brass. The chips produced in the cold-worked tempers are long, tough and quire springy. Turning wols of H.S.S. should have rake angles of 8 to 12 deg. and clearance angles of 5 deg. Use a mineral oil con- taining from 10 to 20% lard oiL Use high speeds...