Alloy Digest (1981) 30 (4): Cu-416.
Published: 01 April 1981
... HITENSO 162 is a copper-cadmium alloy that offers a unique combination of high tensile strength and high electrical conductivity in wire where ordinarily these properties are incompatible. It also is noted for its malleability and toughness. Among its many uses are heating pads, electric blankets...
Journal Articles
Alloy Digest (1974) 23 (8): Cu-283.
Published: 01 August 1974
..., tensile properties, and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-283. Producer or source: Copper alloy foundries. Producer or Source: Copper alloy foundries...
Journal Articles
Alloy Digest (1966) 15 (1): Cu-2.
Published: 01 January 1966
... combustion engines, gears, worm wheels, propellers, shaftin , valve seats for super-heated steam and similar service, %ea liners, thrust pads, machine and tool bearings, v% stems and spindles, wea.r plates, and marine quipment and parts. Manutacturer: American Manganese Bronze Company Phil? Jelphia...
Journal Articles
Alloy Digest (1955) 4 (7): CI-11.
Published: 01 July 1955
... NI-RESIST high nickel alloy cast irons have high resistance to wear, corrosion, and heat. They are furnished in seven different types varying primarily in nickel, chromium, and copper content. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile...
Journal Articles
Alloy Digest (1982) 31 (5): Ni-275.
Published: 01 May 1982
... NICROFER 6020 HMO Filing Code: N i-275 Nickel Alloy MAY 1982 - DATA ON WORLD WIDE METALS AND ALLOYS @ Copyright 1980. Engineering Publications, Inc. Ail rights reserved. ISSN : 002-6 14X Pad&h& by En@eering Alloys Digest, Imr Post office Box 823 Upper Montclair, New jersey NICROFER* 6020 HMO (Heat and...
Journal Articles
Alloy Digest (2006) 55 (7): CS-146.
Published: 01 July 2006
... Sandvik 20C is a strip steel with high fatigue strength, supplied for pad printing or as a shock absorber steel. It has a high yield to tensile strength value. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also...
Journal Articles
Alloy Digest (1967) 16 (10): SA-217.
Published: 01 October 1967
... surface harden- ing (flame or induction) IO approximately Rockwell 0:. Forms Available: Bars, rods, forpiops in rhe heat treated and stress-relieved condition. Applications: Brake dies, goose neck dies, sprinp pad dies. hcmmiop dies, curling dies, pipe bending dies. pressure pads, stripper plates, punch...
Journal Articles
Alloy Digest (1993) 42 (10): TS-520.
Published: 01 October 1993
... THYRODUR 2379 (AISI D2) is an air hardening, high carbon chromium die steel, well suited for long run tool and die applications. It is capable of great hardness and high resistance to abrasive wear. It is non-deforming; consistent in response to all machining, heat treating and production...
Journal Articles
Alloy Digest (1955) 4 (10): Cu-32.
Published: 01 October 1955
... are mad with hardened steel aears. stripe -nits and heavy dury feed nuts. - _ Valve guides in internal combusdon engines, propellers. shafiing~ vake scars for super-heated steam and &dir ser- vice, thrust pads, valve stems and spindles, wear plates and marine equipment Manufacturer: Lumen Bearing...
Journal Articles
Alloy Digest (1978) 27 (7): Co-20.
Published: 01 July 1978
... HAYNES STELLITE alloy No. 6K is a cobalt-base alloy with outstanding resistance to most types of wear. Its wear resistance is a built-in characteristic and not the result of heat-treatment, plating, nitriding, or other methods used to produce a superficial hardness on metal parts. Among its many...
Journal Articles
Alloy Digest (2012) 61 (4): Cu-805.
Published: 01 April 2012
... use as small-gauge wire in termination equipment, spring contacts in automotive and signal relays, and in such applications as high-strength transmission lines, switchgear components, heating pads, electric blanket elements, fuse clips, and tinsel used in the telephone industry. Producer: Ansonia...
Journal Articles
Alloy Digest (1988) 37 (10): Cu-541.
Published: 01 October 1988
... being Joined by welding brazing or soldeting. It is hardenable by cold work but not by heat tmatment. Forms Available: hmakd. hard. spring and extra spring temper strip; annealed and hard drawn rod, annealed. hard, extra hard. spring and extra 6pring wk. tubing. Applications: Trolley wire, heating pad...
Journal Articles
Alloy Digest (2013) 62 (6): TS-717.
Published: 01 June 2013
... Märker WM 28 is an all-purpose hot-working tool steel with very good hot strength. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on heat treating. Filing Code: TS-717. Producer or...
Journal Articles
Alloy Digest (2009) 58 (7): TS-681.
Published: 01 July 2009
... Märker DCM is a hot-working tool steel with good hot toughness and good hot strength. This datasheet provides information on composition, physical properties, and elasticity as well as creep. It also includes information on high temperature performance as well as heat treating. Filing Code: TS-681...
Journal Articles
Alloy Digest (2009) 58 (8): SS-1039.
Published: 01 August 2009
... pads, car seats, baseboard heaters, floor heaters, resistors, etc. Producer: Kanthal AB Kanthal Heating Systems Amherst, NY 14228-2311 Tel: (716) 691-4010 Fax: (716) 691-7850 www.Kanthal.com Table 1 Temperature factor of resistance 100 °C (212 °F) 200 °C (390 °F) 300 °C (570 °F) 400 °C (750 °F) 500 °C...
Journal Articles
Alloy Digest (1966) 15 (8): SA-199.
Published: 01 August 1966
..., railway cars, booms, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and bend strength as well as fracture toughness and fatigue. It also includes information on forming, heat treating, machining, and joining. Filing...
Journal Articles
Alloy Digest (2015) 64 (12): Cu-845.
Published: 01 December 2015
..., heat treating, and joining. Filing Code: Cu-845. Producer or source: Columbia Metals Ltd. Producer or Source: Columbia Metals Ltd Copyright © ASM International® 2015 2015 ASM International chemical composition Colsibro corrosion-resistant alloys hardness heat treatability joinability...
Journal Articles
Alloy Digest (2020) 69 (5): TS-792.
Published: 01 May 2020
... information on composition, hardness, and elasticity. It also includes information on forming and heat treating. Filing Code: TS-792. Producer or source: Deutsche Edelstahlwerke Specialty Steel GmbH. Producer or Source: Deutsche Edelstahlwerke Specialty Steel GmbH Copyright © ASM International® 2020...
Journal Articles
Alloy Digest (1989) 38 (9): SA-439.
Published: 01 September 1989
... properties, elasticity, and tensile properties. It also includes information on heat treating and joining. Filing Code: SA-439. Producer or source: Uddeholm Corporation. Producer or Source: Uddeholm Corporation Copyright © ASM International® 1996 1996 ASM International brinell hardness chemical...
Journal Articles
Alloy Digest (1973) 22 (8): Cu-269.
Published: 01 August 1973
..., and compressive strength as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-269. Producer or source: Bunting Brass & Bronze Company. Producer or Source: Bunting Brass & Bronze Company...